← Back to Patent Explorer
US4632687A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of melting raw materials for glass or the like using solid fuels or fuel-batch mixtures

Assignee: PPG Industries Inc
•
Filing: 1985-06-25
•
Granted: 1986-12-30
•
Expires: 2005-06-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Thermally fusible material such as glass batch is liquefied using a solid carbonaceous fuel such as coal as the major energy source. In another embodiment, solid or liquid fuel is mixed with the batch material being fed to an initial liquefaction stage. Melting may be advanced further in a subsequent stage where the melt may also be re-oxidized.

Inventors

  • 👤 Gerald E. Kunkle
  • 👤 Henry M. Demarest
  • 👤 Larry J. Shelestak

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 02:58
CPC Classifications
C; C03; C03B; C03B5/00; C03B5/16; C03B5/235; C03B5/2356; C03B3/00; C03B3/02; C03B5/14; C03C; C03C1/00; C03C1/02; C03C1/026; Y; Y02; Y02P; Y02P40/00; Y02P40/50

Claims Analysis

Total Claims: 44
Claim 1
Independent Claim 108 words
A method of liquefying glass batch or the like comprising: contacting pulverulent glass batch material with a solid or liquid fuel having an ash content, the fuel being provided in an amount sufficient to supply a major portion of the energy required to liquefy the batch material, combusting the fuel so as to liquefy the batch material, and mixing the ash from the combusted fuel into the liquefying batch at the region of combustion sufficiently rapidly that substantially all of the ash is incorporated into the liquefying batch and flows from the combustion zone entrained therein, whereby buildup of ash deposits in the combustion zone is substantially avoided.
Claim 2
Independent Claim 108 words
A method of liquefying glass batch or the like comprising: contacting pulverulent glass batch material with a solid or liquid fuel having an ash content, the fuel being provided in an amount sufficient to supply a major portion of the energy required to liquefy the batch material, combusting the fuel so as to liquefy the batch material, and mixing the ash from the combusted fuel into the liquefying batch at the region of combustion sufficiently rapidly that substantially all of the ash is incorporated into the liquefying batch and flows from the combustion zone entrained therein, whereby buildup of ash deposits in the combustion zone is substantially avoided.
Claim 3
Dependent Claim 13 words
The method of claim 1 wherein the batch is a soda-lime-silica glass batch.
Claim 4
Dependent Claim 25 words
The method of claim 2 wherein the batch is formulated to produce a glass having a viscosity of at least 100 poises at 1425° C.
Claim 5
Dependent Claim 26 words
The method of claim 1 wherein the fuel is mixed with the batch prior to being fed to a vessel in which the combustion takes place.
Claim 6
Independent Claim 77 words
A method of liquefying glass batch or the like comprising: contacting pulverulent glass batch material with a solid or a liquid fuel having an ash content, the fuel being provided in an amount sufficient to supply a major portion of the energy required to liquefy the batch material, combusting the fuel so as to liquefy the batch material on a sloped surface encircling a central cavity, and incorporating substantially all of the ash into the liquefied product.
Claim 7
Independent Claim 77 words
A method of liquefying glass batch or the like comprising: contacting pulverulent glass batch material with a solid or a liquid fuel having an ash content, the fuel being provided in an amount sufficient to supply a major portion of the energy required to liquefy the batch material, combusting the fuel so as to liquefy the batch material on a sloped surface encircling a central cavity, and incorporating substantially all of the ash into the liquefied product.
Claim 8
Dependent Claim 33 words
The method of claim 5 wherein the liquefied material is drained from the sloped surface in a reduced condition, and is passed to a downstream zone where it is subjected to re-oxidizing conditions.
Claim 9
Dependent Claim 24 words
The method of claim 1 wherein the fuel in contact with the batch material constitutes substantially the entire energy source for liquefying the batch.
Claim 10
Dependent Claim 10 words
The method of claim 1 wherein the fuel is coal
Claim 11
Dependent Claim 13 words
The method of claim 1 wherein the fuel is a liquid petroleum product.
Claim 12
Dependent Claim 23 words
The method of claim 1 wherein the combustion of the fuel is supported by feeding essentially pure oxygen to the region of combustion.
Claim 13
Dependent Claim 19 words
The method of claim 1 wherein the batch material and the fuel are fed separately to the combustion zone.
Claim 14
Dependent Claim 19 words
The method of claim 1 wherein the batch material is liquefied on a sloped surface encircling a central cavity.
Claim 15
Dependent Claim 15 words
The method of claim 12 wherein the sloped surface is rotated about the central cavity.
Claim 16
Dependent Claim 13 words
The method of claim 13 wherein the rotation is about a vertical axis.
Claim 17
Dependent Claim 46 words
The method of claim 1 wherein the combustion of the ash-containing fuel and liquefaction of the batch material takes place in a first vessel from which the material flows in an incompletely melted state, and melting of the liquefied material is furthered in a separate vessel.
Claim 18
Independent Claim 72 words
A method of melting glass comprising: heating glass batch material on a sloped surface in a first zone by combusting solid or liquid fuel in contact with the glass batch, whereby reducing conditions exist as the batch becomes liquefied, draining the liquefied glass batch to a second zone and subjecting the reduced liquefied batch material to oxidizing conditions so as to restore the oxidation state of the product to a desired level.
Claim 19
Independent Claim 72 words
A method of melting glass comprising: heating glass batch material on a sloped surface in a first zone by combusting solid or liquid fuel in contact with the glass batch, whereby reducing conditions exist as the batch becomes liquefied, draining the liquefied glass batch to a second zone and subjecting the reduced liquefied batch material to oxidizing conditions so as to restore the oxidation state of the product to a desired level.
Claim 20
Dependent Claim 23 words
The method of claim 16 wherein the fuel contacting the batch material provides the majority of the energy for liquefying the batch material.
Claim 21
Dependent Claim 10 words
The method of claim 17 wherein the fuel is coal.
Claim 22
Dependent Claim 21 words
The method of claim 16 wherein the fuel is mixed with the batch material before being fed to a combustion zone.
Claim 23
Dependent Claim 23 words
The method of claim 16 wherein liquefied batch material in the second zone is gathered into a pool into which oxygen is injected.
Claim 24
Dependent Claim 17 words
The method of claim 20 wherein the pool in the second zone is heated by submerged combustion.
Claim 25
Dependent Claim 27 words
The method of claim 21 wherein agitation of the material in the second zone is provided by injection of combusting gases into the body of liquefied material.
Claim 26
Dependent Claim 17 words
The method of claim 22 wherein coloring material is added to the material in the second zone.
Claim 27
Dependent Claim 23 words
The method of claim 16 wherein the fuel has an ash content and the ash is substantially incorporated into the liquefied batch material.
Claim 28
Dependent Claim 30 words
The method of claim 16 wherein oxidation in the second zone is sufficient to raise the Fe +3 /Fe +2 ratio of an iron-containing clear glass to at least 1.5.
Claim 29
Independent Claim 94 words
A method of melting a thermally fusible material comprising feeding batch material and solid or liquid carbonaceous fuel onto a sloped melting surface, the fuel being provided in sufficient quantity to yield upon combustion a substantial portion of the heat required to liquefy the batch material, providing an oxidant at the sloped surface in sufficient quantity to support said combustion, draining batch liquefied by the heat from the sloped surface, gathering a pool of the liquefied batch, and providing an oxidizing agent to the pool to raise the oxidation state of the liquefied material.
Claim 30
Independent Claim 94 words
A method of melting a thermally fusible material comprising feeding batch material and solid or liquid carbonaceous fuel onto a sloped melting surface, the fuel being provided in sufficient quantity to yield upon combustion a substantial portion of the heat required to liquefy the batch material, providing an oxidant at the sloped surface in sufficient quantity to support said combustion, draining batch liquefied by the heat from the sloped surface, gathering a pool of the liquefied batch, and providing an oxidizing agent to the pool to raise the oxidation state of the liquefied material.
Claim 31
Dependent Claim 23 words
The method of claim 26, wherein thermal energy is provided to the pool of liquefied batch so as to further the melting thereof.
Claim 32
Dependent Claim 18 words
The method of claim 27, wherein the heat is provided to the pool by means of submerged combustion.
Claim 33
Dependent Claim 32 words
The method of claim 28 wherein the pool is divided into two chambers and the liquefied material passes from one chamber to the other with submerged combustion being provided in each chamber.
Claim 34
Dependent Claim 10 words
The method of claim 29, wherein the material is glass.
Claim 35
Dependent Claim 11 words
The method of claim 26, wherein the carbonaceous fuel is coal.
Claim 36
Dependent Claim 12 words
The method of claim 31, wherein the material being melted is glass.
Claim 37
Dependent Claim 29 words
The method of claim 32, wherein coal is provided in sufficient amount at the sloped melting surface to provide substantially the entire heat required to liquefy the batch material.
Claim 38
Dependent Claim 23 words
The method of claim 26, wherein the fuel is mixed with the batch materials prior to being deposited onto the sloped melting surface.
Claim 39
Dependent Claim 13 words
The method of claim 34, wherein the fuel is a liquid petroleum product.
Claim 40
Dependent Claim 10 words
The method of claim 34, wherein the fuel is coal.
Claim 41
Dependent Claim 19 words
The method of claim 26, wherein the batch is fed onto a sloped surface that encircles a central cavity.
Claim 42
Dependent Claim 16 words
The method of claim 37, wherein the sloped melting surface is rotated around the central cavity.
Claim 43
Dependent Claim 14 words
The method of claim 38, wherein the rotation is about a substantially vertical axis.
Claim 44
Dependent Claim 38 words
The method of claim 37, wherein the rate of feeding batch is controlled relative to the rate of liquefying the batch so as to maintain a substantially stable layer of the batch material as the sloped melting surface.

References Cited (Backward Citations)

US2006987A Cited
US2337072A Cited
GB658141A Cited
US3248205A Cited
US3294505A Cited
US3689251A Cited
US4032121A Cited
US3969068A Cited
US4006003A Cited
US4381934A Cited
US4496313A Cited
US4551161A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-12-29 1990-06-30 1990-12-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-12-29 1994-06-30 1994-12-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-12-29 1998-06-30 1998-12-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag