US4631301A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for incorporating chlorpyrifos into thermoplastic resins

Assignee: Dow Chemical Japan Ltd
•
Filing: 1985-02-06
•
Granted: 1986-12-23
•
Expires: 2005-02-06
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Novel composition and method for thermally stabilizing an O-pyridyl phosphate insecticide such as chlorpyrifos. The insecticide is mixed with a phthalate ester prior to its incorporation into a thermoplastic resin, such as polyvinyl chloride.

Inventors

  • 👤 Jiro Kozuma
  • 👤 Hirohiko Hamaguchi
  • 👤 Tetsuya Shibahara
  • 👤 Joseph P. Strasser

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 12:32
CPC Classifications
C; C08; C08K; C08K5/00; C08K5/49; C08K5/51; A; A01; A01N; A01N25/00; A01N25/22; A01N57/00; A01N57/10; A01N57/16; C08K5/0008; C08K5/0058

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 130 words
A method for thermally stabilizing an O-pyridyl phosphate compound of the formula ##STR4## wherein R represents halopyridyl, Z is oxygen or sulphur, and each R 1 is loweralkyoxy, amino or loweralkylamino, comprising (a) mixing said O-pyridyl phosphate with a phthalate ester of the formula ##STR5## wherein Y is alkyl from about 2 to about 20 carbon atoms or ##STR6## wherein Y 1 is alkyl from about 1 to about 20 carbon atoms, and Y 2 is hydrogen or methyl; said O-pyridyl phosphate and said phthalate ester being present in proportions effective to prevent appreciable ecomposition of said O-pyridyl phosphate upon heating said mixture, and (b) incorporating said mixture into a thermoplastic resin heated to a temperature which would decompose the O-pyridyl phosphate compound if the O-pyridyl phosphate were heated alone.
Claim 2
Independent Claim 130 words
A method for thermally stabilizing an O-pyridyl phosphate compound of the formula ##STR4## wherein R represents halopyridyl, Z is oxygen or sulphur, and each R 1 is loweralkyoxy, amino or loweralkylamino, comprising (a) mixing said O-pyridyl phosphate with a phthalate ester of the formula ##STR5## wherein Y is alkyl from about 2 to about 20 carbon atoms or ##STR6## wherein Y 1 is alkyl from about 1 to about 20 carbon atoms, and Y 2 is hydrogen or methyl; said O-pyridyl phosphate and said phthalate ester being present in proportions effective to prevent appreciable ecomposition of said O-pyridyl phosphate upon heating said mixture, and (b) incorporating said mixture into a thermoplastic resin heated to a temperature which would decompose the O-pyridyl phosphate compound if the O-pyridyl phosphate were heated alone.
Claim 3
Dependent Claim 11 words
The method of claim 1 wherein said O-pyridyl phosphate is chlorpyrifos.
Claim 4
Dependent Claim 12 words
The method of claim 1 wherein said phthalate ester is dioctyl phthalate.
Claim 5
Dependent Claim 18 words
The method of claim 1 wherein said O-pyridyl phosphate is chlorpyrifos and said phthalate ester is dioctyl phthalate.
Claim 6
Dependent Claim 26 words
The method of claim 1 wherein said thermoplastic resin is selected from the group consisting of polyvinyl chloride, polystyrene, acrylonitrile, methacrylate ester, polyethylene and combinations thereof.
Claim 7
Dependent Claim 12 words
The method of claim 1 wherein said thermoplastic resin is polyvinyl chloride.
Claim 8
Dependent Claim 24 words
The method of claim 1 wherein said O-pyridyl phosphate is chlorpyrifos, said phthalate ester is dioctyl phthalate and said thermoplastic resin is polyvinyl chloride.
Claim 9
Dependent Claim 16 words
The method of claim 1 wherein said steps of mixing and incorporating are performed by kneading.
Claim 10
Dependent Claim 15 words
The method of claim 1 further comprising (c) pelleting the resin containing said O-pyridyl phosphate.

References Cited (Backward Citations)

US3886236A Cited
US4160335A Cited
US3890270A Cited
US4435383A Cited
EP0121712A1 Cited
US4528125A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-12-22 1990-06-23 1990-12-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-12-22 1994-06-23 1994-12-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-12-22 1998-06-23 1998-12-23 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag