Method for recovering gallium
Assignee: Mitsubishi Chemical Corp
•
Filing: 1985-07-02
•
Granted: 1986-12-23
•
Expires: 2005-07-02
Abstract
Abstract A method for recovering gallium from an aqueous solution containing gallium, which comprises contacting the aqueous solution containing gallium to a porous polymer having a water-insoluble substituted quinolinol retained therein, to let the polymer adsorb gallium, and then eluting gallium from the polymer.
Inventors
- 👤 Takao Yotsuyanagi
- 👤 Yoshinobu Nishiyama
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-04 09:15
CPC Classifications
C; C01; C01F; C01F7/00; C01F7/02; C01F7/46; C01F7/47; C01G; C01G15/00; C01G15/003; C22; C22B; C22B3/00; C22B3/20; C22B3/22; C22B3/24; Y; Y02; Y02P; Y02P10/00; Y02P10/20; Y10; Y10S; Y10S423/00; Y10S423/09; Y10S423/14
Claims Analysis
Total Claims: 7
Claim 1
Independent Claim
97 words
A method for recovering gallium selectively from an aqueous basic solution containing gallium, which comprises dissolving 7-substituted-8- quinolinol having a C 5 -C 20 hydrocarbon group at the 7-position in a solvent, mixing the resulting solution with a porous polymer having a pore volume of from 0.3 to 1.2 ml/g, letting the solvent evaporate to obtain a porous polymer retaining substantially only the substituted quinolinol, filling a column with the polymer, passing the aqueous basic solution through the column to absorb gallium in the polymer and passing an aqueous acid solution through the column to elute gallium.
Claim 2
Independent Claim
97 words
A method for recovering gallium selectively from an aqueous basic solution containing gallium, which comprises dissolving 7-substituted-8- quinolinol having a C 5 -C 20 hydrocarbon group at the 7-position in a solvent, mixing the resulting solution with a porous polymer having a pore volume of from 0.3 to 1.2 ml/g, letting the solvent evaporate to obtain a porous polymer retaining substantially only the substituted quinolinol, filling a column with the polymer, passing the aqueous basic solution through the column to absorb gallium in the polymer and passing an aqueous acid solution through the column to elute gallium.
Claim 3
Dependent Claim
23 words
The method according to claim 1, wherein the aqueous solution containing gallium is an aqueous sodium aluminate solution formed by a Bayer process.
Claim 4
Dependent Claim
13 words
The method according to claim 1, wherein the waterinsoluble substituted quinolinol is 7-(1-vinyl-3,3,5,5-tetramethylhexyl)-8-quinolinol.
Claim 5
Dependent Claim
28 words
The method of claim 1, wherein the porous polymer is composed essentially of an acrylate, a methacrylate, diallyl phthalate, diallyl succinate, ethylene glycol diacrylate and/or ethylene glycol dimethacrylate.
Claim 6
Dependent Claim
54 words
The method according to claim 1, wherein the galliumadsorbed porous polymer is contacted with sulfuric acid or nitric acid having a concentration of from 0.01 to 0.1 mol/liter to elute aluminum, and then the polymer is contacted with sulfuric acid or nitric acid having a concentration of at least 0.5 mol/liter to elute gallium.
Claim 7
Dependent Claim
48 words
The method according to claim 1, wherein the galliumadsorbed porous polymer is contacted with hydrochloric acid having a concentration of more than 5 mol/liter to elute aluminum, and then the polymer is contacted with hydrochloric acid having a concentration of from 0.1 to 5 mol/liter to elute gallium.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1989-12-22 | 1990-06-23 | 1990-12-23 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1993-12-22 | 1994-06-23 | 1994-12-23 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1997-12-22 | 1998-06-23 | 1998-12-23 | $7700.00 | Window Closed / Lapsed |