US4631079A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method for stretching a glass rod
Assignee: Furukawa Electric North America Inc
•
Filing: 1985-11-25
•
Granted: 1986-12-23
•
Expires: 2005-11-25
Abstract
Abstract Control over the diameter variations in a glass rod (10) during the stretching thereof is accomplished by cooling the rod after heating and initial neck down of a portion (22) thereof. After cooling, the rod (10) is reheated, at a lower temperature sufficient to reflow the glass in the necked-down portion (22) thereof, and is then stretched to the desired final diameter. Heating the rod (10) at a lower temperature during stretching increases the viscosity thereof which reduces its response to the stretching conditions, thereby affording better control over diameter fluctuations.
Inventors
- 👤 Harold R. Clark
- 👤 David A. Nicol
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-03 16:46
CPC Classifications
C; C03; C03B; C03B37/00; C03B37/01; C03B37/012; C03B37/01205; C03B37/01225; C03B37/0124; C03B23/00; C03B23/04; C03B23/047
Claims Analysis
Total Claims: 7
Claim 1
Independent Claim
148 words
A method for stretching a glass rod which affords increased control over fluctuations in the diameter thereof comprising the steps of: (a) heating a portion of the rod to a first temperature which is high enough for reflow thereof; (b) necking down the portion of the rod to approximately the desired final diameter by stretching the rod; (c) cooling the rod; (d) progressively reheating the necked down portion of the rod at a lower temperature which is high enough to reflow that portion thereof which had been necked down, but not high enough to reflow the portion of the rod not yet necked down; and (e) stretching the rod during said progressive reheating to draw out the portion of the rod previously necked down, to the desired final diameter and to provide a new necked down portion from the part of the rod not yet reduced in diameter.
Claim 2
Independent Claim
148 words
A method for stretching a glass rod which affords increased control over fluctuations in the diameter thereof comprising the steps of: (a) heating a portion of the rod to a first temperature which is high enough for reflow thereof; (b) necking down the portion of the rod to approximately the desired final diameter by stretching the rod; (c) cooling the rod; (d) progressively reheating the necked down portion of the rod at a lower temperature which is high enough to reflow that portion thereof which had been necked down, but not high enough to reflow the portion of the rod not yet necked down; and (e) stretching the rod during said progressive reheating to draw out the portion of the rod previously necked down, to the desired final diameter and to provide a new necked down portion from the part of the rod not yet reduced in diameter.
Claim 3
Independent Claim
189 words
A method of stretching a glass rod which affords increased control over fluctuations in the diameter thereof comprising the steps of: (a) mounting the rod on a glass lathe between the headstock and the tailstock thereof; (b) rotating the rod; (c) heating a portion of the rod to a first temperature high enough for reflow thereof; (d) removing the tailstock of the glass lathe away from the headstock during rod rotation until the portion of the rod has been necked down to approximately the desired final diameter; (e) cooling the rod; (f) progressively reheating the necked down portion of the rod to a second temperature which is lower than said first temperature but high enough for reflow of that portion thereof which had been necked down and not high enough to reflow the portion of the rod not yet necked down; and (g) moving the tailstock of the glass lathe further away from the headstock to draw out that portion of the rod necked down, to the desired final diameter and to provide a new necked down portion form the part of the rod not yet reduced in diameter.
Claim 4
Independent Claim
189 words
A method of stretching a glass rod which affords increased control over fluctuations in the diameter thereof comprising the steps of: (a) mounting the rod on a glass lathe between the headstock and the tailstock thereof; (b) rotating the rod; (c) heating a portion of the rod to a first temperature high enough for reflow thereof; (d) removing the tailstock of the glass lathe away from the headstock during rod rotation until the portion of the rod has been necked down to approximately the desired final diameter; (e) cooling the rod; (f) progressively reheating the necked down portion of the rod to a second temperature which is lower than said first temperature but high enough for reflow of that portion thereof which had been necked down and not high enough to reflow the portion of the rod not yet necked down; and (g) moving the tailstock of the glass lathe further away from the headstock to draw out that portion of the rod necked down, to the desired final diameter and to provide a new necked down portion form the part of the rod not yet reduced in diameter.
Claim 5
Dependent Claim
48 words
The method according to claim 2 wherein the step of heating said rod to the predetermined temperature comprising the substeps of: (a) flowing combustible gases into a torch at a first rate; (b) igniting said torch; and (c) moving the torch beneath the rod along the axis thereof.
Claim 6
Dependent Claim
28 words
The method according to claim 3 wherein the step of cooling said rod includes the substep of extinguishing said torch by interrupting the flow of combustible gases thereto.
Claim 7
Dependent Claim
50 words
The method according to claim 3 wherein said step of reheating said rod to said second temperature comprises the substeps of: flowing combustible gases into the torch at a second rate less than said first rate; rekindling said torch; and moving the torch beneath the rod along the axis thereof.
References Cited (Backward Citations)
US2282993A
Cited
DE896710C
Cited
US3293019A
Cited
US3556758A
Cited
US3652248A
Cited
US3852054A
Cited
US4247319A
Cited
JPS5792534A
Cited
US4477273A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1989-12-22 | 1990-06-23 | 1990-12-23 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1993-12-22 | 1994-06-23 | 1994-12-23 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1997-12-22 | 1998-06-23 | 1998-12-23 | $7700.00 | Window Closed / Lapsed |