Selective catalytic oxidation of carbon monoxide in hydrocarbon stream to carbon dioxide

Assignee: Millennium Petrochemicals Inc
•
Filing: 1984-07-27
•
Granted: 1986-12-02
•
Expires: 2004-07-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method is disclosed for selectively oxidizing carbon monoxide present in a hydrocarbon stream to carbon dioxide employing a specially prepared supported catalyst containing cobalt oxide, said catalyst being prepared by successively impregnating the support with a solution of an alkaline compound and a solution containing cobalt ions, calcining the impregnated support and washing the calcined support to activate the catalyst.

Inventors

  • 👤 Jawad H. Murib

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 10:31
CPC Classifications
B; B01; B01J; B01J23/00; B01J23/70; B01J23/74; B01J23/75; C; C07; C07C; C07C51/00; C07C51/16; C07C51/21; C07C51/25; C07C51/252

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 201 words
A method of preparing, from an alkaline compound and a cobalt compound, an alumina supported cobalt oxide catalyst useful for the selective oxidation of CO in a gaseous reaction medium containing a hydrocarbon which consists essentially of: (a) impregnating an alumina support with an aqueous solution of a first water soluble alkaline compound whose anion is capable of forming a water insoluble cobalt compound when said first water soluble alkaline compound is reacted with a water soluble cobalt compound, said water insoluble cobalt compound capable of providing a water insoluble cobalt oxide upon calcination, (b) drying the alkaline compound impregnated alumina support, (c) impregnating the dried alkaline compound impregnated alumina support with an aqueous solution of a water soluble cobalt compound whose anion is capable of forming a second water soluble alkaline compound upon reaction of said first water soluble alkaline compound with said water soluble cobalt compound, whereby an insoluble cobalt compound forms on the support, (d) calcining the cobalt compound impregnated, alkaline compound containing, alumina support to form an insoluble cobalt oxide on the cobalt compound impregnated, alkaline compound containing, alumina support, (e) washing the calcined support with water to remove soluble compounds and activate the cobalt oxide catalyst.
Claim 2
Independent Claim 201 words
A method of preparing, from an alkaline compound and a cobalt compound, an alumina supported cobalt oxide catalyst useful for the selective oxidation of CO in a gaseous reaction medium containing a hydrocarbon which consists essentially of: (a) impregnating an alumina support with an aqueous solution of a first water soluble alkaline compound whose anion is capable of forming a water insoluble cobalt compound when said first water soluble alkaline compound is reacted with a water soluble cobalt compound, said water insoluble cobalt compound capable of providing a water insoluble cobalt oxide upon calcination, (b) drying the alkaline compound impregnated alumina support, (c) impregnating the dried alkaline compound impregnated alumina support with an aqueous solution of a water soluble cobalt compound whose anion is capable of forming a second water soluble alkaline compound upon reaction of said first water soluble alkaline compound with said water soluble cobalt compound, whereby an insoluble cobalt compound forms on the support, (d) calcining the cobalt compound impregnated, alkaline compound containing, alumina support to form an insoluble cobalt oxide on the cobalt compound impregnated, alkaline compound containing, alumina support, (e) washing the calcined support with water to remove soluble compounds and activate the cobalt oxide catalyst.
Claim 3
Dependent Claim 43 words
A method according to claim 1 wherein the first water soluble alkaline compound contains an alkali or alkaline earth metal cation and a hydroxide or a carbonate anion and the water soluble cobalt compound contains a chloride, a nitrate or a sulfate anion.
Claim 4
Dependent Claim 21 words
A method according to claim 2 wherein the first alkaline compound is potassium carbonate, and the cobalt compound is cobaltous chloride.
Claim 5
Dependent Claim 17 words
A method according to claim 1 wherein the water used to wash the calcined support is deionized.
Claim 6
Dependent Claim 27 words
A method according to claim 1 wherein the molar ratio of the first soluble alkaline compound to the soluble cobalt compound is at least the stoichiometric requirement.
Claim 7
Dependent Claim 22 words
A method according to claim 5 wherein the molar ratio is about the stoichiometric requirement to about 5 times the stoichiometric requirement.
Claim 8
Dependent Claim 31 words
A method according to claim 1 wherein, in step (d) the impregnated support in step (c) is calcined at about 200° C. to 800° C. for up to about 48 hours.
Claim 9
Dependent Claim 34 words
A method according to claim 1 wherein, at the conclusion of step (e), the amount of cobalt on the support, calculated as CoO, is about 0.1% to about 10% by weight of the support.
Claim 10
Dependent Claim 34 words
A method according to claim 1 wherein, at the conclusion of step (e), the amount of cobalt on the support, calculated as CoO, is about 0.5% to about 5% by weight of the support.

References Cited (Backward Citations)

US1937689A Cited
US3267045A Cited
US3338952A Cited
US3529935A Cited
US3839549A Cited
US4025561A Cited
US4314084A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-12-01 1990-06-02 1990-12-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-12-01 1994-06-02 1994-12-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-12-01 1998-06-02 1998-12-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag