← Back to Patent Explorer
US4623398A Expired / Lapsed US ⏱️ 0.0 years remaining

Organo-clays

Assignee: SOUTHERN CLAY PRODUCTS Inc A Corp OF TEXAS
•
Filing: 1985-04-25
•
Granted: 1986-11-18
•
Expires: 2005-04-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An organo-clay is prepared by mixing a quaternary ammonium compound with an aqueous suspension of a smectite clay; thereafter subjecting the smectite clay/quaternary ammonium compound/water mixture to high shear mixing for a time sufficient to dissipate in the mixture at least 100 KJ of energy per kg. of dry solids in the mixture; and then dewatering the product thus obtained.

Inventors

  • 👤 Howard Goodman
  • 👤 Andrew R. Fugler

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 04:34
CPC Classifications
C; C01; C01B; C01B33/00; C01B33/20; C01B33/36; C01B33/38; C01B33/44; C09; C09D; C09D5/00; C09D5/04; C09K; C09K8/00; C09K8/02; C09K8/04; C09K8/14; C09K8/145

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 81 words
A process for preparing an organo-clay which is readily dispersible in an organic medium, which process comprises (a) mixing an aqueous suspension of a smectite clay with a quaternary ammounium compound capable of rendering the smectite clay organophilic; (b) subjecting the mixture formed in step (a) to high shear mixing for a time sufficient to dissipate in the mixture at least 100 KJ of energy per kg. of dry solids in the mixture; and (c) dewatering the product of step (b).
Claim 2
Dependent Claim 81 words
A process for preparing an organo-clay which is readily dispersible in an organic medium, which process comprises (a) mixing an aqueous suspension of a smectite clay with a quaternary ammounium compound capable of rendering the smectite clay organophilic; (b) subjecting the mixture formed in step (a) to high shear mixing for a time sufficient to dissipate in the mixture at least 100 KJ of energy per kg. of dry solids in the mixture; and (c) dewatering the product of step (b).
Claim 3
Dependent Claim 17 words
A process according to claim 1, wherein the dewatered product of step (c) is dried and milled.
Claim 4
Dependent Claim 45 words
A process according to claim 1, wherein before the aqueous suspension of the smectite clay is mixed with the quaternary ammonium compound, the latter is melted and then mixed with hot water at a temperature higher than the melting point of the quaternary ammonium compound.
Claim 5
Dependent Claim 58 words
A process according to claim 3, wherein the mixture of the molten quaternary ammonium compound and hot water is subjected to high shear mixing for a time sufficient to dissipate in the mixture at least 100 KJ of energy per kg. of dry quaternary ammonium compound, before it is mixed with the aqueous suspension of the smectite clay.
Claim 6
Dependent Claim 120 words
A process according to claim 1, wherein the quaternary ammonium compound can be represented by the general formula: ##STR2## wherein R 1 is selected from saturated and unsaturated alkyl groups having from 10 to 24 carbon atoms, R 2 and R 3 , which may be the same or different, are each selected from saturated and unsaturated alkyl groups having from 1 to 24 carbon atoms and aralkyl groups having from 7 to 10 carbon atoms, R 4 is selected from alkyl groups having from 1 to 6 carbon atoms and aralkyl groups having from 7 to 10 carbon atoms, and X is selected from OH, Cl, Br, I, NO 2 , CH 3 SO 4 and CH 3 .COO.
Claim 7
Dependent Claim 65 words
A process according to claim 5, wherein the quaternary ammonium compound is selected from the group consisting of benzyl methyl dialkyl ammonium chlorides, dimethyl dialkyl ammonium chlorides, benzyl dimethyl alkyl ammonium chlorides, benzyl trialkyl ammonium chlorides and methyl trialkyl ammonium chlorides in which the one or more alkyl group represents a mixture of hydrocarbon radicals derived from tallow having from 14 to 20 carbon atoms.
Claim 8
Dependent Claim 25 words
A process according to claim 1, wherein the aqueous suspension of the smectite clay is added to the quaternary ammonium compound and not vice versa.
Claim 9
Dependent Claim 39 words
A process according to claim 1, wherein the smectite clay is mixed with the quaternary ammonium compound in proportions such that there are present from 95 to 140 milliequivalents of quaternary ammonium cation per 100 g of dry clay.

References Cited (Backward Citations)

US4208218A Cited
US4371626A Cited
US4391637A Cited
US4483934A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-11-17 1990-05-19 1990-11-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-11-17 1994-05-19 1994-11-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-11-17 1998-05-19 1998-11-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag