Sensor with polycrystalline silicon resistors

Assignee: Siemens AG
•
Filing: 1984-05-25
•
Granted: 1986-11-18
•
Expires: 2004-05-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Sensor with polycrystalline silicon resistors which are applied to a substrate and are covered with a dielectric passivating layer, characterized by the feature that the resistors are thermally adapted by targeted adjustment of their dopings and by suitable healing, and are balanced by laser trimming.

Inventors

  • 👤 Josef Binder
  • 👤 David Cutter
  • 👤 Wolfgang Henning
  • 👤 Hans-Christian Schaber
  • 👤 Frank Mollmer
  • 👤 Hansjorg Reichert

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 08:47
CPC Classifications
G; G01; G01L; G01L1/00; G01L1/20; G01L1/22; G01L1/225; G01L1/2262; G01L1/2287; G01L1/2293; G01L9/00; G01L9/0041; G01L9/0051; G01L9/0052; G01L9/0055; Y; Y10; Y10S; Y10S73/00; Y10S73/04; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49004; Y10T29/49082; Y10T29/49103

Claims Analysis

Total Claims: 28
Claim 1
Independent Claim 60 words
Sensor with polycrystalline silicon resistors which are applied to a substrate and are covered with a dielectric passivating layer, in which temperature coefficients and resistance values of the resistors are adjusted and equalized by laser trimming, by doping the resistors and by healing with partial recrystallization of the resistors by laser healing with application of laser radiation or oven healing.
Claim 2
Dependent Claim 60 words
Sensor with polycrystalline silicon resistors which are applied to a substrate and are covered with a dielectric passivating layer, in which temperature coefficients and resistance values of the resistors are adjusted and equalized by laser trimming, by doping the resistors and by healing with partial recrystallization of the resistors by laser healing with application of laser radiation or oven healing.
Claim 3
Dependent Claim 70 words
Sensor according to claim 1, wherein resistors which are adjusted by laser healing by application of laser radiation, the thickness d of the passivating layer is ##EQU11## where λ vac is the wavelength of the laser radiation used in a vacuum, i is zero or a natural number, and n 1 is the index of refraction of the passivating layer, whereby optimum input coupling of the laser radiation is assured.
Claim 4
Dependent Claim 59 words
Sensor according to claim 2, wherein the substrate contains underneath the polycrystalline silicon resistors, at least one insulating layer provided with optimum reflection conditions, of the thickness ##EQU12## where λ vac is the wavelength of laser radiation used in a vacuum, i is zero or a natural number, and n 2 the index of refraction of the insulating layer.
Claim 5
Dependent Claim 23 words
Sensor according to claim 2, wherein the resistors are piezoresistive and are arranged in a bridge circuit, to form a pressure measuring device.
Claim 6
Dependent Claim 16 words
Sensor according to claim 2, wherein the resistors form a temperature sensor or a position sensor.
Claim 7
Dependent Claim 59 words
Sensor according to claim 1, wherein the substrate contains underneath the polycrystalline silicon resistors, at least one insulating layer provided with optimum reflection conditions, of the thickness ##EQU13## where λ vac is the wavelength of laser radiation used in a vacuum, i is zero or a natural number, and n 2 the index of refraction of the insulating layer.
Claim 8
Dependent Claim 23 words
Sensor according to claim 6, wherein the resistors are piezoresistive and are arranged in a bridge circuit, to form a pressure measuring device.
Claim 9
Dependent Claim 16 words
Sensor according to claim 6, wherein the resistors form a temperature sensor or a position sensor.
Claim 10
Dependent Claim 23 words
Sensor according to claim 1, wherein the resistors are piezoresistive and are arranged in a bridge circuit, to form a pressure measuring device.
Claim 11
Dependent Claim 31 words
Sensor according to claim 9, wherein the resistors form additionally compensating resistors of the bridge circuit, which bring about a compensation of the temperature coefficient of the offset of the bridge.
Claim 12
Dependent Claim 25 words
Sensor according to claim 9, including an operational amplifier following the bridge, and wherein polycrystalline resistors are connected between the bridge and the operational amplifier.
Claim 13
Dependent Claim 16 words
Sensor according to claim 1, wherein the resistors form a temperature sensor or a position sensor.
Claim 14
Dependent Claim 20 words
Sensor according to claim 1, wherein the doping concentration of the resistors has the value 2·10 20 cm -3 .
Claim 15
Dependent Claim 19 words
Sensor according to claim 1, wherein the resistors are arranged in a bridge circuit to form a measuring device.
Claim 16
Dependent Claim 105 words
Sensor with polycrystalline silicon resistors which are applied to a substrate and are covered with a dielectric passivating layer, in which temperature coefficients and resistance values of the resistors are adjusted and equalized by laser trimming, by doping the resistors and by healing with partial recrystallization of the resistors by laser healing with application of laser radiation or oven healing, wherein the resistors are piezoresistive and are arranged in a bridge circuit, to form a pressure measuring device, wherein the resistors form additionally balancing resistors which have the same doping as the piezoresistive resistors to bring about compensation of the temperature coefficient of the bridge.
Claim 17
Dependent Claim 105 words
Sensor with polycrystalline silicon resistors which are applied to a substrate and are covered with a dielectric passivating layer, in which temperature coefficients and resistance values of the resistors are adjusted and equalized by laser trimming, by doping the resistors and by healing with partial recrystallization of the resistors by laser healing with application of laser radiation or oven healing, wherein the resistors are piezoresistive and are arranged in a bridge circuit, to form a pressure measuring device, wherein the resistors form additionally balancing resistors which have the same doping as the piezoresistive resistors to bring about compensation of the temperature coefficient of the bridge.
Claim 18
Dependent Claim 24 words
Sensor according to claim 15, wherein the piezoresistive resistors and the balancing resistors are doped to give a zero value for the temperature coefficient.
Claim 19
Dependent Claim 22 words
Sensor according to claim 16, wherein the doping concentration of the resistors is between 10 18 and 10 19 cm -3 .
Claim 20
Dependent Claim 25 words
Sensor according to claim 17, wherein the doping is carried out with a doping material selected from the group consisting of boron, arsenic and phosphorous.
Claim 21
Dependent Claim 25 words
Sensor according to claim 16, wherein the doping is carried out with a doping material selected from the group consisting of boron, arsenic and phosphorous.
Claim 22
Dependent Claim 25 words
Sensor according to claim 15, wherein the doping is carried out with a doping material selected from the group consisting of boron, arsenic and phosphorous.
Claim 23
Dependent Claim 94 words
Sensor with polycrystalline silicon resistors which are applied to a substrate and are covered with a dielectric passivating layer, in which temperature coefficients and resistance values of the resistors are adjusted and equalized by laser trimming, by doping the resistors and by healing with partial recrystallization of the resistors by laser healing with application of laser radiation or oven healing wherein the resistors are piezoresistive and are arranged in a bridge circuit, to form a pressure measuring device, wherein the piezoresistive resistors are doped to give a zero value temperature dependence of their sensitivity.
Claim 24
Dependent Claim 94 words
Sensor with polycrystalline silicon resistors which are applied to a substrate and are covered with a dielectric passivating layer, in which temperature coefficients and resistance values of the resistors are adjusted and equalized by laser trimming, by doping the resistors and by healing with partial recrystallization of the resistors by laser healing with application of laser radiation or oven healing wherein the resistors are piezoresistive and are arranged in a bridge circuit, to form a pressure measuring device, wherein the piezoresistive resistors are doped to give a zero value temperature dependence of their sensitivity.
Claim 25
Dependent Claim 243 words
Method for manufacturing a sensor with polycrystalline silicon resistors which comprises (a) depositing a n-silicon layer epitaxially on an n + -silicon substrate, (b) placing p-doped bridge resistors R b which form the sensor, into the n-silicon layer by means of phototechniques, (c) applying a silicon dioxide layer to the entire semiconductor substrate over the entire surface, (d) reducing the applied silicon dioxide layer in the region of the bridge resistors (R b ) to a smaller layer thickness by means of a phototechnique, (e) thereupon, depositing a thin silicon nitride layer over the entire surface, (f) applying amorphous silicon to the silicon nitride layer over the entire surface, (g) doping parts of the applied amorphous silicon layer to obtain one and maximally two doping concentrations, (h) depositing a passivating layer in a predetermined layer thickness over the entire surface of the entire semiconductor wafer, (i) performing laser healing of certain regions of the amorphous silicon layer wherein the laser illuminates the regions line by line, (j) performing oven-healing of the entire semiconductor wafer, (k) structuring the amorphous silicon layer, whereby different polysilicon resistors (R K ) and (R K' ) are formed, (l) performing a new passivation operation, (m) reducing the silicon substrate at the place of the bridge resistors (R b ) by means of etching on the back side, and (n) subjecting the polysilicon resistors (R K and R K' ) to a fine adjustment by means of laser trimming.
Claim 26
Dependent Claim 243 words
Method for manufacturing a sensor with polycrystalline silicon resistors which comprises (a) depositing a n-silicon layer epitaxially on an n + -silicon substrate, (b) placing p-doped bridge resistors R b which form the sensor, into the n-silicon layer by means of phototechniques, (c) applying a silicon dioxide layer to the entire semiconductor substrate over the entire surface, (d) reducing the applied silicon dioxide layer in the region of the bridge resistors (R b ) to a smaller layer thickness by means of a phototechnique, (e) thereupon, depositing a thin silicon nitride layer over the entire surface, (f) applying amorphous silicon to the silicon nitride layer over the entire surface, (g) doping parts of the applied amorphous silicon layer to obtain one and maximally two doping concentrations, (h) depositing a passivating layer in a predetermined layer thickness over the entire surface of the entire semiconductor wafer, (i) performing laser healing of certain regions of the amorphous silicon layer wherein the laser illuminates the regions line by line, (j) performing oven-healing of the entire semiconductor wafer, (k) structuring the amorphous silicon layer, whereby different polysilicon resistors (R K ) and (R K' ) are formed, (l) performing a new passivation operation, (m) reducing the silicon substrate at the place of the bridge resistors (R b ) by means of etching on the back side, and (n) subjecting the polysilicon resistors (R K and R K' ) to a fine adjustment by means of laser trimming.
Claim 27
Dependent Claim 183 words
Method for manufacturing a sensor with polycrystalline silicon resistors which comprises (a) depositing a n-silicon layer epitaxially on an n + -silicon substrate, (b) applying a silicon dioxide layer to the entire semiconductor substrate over the entire surface, (c) optionally, depositing a thin silicon nitride layer thereon over the entire surface, (d) applying amorphous silicon over the entire surface on the silicon nitride layer or silicon oxide layer, (e) doping parts of the applied amorphous silicon layer to obtain one and maximally two different doping concentration, (f) subsequently, performing laser healing of regions of the amorphous silicon layer wherein the laser illuminates the regions line by line, (g) performing oven-heating of the entire semiconductor wafer, (h) structuring the amorphous silicon layer, whereby different polysilicon resistors together with the bridge resistors are produced as pressure sensors, (i) performing a new passivation operation, (j) reducing the thickness of the substrate layer at the location of the bridge resistors (R b ) by means of etching on the back side, and (k) subjecting the polycrystalline silicon resistors to a fine adjustment by means of laser trimming.
Claim 28
Dependent Claim 183 words
Method for manufacturing a sensor with polycrystalline silicon resistors which comprises (a) depositing a n-silicon layer epitaxially on an n + -silicon substrate, (b) applying a silicon dioxide layer to the entire semiconductor substrate over the entire surface, (c) optionally, depositing a thin silicon nitride layer thereon over the entire surface, (d) applying amorphous silicon over the entire surface on the silicon nitride layer or silicon oxide layer, (e) doping parts of the applied amorphous silicon layer to obtain one and maximally two different doping concentration, (f) subsequently, performing laser healing of regions of the amorphous silicon layer wherein the laser illuminates the regions line by line, (g) performing oven-heating of the entire semiconductor wafer, (h) structuring the amorphous silicon layer, whereby different polysilicon resistors together with the bridge resistors are produced as pressure sensors, (i) performing a new passivation operation, (j) reducing the thickness of the substrate layer at the location of the bridge resistors (R b ) by means of etching on the back side, and (k) subjecting the polycrystalline silicon resistors to a fine adjustment by means of laser trimming.

References Cited (Backward Citations)

US3938175A Cited
US4503709A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-11-17 1990-05-19 1990-11-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-11-17 1994-05-19 1994-11-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-11-17 1998-05-19 1998-11-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag