Method of forming phosphor pattern on fluorescent screen for color picture tubes with polymer coagulent

Assignee: Hitachi Ltd
•
Filing: 1985-07-08
•
Granted: 1986-09-16
•
Expires: 2005-07-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method of forming a color picture tube fluorescent screen by so-called dry process. After a photosticky substance mainly containing a diazonium compound is coated on a panel inner face, phosphor is adhered to portions of the compound which have been exposed to light through a color selection electrode and rendered sticky, and surplus phosphor applied on unexposed portions of the compound is removed, the above steps being consecutively repeated for phosphors of three colors to form picture elements of triads of three color phosphors on the panel inner face. The panel inner face is then treated with an aqueous solution containing at least polymer coagulant.

Inventors

  • 👤 Kiyoshi Miura
  • 👤 Hiroshi Yokomizo
  • 👤 Osamu Sasaya
  • 👤 Hajime Morishita
  • 👤 Yoshifumi Tomita

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 05:04
CPC Classifications
H; H01; H01J; H01J9/00; H01J9/20; H01J9/22; H01J9/227; H01J9/2271; G; G03; G03F; G03F7/00; G03F7/26; G03F7/28; H01J29/00; H01J29/02; H01J29/10; H01J29/18; H01J29/22; H01J29/225

Claims Analysis

Total Claims: 22
Claim 1
Independent Claim 240 words
In a method of forming a fluorescent screen for a color picture tube comprising: a first step of coating an inner panel face of a bulb of the color picture tube with a photosticky substance mainly containing a diazonium compound to form a layer of the compound: a second step of exposing to light through a color selection electrode portions of said compound layer where a first color phosphor is to be adhered to as to render exposed portions of said compound sticky; a third step of applying the first color phosphor on the surface of said compound layer; a fourth step of removing surplus first color phosphor applied on unexposed portions of said compound layer; a fifth step of conducting said second, third and fourth steps consecutively for the phosphor of second and third colors to form a fluorescent screen comprising picture elements of triads of three color phosphors on the inner face of the panel; and a sixth step of filming or aluminizing said fluorescent screen; the improvement wherein after applying the three color phosphors to the inner face of the panel and before said filming or aluminizing step, said said inner panel face with picture elements of three color phosphors is treated with an aqueous solution of polymer coagulant to improve the adhesiveness of the phosphor to the inner panel face thereby allowing sufficient washing to form a color picture tube having better quality and improved brightness.
Claim 2
Dependent Claim 240 words
In a method of forming a fluorescent screen for a color picture tube comprising: a first step of coating an inner panel face of a bulb of the color picture tube with a photosticky substance mainly containing a diazonium compound to form a layer of the compound: a second step of exposing to light through a color selection electrode portions of said compound layer where a first color phosphor is to be adhered to as to render exposed portions of said compound sticky; a third step of applying the first color phosphor on the surface of said compound layer; a fourth step of removing surplus first color phosphor applied on unexposed portions of said compound layer; a fifth step of conducting said second, third and fourth steps consecutively for the phosphor of second and third colors to form a fluorescent screen comprising picture elements of triads of three color phosphors on the inner face of the panel; and a sixth step of filming or aluminizing said fluorescent screen; the improvement wherein after applying the three color phosphors to the inner face of the panel and before said filming or aluminizing step, said said inner panel face with picture elements of three color phosphors is treated with an aqueous solution of polymer coagulant to improve the adhesiveness of the phosphor to the inner panel face thereby allowing sufficient washing to form a color picture tube having better quality and improved brightness.
Claim 3
Dependent Claim 22 words
A method according to claim 1 wherein the concentration of the polymer coagulant in said aqueous solution is 0.01 to weight %.
Claim 4
Dependent Claim 18 words
A method according to claim 1 which further includes washing the panel inner face after said treating step.
Claim 5
Dependent Claim 27 words
A method according to claim 1 or 3 wherein the panel inner face is rotated at 15 to 180 rpm in the treatment of the treating step.
Claim 6
Dependent Claim 12 words
A method according to claim 3 wherein the washing agent is water.
Claim 7
Dependent Claim 18 words
A method according to claim 3 wherein the washing agent is the solution used in the treating step.
Claim 8
Dependent Claim 27 words
A method according to claim 3 wherein the washing agent is polymer coagulant having a concentration lower than that of the solution used in the treating step.
Claim 9
Independent Claim 222 words
A method of forming a fluorescent screen for a color picture tube comprising: a first step of coating an inner panel face of the color picture tube with a photosticky substance mainly containing a diazonium compound to form a layer of the compound; a second step of exposing to light through a color selection electrode portions of said compound layer where a first color phosphor is to be adhered so as to render exposed portions of said compound sticky; a third step of applying the first color phosphor on the surface of said compound layer; a fourth step of removing surplus first color phosphor applied on unexposed portions of said compound layer; a fifth step of conducting said second, third, fourth steps consecutively for the phosphor of second and third colors to form a fluorescent screen comprising picture elements of triads of three color phosphors on the inner face of the panel; and a sixth step of filming or aluminizing said fluorescent screen; the improvement wherein after applying the three color phosphors to the inner face of the panel and before said filming or aluminizing step, said inner panel face with picture elements of triads of three color phosphors is treated with an aqueous solution containing polymer coagulant and surfactant, thereby improving the quality and brightness of the fluorescent screen after filming.
Claim 10
Independent Claim 222 words
A method of forming a fluorescent screen for a color picture tube comprising: a first step of coating an inner panel face of the color picture tube with a photosticky substance mainly containing a diazonium compound to form a layer of the compound; a second step of exposing to light through a color selection electrode portions of said compound layer where a first color phosphor is to be adhered so as to render exposed portions of said compound sticky; a third step of applying the first color phosphor on the surface of said compound layer; a fourth step of removing surplus first color phosphor applied on unexposed portions of said compound layer; a fifth step of conducting said second, third, fourth steps consecutively for the phosphor of second and third colors to form a fluorescent screen comprising picture elements of triads of three color phosphors on the inner face of the panel; and a sixth step of filming or aluminizing said fluorescent screen; the improvement wherein after applying the three color phosphors to the inner face of the panel and before said filming or aluminizing step, said inner panel face with picture elements of triads of three color phosphors is treated with an aqueous solution containing polymer coagulant and surfactant, thereby improving the quality and brightness of the fluorescent screen after filming.
Claim 11
Dependent Claim 39 words
A method according to claim 8 wherein the concentration in said aqueous solution of the polymer coagulant is 0.01 to 1 weight % and that of the surfactant is 0.05 to 10 weight %, the relation therebetween being complementary.
Claim 12
Dependent Claim 27 words
A method according to claim 8 or 11 wherein the panel inner face is rotated at 15 to 180 rpm in the treatment of the treating step.
Claim 13
Dependent Claim 17 words
A method according to claim 8 which include washing the panel inner face after said treating step.
Claim 14
Dependent Claim 12 words
A method according to claim 11 wherein the washing agent is water.
Claim 15
Dependent Claim 18 words
A method according to claim 11 wherein the washing agent is the solution used in the treating step.
Claim 16
Dependent Claim 33 words
A method according to claim 11 wherein the washing agent is an aqueous solution containing polymer coagulant having a concentration lower than that of the solution used in the treating step and surfactant.
Claim 17
Dependent Claim 25 words
A method according to claim 1, 8, 3 or 11 or wherein the panel inner face is dipped in the solution in the treating step.
Claim 18
Dependent Claim 39 words
A method according to claim 1, 8, 3 or 11 wherein the polymer coagulant comprises polyacrylamide, partially hydrolyzed salt of polyacrylamide, polyacrylic acid sodium salt, gelatin, polyalginic acid soda or carboxymethylcellulose, or a mixture of some of these substances.
Claim 19
Dependent Claim 29 words
A method according to claim 8 or 11 wherein the surfactant comprises polyoxyethylenealkyl ether, polyoxyethylenealkylphenol ether, alkylbetaine, or polyoxyethylene sulfate salt, or a mixture of some of these substances.
Claim 20
Dependent Claim 25 words
A method according to claim 9 or 11 wherein the treatment solution further contains 0.01 to 0.5 weight % of colloidal silica in said solution.
Claim 21
Dependent Claim 19 words
A method acording to claim 1 or 8 wherein said aqueous solution has a pH of 4.5 to 9.
Claim 22
Dependent Claim 13 words
A method according to claim 19 wherein the pH is 5.5 to 8.

References Cited (Backward Citations)

US3515553A Cited
US3269838A Cited
US3484240A Cited
US3981729A Cited
NL7803907A Cited
US4273842A Cited
JPS552201A Cited
US4293586A Cited
US4339475A Cited
US4324850A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-09-15 1990-03-17 1990-09-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-09-15 1994-03-17 1994-09-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-09-15 1998-03-17 1998-09-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag