← Back to Patent Explorer
US4611480A Expired / Lapsed US ⏱️ 0.0 years remaining

Metallic wall having knockouts and method of forming

Assignee: Allied Tube and Conduit Corp
•
Filing: 1984-04-12
•
Granted: 1986-09-16
•
Expires: 2004-04-12
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An elongated wall formed substantially of metallic material. The wall includes a first surface and a second surface spaced from the first surface. A plurality of spaced knockout portions are disposed in incipient apertures extending through the wall and these knockout portions are adapted to be selectively removed from the remainder of the wall by application of force to the portion to be removed. This force could be applied as by subjecting the knockout to a sharp blow directed to the portion. Each knockout portion so completely fills its corresponding aperture as to render the wall substantially impervious to the passage of fluid. The wall further comprises a coating applied to one of its surfaces. A method of forming the wall is also disclosed.

Inventors

  • 👤 Charles A. Willetts

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 13:18
CPC Classifications
B; B21; B21D; B21D28/00; B21D28/02; B21D28/10

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 331 words
A method of fabricating, from flat strip steel, galvanized tubing having a plurality of spaced knockout portions adapted for selective removal by the application of force to the portion to be removed, such as by applying a sharp blow to that portion, said method comprising the following steps: forming the knockout portions in said flat strip, each portion being defined, at least partially, by a plurality of lines of cleavage so that each knockout portion is attached to surrounding material by tab means, the forming step being carried out so that the passage of a fluid between the knockout portions and the remainder of said strip is precluded; transversely bending said strip until the lateral ends thereof abut; continuously welding said lateral ends together to form a tube; applying liquids to the outside surface of said tube to remove contaminants therefrom; rinsing the outside surface of said tube with water; drying the outside surface of said tube; and galvanizing the outside surface of said tube by passing said tube through a molten zinc bath, said step of forming knockout portions comprising the following substeps: striking said flat strip steel with cutting punch means for forming in said strip a plurality of lines of cleavage at least partially defining a knockout portion; displacing said portion, at least partially, from the remainder of said strip; applying sufficient forces to opposing surfaces of said knockout portion and said strip to move said knockout portion toward said strip and to close any opening therebetween to prevent the passage of a fluid between said knockout portion and said remainder of said strip; and repeating the aforementioned steps of striking, displacing and applying until formation of the desired number of knockout portions is completed, said steps of bending, welding, application of liquids, rinsing, drying and galvanizing being performed in a continuous rolling mill production line, said step of forming the knockout portions being completed off said production line with the strip being coiled after said forming step.
Claim 2
Independent Claim 331 words
A method of fabricating, from flat strip steel, galvanized tubing having a plurality of spaced knockout portions adapted for selective removal by the application of force to the portion to be removed, such as by applying a sharp blow to that portion, said method comprising the following steps: forming the knockout portions in said flat strip, each portion being defined, at least partially, by a plurality of lines of cleavage so that each knockout portion is attached to surrounding material by tab means, the forming step being carried out so that the passage of a fluid between the knockout portions and the remainder of said strip is precluded; transversely bending said strip until the lateral ends thereof abut; continuously welding said lateral ends together to form a tube; applying liquids to the outside surface of said tube to remove contaminants therefrom; rinsing the outside surface of said tube with water; drying the outside surface of said tube; and galvanizing the outside surface of said tube by passing said tube through a molten zinc bath, said step of forming knockout portions comprising the following substeps: striking said flat strip steel with cutting punch means for forming in said strip a plurality of lines of cleavage at least partially defining a knockout portion; displacing said portion, at least partially, from the remainder of said strip; applying sufficient forces to opposing surfaces of said knockout portion and said strip to move said knockout portion toward said strip and to close any opening therebetween to prevent the passage of a fluid between said knockout portion and said remainder of said strip; and repeating the aforementioned steps of striking, displacing and applying until formation of the desired number of knockout portions is completed, said steps of bending, welding, application of liquids, rinsing, drying and galvanizing being performed in a continuous rolling mill production line, said step of forming the knockout portions being completed off said production line with the strip being coiled after said forming step.
Claim 3
Dependent Claim 41 words
The method as set forth in claim 1 further comprising the step of applying a protective coating to the inside of said tube, the last-mentioned step to be performed prior to the step of applying liquids to the outside tube surface.

References Cited (Backward Citations)

US2114289A Cited
FR1181683A Cited
GB998190A Cited
US3266051A Cited
US3580122A Cited
US3827139A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-09-15 1990-03-17 1990-09-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-09-15 1994-03-17 1994-09-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-09-15 1998-03-17 1998-09-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag