Abstract

Abstract A method of coating testing comprises applying a consistantly perpendicular minimum tension force to a dolly for testing to see if the adhesive bond strength between a coating and a substrate meets a minimum specification for such bond. The tester comprises a ram passing through an axially centered opening in a dolly bonded to the coating. A piston and cylinder are associated with the ram and the dolly so that pressure within the piston chamber formed thereby causes the development of a tension force within the dolly which is perpendicular to the coating being tested because of the coaxially centered orientation of the dolly with respect to the ram. The pressure is increased only to a point wherein the tension force is equal to a minimum specification for bonding adhesion. If the coating has not separated from the substrate, the bond therebetween meets the specification. The testing apparatus may then be removed by causing the bonding agent attaching the dolly to the coating to fail as by heating.

Inventors

  • 👤 William H. Thomason
  • 👤 Randall G. Ivie

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 21:19
CPC Classifications
G; G01; G01N; G01N19/00; G01N19/04; G01N2203/00; G01N2203/02; G01N2203/026; G01N2203/0262; G01N2203/0278; G01N2203/0282

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 134 words
A method of testing an adhesive bond of a coating to a substrate to meet a minimum specification in a tensile mode comprising the steps of providing a dolly having an axially centered opening therethrough; bonding the dolly to the coating with bonding means having a bond strength in excess of an adhesive bond strength of an adhesive bond between the coating and the substrate; attaching piston and cylinder means to the dolly, the piston and cylinder means including an axially centered ram, the ram passing through the axially centered opening of the dolly; applying pressure to the piston and cylinder means to force the ram into pressure engagement against the coating and increasing the pressure to a predetermined monitored pressure at which a tensile force developed in the dolly meets the minimum specification.
Claim 2
Independent Claim 134 words
A method of testing an adhesive bond of a coating to a substrate to meet a minimum specification in a tensile mode comprising the steps of providing a dolly having an axially centered opening therethrough; bonding the dolly to the coating with bonding means having a bond strength in excess of an adhesive bond strength of an adhesive bond between the coating and the substrate; attaching piston and cylinder means to the dolly, the piston and cylinder means including an axially centered ram, the ram passing through the axially centered opening of the dolly; applying pressure to the piston and cylinder means to force the ram into pressure engagement against the coating and increasing the pressure to a predetermined monitored pressure at which a tensile force developed in the dolly meets the minimum specification.
Claim 3
Dependent Claim 25 words
The method as set forth in claim 1 further including the step of removing the piston and cylinder means and the ram from the dolly.
Claim 4
Dependent Claim 24 words
The method as set forth in claim 2 further including the step of causing said bonding means to fail following completion of the testing.
Claim 5
Dependent Claim 23 words
The method as set forth in claim 3 wherein said step of causing said bonding means to fail comprises heating said bonding means.
Claim 6
Dependent Claim 28 words
The method as set forth in claim 4 wherein the step of heating said bonding means comprises heating said dolly at a point remote from said bonding means.
Claim 7
Dependent Claim 35 words
The method as set forth in claim 3 wherein said step of causing said bonding means to fail comprises striking said dolly such that an impact from the striking causes the bonding means to shatter.
Claim 8
Dependent Claim 26 words
The method as set forth in claim 3 wherein said step of causing said bonding means to fail comprises solvating said bonding means with a solvent.

References Cited (Backward Citations)

US2711775A Cited
US3527093A Cited
US3577775A Cited
US3628378A Cited
US3821892A Cited
US4381248A Cited
US4413510A Cited
US4487643A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-08-18 1990-02-17 1990-08-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-08-18 1994-02-17 1994-08-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-08-18 1998-02-17 1998-08-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag