Abstract

Abstract Through a pattern mask, small sections of a semiconductor wafer are exposed successively to light radiated from a mercury-vapor lamp in high-level steps, during each of which the power consumption and discharge current of the mercury-vapor lamp are at a high level, by continuously lighting the mercury-vapor lamp and repeatedly alternating each of the high-level steps and a low-level step during which the power consumption and discharge current of the mercury-vapor lamp are at a low level. The alternation of the high-level step and low-level step is effected while controlling the magnitude of each of the overshoot and undershoot in the waveform of the discharge current for the mercury-vapor lamp below 10%. The exposure method of this invention is effective in avoiding or minimizing the wearing of electrodes of a mercury-vapor lamp. Thus, the mercury-vapor lamp can enjoy long service life while permitting stable exposure over a long period of time.

Inventors

  • 👤 Takehiro Kira

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 11:42
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/70; G03F7/70008; G03F7/70016; G03F7/70483; G03F7/7055; G03F7/70558

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 179 words
In a method for exposing, through a pattern mask, small sections of a semiconductor wafer successively to light radiated from a mercury-vapor lamp in highlevel steps, during each of which the power consumption and discharge current of the mercury-vapor lamp are at a high level, by continuously lighting the mercury-vapor lamp and repeatedly alternating each of the high-level steps and a low-level step during which the power consumption and discharge current of the mercury-vapor lamp are at a low level, wherein the discharge current of the mercury-vapor lamp overshoots the discharge current of the high-level step when the mercury-vapor lamp is switched from the low-level step to the high-level step and undershoots the discharge current of the low-level step when the mercury-vapor lamp is switched from the high-level step to the low-level step, the improvement comprising effecting the alternation of the high-level step and low-level step while limiting the magnitude of each of the overshoot and undershoot to below 10% of the difference between the discharge current in the high-level step and the discharge current in the low-level step.
Claim 2
Dependent Claim 179 words
In a method for exposing, through a pattern mask, small sections of a semiconductor wafer successively to light radiated from a mercury-vapor lamp in highlevel steps, during each of which the power consumption and discharge current of the mercury-vapor lamp are at a high level, by continuously lighting the mercury-vapor lamp and repeatedly alternating each of the high-level steps and a low-level step during which the power consumption and discharge current of the mercury-vapor lamp are at a low level, wherein the discharge current of the mercury-vapor lamp overshoots the discharge current of the high-level step when the mercury-vapor lamp is switched from the low-level step to the high-level step and undershoots the discharge current of the low-level step when the mercury-vapor lamp is switched from the high-level step to the low-level step, the improvement comprising effecting the alternation of the high-level step and low-level step while limiting the magnitude of each of the overshoot and undershoot to below 10% of the difference between the discharge current in the high-level step and the discharge current in the low-level step.
Claim 3
Dependent Claim 67 words
A method as claimed in claim 1, wherein a shutter is opened and then closed only once during the period of each of the high-level steps so as to expose the corresponding one of the small sections of the semiconductor wafer at an exposure position and while the shutter is closed, the semiconductor wafer is shifted stepwise to place the next small section at the exposure position.
Claim 4
Dependent Claim 63 words
A method as claimed in claim 1, wherein the level of the power consumption in each of the low-level steps is substantially equal to the rated power consumption of the mercury-vapor lamp and the level of the power consumption in each of the high-level steps is within the range of from 1.3 to 2.5 times the rated power consumption of the mercury-vapor lamp.
Claim 5
Dependent Claim 39 words
A method as claimed in claim 1, wherein the the high-level steps are repeated while increasing the power consumption little by little so as to compensate the reduction of the quantity to be radiated along the passage of time.
Claim 6
Dependent Claim 123 words
In a method for exposing, through a pattern mask, small sections of a semiconductor wafer successively to light radiated from a mercury-vapor lamp in high-level steps, during each of which the power consumption of the mercury-vapor lamp is at a high level, by continuously lighting the mercury-vapor lamp and repeatedly alternating each of the high-level steps and a low-level step during which the power consumption of the mercury-vapor lamp is at a low level, the improvement comprising the switch-over from each low-level step to its subsequent high-level step being carried out in such a way that the power consumption of the mercury-vapor lamp reaches 95% of the power consumption in the high-level step within a period ranging from 1 msec. to 30 msec.
Claim 7
Dependent Claim 123 words
In a method for exposing, through a pattern mask, small sections of a semiconductor wafer successively to light radiated from a mercury-vapor lamp in high-level steps, during each of which the power consumption of the mercury-vapor lamp is at a high level, by continuously lighting the mercury-vapor lamp and repeatedly alternating each of the high-level steps and a low-level step during which the power consumption of the mercury-vapor lamp is at a low level, the improvement comprising the switch-over from each low-level step to its subsequent high-level step being carried out in such a way that the power consumption of the mercury-vapor lamp reaches 95% of the power consumption in the high-level step within a period ranging from 1 msec. to 30 msec.
Claim 8
Dependent Claim 226 words
In a method for exposing, through a pattern mask, small sections of a semiconductor wafer successively to light radiated from a mercury-vapor lamp in high-level steps, during each of which the power consumption and discharge current of the mercury-vapor lamp are at a high level, by continuously lighting the mercury-vapor lamp and repeatedly alternating each of the high-level steps and a low-level step during which the power consumption and discharge current of the mercury-vapor lamp are at a low level, wherein the discharge current of the mercury-vapor lamp over-shoots the discharge current of the high-level step when the mercury-vapor lamp is switched from the low-level step to the high-level step and undershoots the discharge current of the low-level step when the mercury-vapor lamp is switched from the high-level step to the low-level step, the improvement comprising effecting the alternation of the high-level step and low-level step while limiting the magnitude of each of the overshoot and undershoot to below 10% of the difference between the discharge current in the high-level step and the discharge current in the low-level step, and the switch-over from each low-level step to its subsequent high-level step is carried out in such a way that the power consumption of the mercury-vapor lamp reaches 95% of the power consumption in the high-level step within a period ranging from 1 msec. to 30 msec.
Claim 9
Dependent Claim 226 words
In a method for exposing, through a pattern mask, small sections of a semiconductor wafer successively to light radiated from a mercury-vapor lamp in high-level steps, during each of which the power consumption and discharge current of the mercury-vapor lamp are at a high level, by continuously lighting the mercury-vapor lamp and repeatedly alternating each of the high-level steps and a low-level step during which the power consumption and discharge current of the mercury-vapor lamp are at a low level, wherein the discharge current of the mercury-vapor lamp over-shoots the discharge current of the high-level step when the mercury-vapor lamp is switched from the low-level step to the high-level step and undershoots the discharge current of the low-level step when the mercury-vapor lamp is switched from the high-level step to the low-level step, the improvement comprising effecting the alternation of the high-level step and low-level step while limiting the magnitude of each of the overshoot and undershoot to below 10% of the difference between the discharge current in the high-level step and the discharge current in the low-level step, and the switch-over from each low-level step to its subsequent high-level step is carried out in such a way that the power consumption of the mercury-vapor lamp reaches 95% of the power consumption in the high-level step within a period ranging from 1 msec. to 30 msec.

References Cited (Backward Citations)

US4024428A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-08-11 1990-02-10 1990-08-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-08-11 1994-02-10 1994-08-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-08-11 1998-02-10 1998-08-12 $7700.00 Window Closed / Lapsed