Method for making a thin-film humidity sensor for measuring absolute humidity

Assignee: GENERAL EASTERN INSTRUMENTS Inc
•
Filing: 1985-04-19
•
Granted: 1986-08-05
•
Expires: 2005-04-19
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A thin-film humidity sensor for measuring the absolute humidity having a base electrode, a moisture-sensitive dielectric layer and a top electrode is formed at the end face of an electrically insulating bushing body by the thin-film technique. The connecting conductors are led through the bushing body and terminate in contact areas which are ground plane and polished together with the end face of the bushing body. The metal layers forming the electrodes are so shaped on application, preferably by means of perforated masks, that they each cover the contact area of the associated connecting conductor and are electrically connected thereto. The bushing body is inserted into a sleeve of a highly alloyed nickel-molybdenum compound and connected thereto in pressure-resistant manner.

Inventors

  • 👤 Wolfgang Woest
  • 👤 Rainer Silbermann
  • 👤 Frank Hegner

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 11:45
CPC Classifications
G; G01; G01N; G01N27/00; G01N27/02; G01N27/22; G01N27/223; G01N27/225; Y; Y10; Y10T; Y10T29/00; Y10T29/43; Y10T29/435; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49169

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 244 words
Method of making a thin-film humidity sensor for measuring absolute humidity, characterized in that in a bushing body (14) of electrically insulating material at least two axial bores (22, 24) are formed spaced apart from each other which widen towards the end face of the bushing body (14), that in each bore a lead-through conductor (18) is disposed so that it projects into the widening (26, 28), that each lead-through conductor (18, 20) is connected to the bushing body (14) by means of brazing solder (30, 32) which fills the widening (26, 28), that the end face (34) of the bushing body (14) together with the brazing solder (30, 32) disposed in each widening (26, 28) is ground plane and polished, that to a portion of the end face (34) a metal layer forming the base electrode (40) is applied so that said layer is electrically connected to the brazing solder (30) disposed in a widening (26) and does not cover the brazing solder (32) disposed in another widening (28), that on the metal layer (40) a moisture-sensitive dielectric layer (42) is formed, and that a further metal layer forming the top electrode (44) is applied to the portion of the end face (34) not covered by the base electrode (40) and to at least a portion of the moisture-sensitive layer (42) in such a manner that said further layer is electrically connected to the brazing solder (32) disposed in the other widening (28).
Claim 2
Dependent Claim 244 words
Method of making a thin-film humidity sensor for measuring absolute humidity, characterized in that in a bushing body (14) of electrically insulating material at least two axial bores (22, 24) are formed spaced apart from each other which widen towards the end face of the bushing body (14), that in each bore a lead-through conductor (18) is disposed so that it projects into the widening (26, 28), that each lead-through conductor (18, 20) is connected to the bushing body (14) by means of brazing solder (30, 32) which fills the widening (26, 28), that the end face (34) of the bushing body (14) together with the brazing solder (30, 32) disposed in each widening (26, 28) is ground plane and polished, that to a portion of the end face (34) a metal layer forming the base electrode (40) is applied so that said layer is electrically connected to the brazing solder (30) disposed in a widening (26) and does not cover the brazing solder (32) disposed in another widening (28), that on the metal layer (40) a moisture-sensitive dielectric layer (42) is formed, and that a further metal layer forming the top electrode (44) is applied to the portion of the end face (34) not covered by the base electrode (40) and to at least a portion of the moisture-sensitive layer (42) in such a manner that said further layer is electrically connected to the brazing solder (32) disposed in the other widening (28).
Claim 3
Dependent Claim 27 words
Method according to claim 1, characterized in that prior to the application of the metal layer forming the base electrode (40) a diffusion barrier layer is applied.
Claim 4
Dependent Claim 32 words
Method according to claim 1, characterized in that at least to a portion of the metal layer forming the top electrode (44) a further metal layer (46) is applied for contact intensification.
Claim 5
Dependent Claim 24 words
Method according to claim 1, characterized in that the layers (40, 42, 44, 46) of the moisture-sensitive system are formed by the thin-film technique.
Claim 6
Dependent Claim 19 words
Method according to claim 4, characterized in that the metal layers (40, 44, 46) are applied by cathode sputtering.
Claim 7
Dependent Claim 17 words
Method according to claim 4, characterized in that the metal layers (40, 44, 46) are vapor deposited.
Claim 8
Dependent Claim 23 words
Method according to claim 4, characterized in that the shaping of the metal layers (40, 44, 46) is by application through perforated masks.
Claim 9
Dependent Claim 40 words
Method according to claim 1, characterized in that the metal layer forming the base electrode (40) is made from aluminum and that the moisture-sensitive dielectric layer (42) is produced by anodic oxidation of the surface of the aluminum layer (40).

References Cited (Backward Citations)

US3317983A Cited
US4528613A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-08-04 1990-02-03 1990-08-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-08-04 1994-02-03 1994-08-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-08-04 1998-02-03 1998-08-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag