Abstract
Abstract The invention provides a method for the preparation of a shaped article of a flexible or semi-rigid polyvinyl chloride resin having a metallized surface, of which the adhesive bonding of the metallizing layer to the substrate surface is greatly improved. In the inventive method, the surface of the shaped article is first exposed to low temperature plasma generated in an atmosphere containing a vapor of a specified organosilicon compound before the metallizing treatment in a dry process such as vacuum vapor deposition, ion plating and the like.
Inventors
- 👤 Susumu Ueno
- 👤 Hirokazu Nomura
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-01 19:55
CPC Classifications
C; C08; C08J; C08J7/00; C08J7/12; C08J7/123; C23; C23C; C23C14/00; C23C14/02; C23C14/021; C23C14/022; C08J2327/00; C08J2327/02; C08J2327/04; C08J2327/06
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
105 words
A method for the preparation of a shaped article of a flexible or semi-rigid polyvinyl chloride resin with a metallized surface which comprises the steps of: (a) subjecting the surface of a shaped article of a flexible or semi-rigid polyvinyl chloride resin to exposure to low temperature plasma generated in an atmosphere containing a vapor of an organosilicon compound under a pressure in the range from 0.001 to 10 Torr to deposit a polymerized layer of the organosilicon compound on the surface; and (b) metallizing the surface of the shaped article thus coated with the polymerized layer of the organosilicon compound in a dry process.
Claim 2
Independent Claim
105 words
A method for the preparation of a shaped article of a flexible or semi-rigid polyvinyl chloride resin with a metallized surface which comprises the steps of: (a) subjecting the surface of a shaped article of a flexible or semi-rigid polyvinyl chloride resin to exposure to low temperature plasma generated in an atmosphere containing a vapor of an organosilicon compound under a pressure in the range from 0.001 to 10 Torr to deposit a polymerized layer of the organosilicon compound on the surface; and (b) metallizing the surface of the shaped article thus coated with the polymerized layer of the organosilicon compound in a dry process.
Claim 3
Dependent Claim
84 words
The method as claimed in claim 1 wherein the organosilicon compound is an organosilane represented by the general formula R a H b SiX 4-a-b , in which R is a substituted or unsubstituted monovalent hydrocarbon group, X is a halogen atom or an alkoxy group, the suffix a is a number of zero, 1, 2 or 3 and the suffix b is a number of zero or 1 with the proviso that a+b does not exceed 3, or a partial hydrolysis-condensation product thereof.
Claim 4
Dependent Claim
30 words
The method as claimed in claim 1 wherein the step (a) is preceded by a low temperature plasma treatment of the shaped article in an atmosphere of an inorganic gas.
Claim 5
Dependent Claim
41 words
The method as claimed in claim 3 wherein the inorganic gas is selected from the class consisting of helium, neon, argon, nitrogen, oxygen, air, nitrous oxide, nitrogen monoxide, nitric oxide, carbon monoxide, carbon dioxide, bromine cyanide, sulfur dioxide and hydrogen sulfide.
Claim 6
Dependent Claim
23 words
The method as claimed in claim 1 wherein the polymerized layer of the organosilicon compound has a thickness of at least 5 nm.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1989-07-28 | 1990-01-27 | 1990-07-29 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1993-07-28 | 1994-01-27 | 1994-07-29 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1997-07-28 | 1998-01-27 | 1998-07-29 | $7700.00 | Window Closed / Lapsed |