Claims Analysis
Total Claims: 22
Claim 1
Independent Claim
101 words
The method of preparing a polyimide coating composition which comprises the steps of: mixing an aromatic dianhydride with an oxoimine having the general formula: ##STR2## where x is an integer from 4 to 7 in a mole ratio of oxomine to dianhydride between about 0.01:1 and 10:1 to produce a carboxy terminated bisimide; dissolving said imide in a solvent which renders the resulting solution water soluble; adding sufficient water to make at least a 10 wt. % water solution adding thereto aromatic diamine; and adding thereto from about 2 to 20% of the weight of the water of a tertiary amine.
Claim 2
Independent Claim
101 words
The method of preparing a polyimide coating composition which comprises the steps of: mixing an aromatic dianhydride with an oxoimine having the general formula: ##STR2## where x is an integer from 4 to 7 in a mole ratio of oxomine to dianhydride between about 0.01:1 and 10:1 to produce a carboxy terminated bisimide; dissolving said imide in a solvent which renders the resulting solution water soluble; adding sufficient water to make at least a 10 wt. % water solution adding thereto aromatic diamine; and adding thereto from about 2 to 20% of the weight of the water of a tertiary amine.
Claim 3
Dependent Claim
48 words
The method according to claim 1 wherein said solvent is selected from the group consisting of ethylene glycol monoethyl ether, ethylene glycol monoethyl ether, ethylene glycol monobutyl ether, ethylene glycol monoethyl ether acetate, ethylene glycol monoethyl ether acetate, ethylene glycol monobutyl ether acetate ethylene glycol and mixtures thereof.
Claim 4
Dependent Claim
20 words
The method according to claim 1 wherein said solvent is ethylene glycol monobutyl ether or ethylene glycol monoethyl ether acetate.
Claim 5
Dependent Claim
22 words
The method according to claim 1 wherein said aromatic dianhydride is either 3,3',4,4'-benzophenone tetracarboxylic acid dianhydride, pyromellitic dianhydride or a mixture thereof.
Claim 6
Dependent Claim
13 words
The method according to claim 1 wherein said aliphatic dianhydride is 1,2,3,4-butanetetracarboxylic acid
Claim 7
Dependent Claim
11 words
The method according to claim 1 wherein said oxoimine is caprolactam.
Claim 8
Dependent Claim
21 words
The method according to claim 1 wherein the number of moles of diamine is substantially equal to the moles of dianhydride.
Claim 9
Dependent Claim
15 words
The method according to claim 1 wherein said diamine is 4,4'-diaminophenyl ether or 4,4'-diaminodiphenyl methane.
Claim 10
Dependent Claim
19 words
The method according to claim 1 wherein said tertiary amine is N-methyl morpholine, triethyl amine or a mixture thereof.
Claim 11
Dependent Claim
20 words
The method according to claim 1 wherein up to about 50 mole % of said dianhydride is an aliphatic dianhydride.
Claim 12
Dependent Claim
21 words
The method according to claim 1 wherein at least some of said aromatic diamine has an aliphatic moiety in the molecule.
Claim 13
Dependent Claim
105 words
An imide coating composition comprising a mixture of: an oxoimine having the general formula ##STR3## where X is an integer from 4 to 7; from about 0.1 to 10.0 moles of a dianhydride per mole of oxoimine; from about 2 to 20 moles of a water soluble solvent per mole of oxoimine; an aromatic diamine present in a molar quantity substantially equal to the sum of the moles of said dianhydride; sufficient water to produce a solution having from about 10 to 80 wt. % water; and a tertiary amine in a quantity equal to about 2 to 20% of the weight of the water.
Claim 14
Dependent Claim
105 words
An imide coating composition comprising a mixture of: an oxoimine having the general formula ##STR3## where X is an integer from 4 to 7; from about 0.1 to 10.0 moles of a dianhydride per mole of oxoimine; from about 2 to 20 moles of a water soluble solvent per mole of oxoimine; an aromatic diamine present in a molar quantity substantially equal to the sum of the moles of said dianhydride; sufficient water to produce a solution having from about 10 to 80 wt. % water; and a tertiary amine in a quantity equal to about 2 to 20% of the weight of the water.
Claim 15
Dependent Claim
50 words
The composition according to claim 12 wherein said water soluble solvent is selected from the group consisting of ethylene glycol monoethyl ether, ethylene glycol monoethyl ether, ethylene glycol monobutyl ether, ethylene glycol monoethyl ether acetate, ethylene glycol monoethyl ether acetate, ethylene glycol monobutyl ether acetate, ethylene glycol and mixtures thereof.
Claim 16
Dependent Claim
26 words
The composition according to claim 12 wherein sai tertiary amine is selected from the group consisting of N-methyl morpholine, triethyl amine, methyl pyridine and mixtures thereof.
Claim 17
Dependent Claim
19 words
The composition according to claim 12 wherein said dianhydride is 3,3',4,4'-benzophenone tetracarboxylic acid dianhydride, pyromellitic dianhydride or mixtures thereof.
Claim 18
Dependent Claim
11 words
The composition according to claim 12 wherein said oxoimine is caprolactam.
Claim 19
Dependent Claim
41 words
The coating according to claim 12 wherein said aromatic diamine is selected from the group consisting of 4,4' p-Phenylenediisopropylidene bisaniline; 4,4' diamino diphenyl ether; 4,4' diamino diphenyl methane; 1,4' diamino benzene; 1,3' diamino benzene; 4,4' diamino diphenyl sulfone and mixtures thereof.
Claim 20
Dependent Claim
34 words
The composition according to claim 12 wherein said dianhydride is a mixture of an aromatic dianhydride and an aliphatic dianhydride with up to about 50 mole % of said mixture being the aliphatic dianhydride.
Claim 21
Dependent Claim
46 words
A method of producing a polyimide coating which comprises the steps of: applying a substantially uniform coating of the composition of claim 1 to a surface; heating said coating to a temperature of from about 176.6° to 316° C. for from about 5 to 60 min.
Claim 22
Dependent Claim
40 words
The method according to claim 19 further including a step prior to said heating step of drying said coating by heating said coating to a temperature of from about 90° to 150° C. for from about 10 to 60 minutes.