Claims Analysis
Total Claims: 18
Claim 1
Independent Claim
158 words
The process for combusting sulfur-containing coal while producing of off-gas low in sulfur which comprises combusting particulate coal in a furnace burner cavity providing rapid coal combustion, a hot, turbulent combustion zone and a combustion temperature of at least about 1100° C. in the presence of a finely divided sulfur-fixing material from the group consisting of iron oxide, iron powder and copper oxide in amounts about 25% to about 100% in excess of the stoichiometric quantity required to produce metal sulfide based on the sulfur content of said coal distributed throughout said combustion zone and at least about 60% of the oxygen stoichiometrically required for complete combustion of said coal to form a particulate liquid oxysulfide phase within a turbulent atmosphere of combustion-product gases, said liquid oxysulfide acting to scrub sulfur-containing gaseous species from said atmosphere to yield an essentially sulfur-free flue gas and a liquid oxysulfide slag containing essentially all the sulfur originally contained in said coal.
Claim 2
Dependent Claim
158 words
The process for combusting sulfur-containing coal while producing of off-gas low in sulfur which comprises combusting particulate coal in a furnace burner cavity providing rapid coal combustion, a hot, turbulent combustion zone and a combustion temperature of at least about 1100° C. in the presence of a finely divided sulfur-fixing material from the group consisting of iron oxide, iron powder and copper oxide in amounts about 25% to about 100% in excess of the stoichiometric quantity required to produce metal sulfide based on the sulfur content of said coal distributed throughout said combustion zone and at least about 60% of the oxygen stoichiometrically required for complete combustion of said coal to form a particulate liquid oxysulfide phase within a turbulent atmosphere of combustion-product gases, said liquid oxysulfide acting to scrub sulfur-containing gaseous species from said atmosphere to yield an essentially sulfur-free flue gas and a liquid oxysulfide slag containing essentially all the sulfur originally contained in said coal.
Claim 3
Dependent Claim
29 words
The process in accordance with claim 1 wherein said liquid oxysulfide is iron oxysulfide and is controlled essentially to the proportions FeO x S y wherein 1<x<1.33 and o<y<1.
Claim 4
Dependent Claim
27 words
The process in accordance with claim 1 wherein said liquid oxysulfide slag is removed from contact with said combustion-product gas before said oxysulfide is saturated with sulfur.
Claim 5
Dependent Claim
17 words
The process in accordance with claim 1 wherein said burner cavity is provided in a flash furnace.
Claim 6
Dependent Claim
18 words
The process in accordance with claim 1 wherein said burner cavity is provided in a cyclone type furnace.
Claim 7
Dependent Claim
92 words
The process in accordance with claim 1 wherein the temperature within said furnace atmosphere is at least about 1100° C. and the ratios of coal feed, oxygen feed and sulfur-fixing material feed are controlled by measuring the contents of carbon dioxide and carbon monoxide, and controlling the ratio of carbon dioxide and carbon monoxide to maintain within said burner cavity a liquid oxysulfide phase and an atmosphere of reduced sulfur content in contact with said phase; and removing said liquid oxysulfide from said burner cavity before said oxysulfide becomes saturated with sulfur.
Claim 8
Dependent Claim
22 words
The process in accordance with claim 1 wherein said coal and sulfur-fixing material are uniformly mixed before being fed to said furnace.
Claim 9
Dependent Claim
14 words
The process in accordance with claim 1 wherein said oxygen is supplied as air.
Claim 10
Dependent Claim
15 words
The process in accordance with claim 1 wherein said iron oxide is supplied as taconite.
Claim 11
Dependent Claim
20 words
The process in accordance with claim 1 wherein said sulfur-fixing material is iron powder and said oxysulfide is iron oxysulfide.
Claim 12
Dependent Claim
20 words
The process in accordance with claim 1 wherein said sulfur-fixing material is iron oxide and said oxysulfide is iron oxysulfide.
Claim 13
Dependent Claim
14 words
The process in accordance with claim 1 wherein said sulfur-fixing material is copper oxide.
Claim 14
Dependent Claim
26 words
The process in accordance with claim 6 wherein said liquid oxysulfide is removed from said combustion zone by deposition upon the walls of said burner cavity.
Claim 15
Dependent Claim
18 words
The process in accordance with claim 13 wherein ash present in said coal is codeposited with said oxysulfide.
Claim 16
Independent Claim
169 words
The method for combusting sulfur-containing coal while producing a substantially sulfur-free combustion-product gas and fixing essentially all the sulfur content of said coal in a sulfidic slag which comprises mixing the sulfur-containing coal to be combusted with a finely-divided sulfur-fixing material from the group consisting of iron oxide, iron powder and copper oxide, said sulfur-fixing material being stoichiometrically in excess of the sulfur content of said coal and combusting said mixture along with at least about 60% of the oxygen stoichiometrically required for complete combustion of said coal in a turbulent combustion zone at a temperature of about 1100° C. to about 1500° C. wherein high combustion gas velocities are maintained and wherein the particles of said sulfur-fixing material rapidly incandesce and react with gaseous sulfur species in said combustion gas to form a myriad of liquid oxysulfide particles which scrub sulfur-containing species from said combustion zone to yield an essentially sulfur-free combustion-product gas and a liquid oxysulfide slag containing essentially all the sulfur originally contained in said coal.
Claim 17
Independent Claim
169 words
The method for combusting sulfur-containing coal while producing a substantially sulfur-free combustion-product gas and fixing essentially all the sulfur content of said coal in a sulfidic slag which comprises mixing the sulfur-containing coal to be combusted with a finely-divided sulfur-fixing material from the group consisting of iron oxide, iron powder and copper oxide, said sulfur-fixing material being stoichiometrically in excess of the sulfur content of said coal and combusting said mixture along with at least about 60% of the oxygen stoichiometrically required for complete combustion of said coal in a turbulent combustion zone at a temperature of about 1100° C. to about 1500° C. wherein high combustion gas velocities are maintained and wherein the particles of said sulfur-fixing material rapidly incandesce and react with gaseous sulfur species in said combustion gas to form a myriad of liquid oxysulfide particles which scrub sulfur-containing species from said combustion zone to yield an essentially sulfur-free combustion-product gas and a liquid oxysulfide slag containing essentially all the sulfur originally contained in said coal.
Claim 18
Dependent Claim
15 words
The method in accordance with claim 15 wherein the gas containing said oxygen is preheated.