Abstract

Abstract This invention relates to a mixture of from 60 to 95% by weight of a diglycidyl ester of hexahydrophthalic acids and from 5 to 40% by weight of 3,4-epoxycyclohexylmethyl-3,4-epoxycyclohexane carboxylate. In combination with conventional polycarboxylic acid anhydrides as hardeners, this mixture is used for the production of molded bodies with excellent weathering resistance, good electrical properties and surprisingly good mechanical properties.

Inventors

  • 👤 Frank Kleiner
  • 👤 Rolf Kubens
  • 👤 Heinrich Heine

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 06:14
CPC Classifications
C; C08; C08G; C08G59/00; C08G59/18; C08G59/20; C08G59/22; C08G59/226

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 22 words
A mixture comprising: 60-95% by weight of at least one diglycidyl ester of hexahydrophthalic acid, and 5-40% by weight of 3,4-epoxycyclohexylmethyl-3,4-epoxycyclohexane carboxylate.
Claim 2
Dependent Claim 22 words
A mixture comprising: 60-95% by weight of at least one diglycidyl ester of hexahydrophthalic acid, and 5-40% by weight of 3,4-epoxycyclohexylmethyl-3,4-epoxycyclohexane carboxylate.
Claim 3
Dependent Claim 27 words
A mixture as claimed in claim 1, comprising: 70-95% by weight of at least one diglycidyl ester of hexahydrophthalic acid, and 5-30% by weight of 3,4-epoxycyclohexylmethyl-3,4-epoxycyclohexane carboxylate.
Claim 4
Dependent Claim 64 words
A process for the production of molded epoxide resin products, which comprises hardening a mixture as claimed in claim 1 with from 0.6 to 1.2 anhydride equivalents of a polycarboxylic acid anhydride per epoxide equivalent at a temperature of from 60° to 180° C., optionally under excess pressure and optionally in the presence of a conventional hardening accelerator, filler, dye, pigment or reinforcing material.
Claim 5
Dependent Claim 19 words
A process as claimed in claim 3, wherein from 0.9 to 1.1 anhydride equivalents are used per epoxide equivalent.

References Cited (Backward Citations)

US3511922A Cited
US4336367A Cited
US3764584A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-04-07 1989-10-07 1990-04-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-04-07 1993-10-07 1994-04-08 $3760.00 Window Closed / Lapsed