Voltage-dependent resistor and method of manufacturing same
Abstract
Abstract A voltage-dependent resistor having a low operational field strength with a ceramic sintered body on the basis of a polycrystalline alkaline earth metal titanate doped with a small quantity of a metal oxide so as to produce an N-type conductivity, in which the sintered body comprises at its grain boundaries insulating layers formed by in-diffusion of at least a metal oxide or at least a metal oxide compound and comprises of an alkaline earth metal titanate having Perowskite structure of the general formula: (A.sub.1-x Ln.sub.x)TiO.sub.3.yTiO.sub.2 or A(Ti.sub.1-x Me x )O 3 .yTiO 2 wherein: A=alkaline earth metal; Ln=rare earth metal; Me=metal having a valency of 5 or more; 0.0005<x<solubility limit in the Perowskite phase; y=0.001 to 0.02. The insulating layers are formed in that the sintered body is covered on its surface with a suspension containing at least a metal oxide having a comparatively low melting-point as compared with the sintered body or at least a metal oxide compound having a comparatively low melting-point with respect to the sintered body and is tempered in an oxidizing atmosphere at a temperature which is above the melting-point of the suspension component(s).
Inventors
- 👤 Detlev Hennings
- 👤 Axel Schnell
- 👤 Herbert Schreinemacher
Bibliographic Details
Claims Analysis
Total Claims: 9References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1989-04-07 | 1989-10-07 | 1990-04-08 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1993-04-07 | 1993-10-07 | 1994-04-08 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1997-04-07 | 1997-10-07 | 1998-04-08 | $7700.00 | Window Closed / Lapsed |