Method of producing a strip having a non-uniform cross section by a rolling process

Assignee: Hitachi Cable Ltd
•
Filing: 1983-08-26
•
Granted: 1986-04-01
•
Expires: 2003-08-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for producing a strip of material having a non-uniform cross section is carried out by passing a strip of material in the longitudinal direction through a first set of working rolls, at least one of which is provided with an annular slot intermediate the ends thereof so that a reducing force is applied only to those portions of the strip engaging said roll on opposite sides of the slot whereby the excess material flows toward that portion of the strip opposed to the slot to cause the strip to buckle outwardly into the slot. The strip is subsequently passed through a set of smooth rolls to flatten the buckled portion. This procedure is repeated any desired number of times with the width of the slot becoming progressively smaller. The strip may then be passed through one or more sets of finishing rolls and a heating and annealing operation can take place before each passage through a set of finishing rolls.

Inventors

  • 👤 Hajime Abe
  • 👤 Noboru Hagiwara
  • 👤 Kazuo Ishida
  • 👤 Tadao Otani
  • 👤 Osamu Kawamata
  • 👤 Manabu Kagawa

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 01:41
CPC Classifications
B; B21; B21B; B21B1/00; B21B1/08; B21B1/0805

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 181 words
A method for shaping a substantially continuous strip of material having a substantially uniform cross section into a substantially continuous strip having a non-uniform cross section defined by at least one thick section and two thin sections on opposite sides of said thick section, comprising the steps of: passing said continuous strip having a substantially uniform cross section in the longitudinal direction through a first pair of reduction rolls, at least one of which has an annular slot intermediate the ends thereof, to provide a reducing force to reduce the thickness of only those portions of said strip engaging said roll on opposite sides of said slot, said passing step including the provision of sufficient reducing force on said engaging portions of said strip to cause the unengaged portion of said strip to form a buckled portion in said slot, and passing the strip coming through said first pair of rolls through a second pair of reduction rolls, each having a smooth cylindrical surface, to roll said buckled portion to a predetermined thickness, thicker than the remaining portions of said strip.
Claim 2
Independent Claim 181 words
A method for shaping a substantially continuous strip of material having a substantially uniform cross section into a substantially continuous strip having a non-uniform cross section defined by at least one thick section and two thin sections on opposite sides of said thick section, comprising the steps of: passing said continuous strip having a substantially uniform cross section in the longitudinal direction through a first pair of reduction rolls, at least one of which has an annular slot intermediate the ends thereof, to provide a reducing force to reduce the thickness of only those portions of said strip engaging said roll on opposite sides of said slot, said passing step including the provision of sufficient reducing force on said engaging portions of said strip to cause the unengaged portion of said strip to form a buckled portion in said slot, and passing the strip coming through said first pair of rolls through a second pair of reduction rolls, each having a smooth cylindrical surface, to roll said buckled portion to a predetermined thickness, thicker than the remaining portions of said strip.
Claim 3
Dependent Claim 65 words
A method according to claim 1 further comprising passing the strip exiting from said second pair of rolls through successive additional pairs of working rolls, with pairs having at least one roll with an annular slot being arranged alternately with pairs having smooth rolls, the respective slots of all rolls having said annular slots being progressively smaller in the processing direction of said shaping method.
Claim 4
Dependent Claim 31 words
A method according to claim 1 further comprising rolling said strip with a substantially uniform reduction rate in accordance with the thickness ratio in the direction of width of said strip.
Claim 5
Dependent Claim 45 words
A method according to claim 3 wherein said rolling of said strip is carried out by means of at least one set of finishing rolls one of which has a variable diameter across the width thereof adapted to contact the strip across its entire width.
Claim 6
Dependent Claim 21 words
A method according to claim 4 further comprising heating and annealing said strip before passing said strip through said finishing rolls.
Claim 7
Dependent Claim 35 words
A method according to claim 5 wherein a plurality of said finishing rolls are provided and further comprising heating and annealing said strip prior to each passage of said strip through a finishing roll set.

References Cited (Backward Citations)

US2193737A Cited
US4433565A Cited
US4295354A Cited
US4279139A Cited
US4402206A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-03-31 1989-09-30 1990-04-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-03-31 1993-09-30 1994-04-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-03-31 1997-09-30 1998-04-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag