← Back to Patent Explorer
US4574011A Expired / Lapsed US ⏱️ 0.0 years remaining

Sintered alloy based on carbides

Assignee: Stellram SA
•
Filing: 1984-03-06
•
Granted: 1986-03-04
•
Expires: 2004-03-06
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The alloy of the invention comprises 75 to 90% by weight of a mixture of carbides, for example WC and TiC, and 10 to 25% of a binder. This binder comprises Co, Ni and Ru, representing together 7 to 15% of the alloy, as well as Mo 2 C. This alloy is useful for the production of decorative articles having a density similar to that of stainless steel.

Inventors

  • 👤 Christian Bonjour
  • 👤 Francois Duvanel

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 04:19
CPC Classifications
C; C22; C22C; C22C29/00; C22C29/02; C22C29/06; C22C29/067; G; G04; G04B; G04B37/00; G04B37/22

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 91 words
Sintered alloy for use in the manufacture or ornamental articles and consisting essentially of 75 to 90% by weight of a mixture of carbides and 10 to 25% by weight of a binder, said binder consisting essentially of 60 to 70% by weight of Ni, Co and Ru, and 30 to 40% by weight of molybdenum carbide, and in which the Ru is present in a quantity of 10 to 25% of the whole of the three elements Co, Ni and Ru, the density of the alloy being 7.5 to 8.0.
Claim 2
Dependent Claim 91 words
Sintered alloy for use in the manufacture or ornamental articles and consisting essentially of 75 to 90% by weight of a mixture of carbides and 10 to 25% by weight of a binder, said binder consisting essentially of 60 to 70% by weight of Ni, Co and Ru, and 30 to 40% by weight of molybdenum carbide, and in which the Ru is present in a quantity of 10 to 25% of the whole of the three elements Co, Ni and Ru, the density of the alloy being 7.5 to 8.0.
Claim 3
Dependent Claim 24 words
Alloy according to claim 1, which is 83% of a mixture WC--TiC, 12% of Co, Ni and Ru, and 5% of Mo 2 C.
Claim 4
Dependent Claim 17 words
Alloy according to claim 2, which is 2% of Co, 8% of Ni and 2% of Ru.
Claim 5
Dependent Claim 14 words
Alloy according to claim 2, which is 41.5% of WC and 41.5% of TiC.
Claim 6
Dependent Claim 24 words
Alloy according to claim 1, which is 90% of a mixture WC--TiC, 7% of Co, Ni and Ru, and 3% of Mo 2 C.
Claim 7
Dependent Claim 24 words
Alloy according to claim 1, which is 75% of a mixture WC--TiC, 15% of Co, Ni and Ru and 10% of Mo 2 C.
Claim 8
Dependent Claim 27 words
Alloy according to claim 1, in which in the mixture of carbides a part thereof is replaced by at least a nitride and/or at least a boride.
Claim 9
Dependent Claim 19 words
Alloy according to claim 1, in which the Mo 2 C of the binder is partly replaced by HfC.

References Cited (Backward Citations)

GB622041A Cited
FR1007185A Cited
CH517963A Cited
US3245763A Cited
GB1282009A Cited
FR2037801A5 Cited
FR2097258A5 Cited
EP0044351A1 Cited
FR2487380A1 Cited
GB2081741A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-03-03 1989-09-02 1990-03-04 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-03-03 1993-09-02 1994-03-04 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-03-03 1997-09-02 1998-03-04 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag