Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
256 words
A fluorescent lamp having a phosphor film comprising: a blue-emitting phosphor consisting essentially of at least one of a divalent europium activated chlorophosphate phosphor having a general formula 3(M, Eu) 3 (PO 4 ) 2 .M'Cl 2 wherein M and M' are independently at least one of strontium (Sr), calcium (Ca) and barium (Ba); and a divalent europium activated haloborophosphate phosphor having a general formula: x(M.sub.1-p.Eu.sub.p.O).yP.sub.2 O.sub.5.aM'X.sub.2.bB.sub.2 O.sub.3 wherein M and M' are independently at least one of strontium (Sr), calcium (Ca) and barium (Ba); X is at least one of chlorine (Cl), fluorine (F) and bromine (Br); and 2.7≦x≦3.3, 0.50≦y≦1.50, 0.10≦a≦0.50, 0.01≦b≦0.50, and 0.001≦p≦0.20; a green-emitting phosphor consisting essentially of a cerium and terbium activated silicophosphate phosphor of a general formula: (Re.sub.1-c-d-3e Tb.sub.c Ce.sub.d A.sub.3e).sub.2 O.sub.3.qP.sub.2 O.sub.5.rSiO.sub.2 wherein Re is at least one of yttrium (Y), lanthanum (La) and gadolinium (Gd); A is at least one of lithium (Li), sodium (Na), potassium (K), rubidium (Rb), and cesium (Cs); and 0<c, O<d, 5×10 -2 ≧e≧1×10 -5 , 0<c+d+3e<1, 0<q, and 0<r; and a red-emitting phosphor consisting essentially of a trivalent europium activated yttrium oxide phosphor having a general formula (Y, Eu) 2 O 3 , wherein the phosphor film comprises 1 to 38% by weight of the blue-emitting phosphor, 13 to 73% by weight of the green-emitting phosphor and 15 to 65% by weight of the red-emitting phosphor based on 100% by weight of a total weight of the phosphors, and wherein said lamp exhibits a starting voltage at 21° C. of 88 V or less.
Claim 2
Dependent Claim
256 words
A fluorescent lamp having a phosphor film comprising: a blue-emitting phosphor consisting essentially of at least one of a divalent europium activated chlorophosphate phosphor having a general formula 3(M, Eu) 3 (PO 4 ) 2 .M'Cl 2 wherein M and M' are independently at least one of strontium (Sr), calcium (Ca) and barium (Ba); and a divalent europium activated haloborophosphate phosphor having a general formula: x(M.sub.1-p.Eu.sub.p.O).yP.sub.2 O.sub.5.aM'X.sub.2.bB.sub.2 O.sub.3 wherein M and M' are independently at least one of strontium (Sr), calcium (Ca) and barium (Ba); X is at least one of chlorine (Cl), fluorine (F) and bromine (Br); and 2.7≦x≦3.3, 0.50≦y≦1.50, 0.10≦a≦0.50, 0.01≦b≦0.50, and 0.001≦p≦0.20; a green-emitting phosphor consisting essentially of a cerium and terbium activated silicophosphate phosphor of a general formula: (Re.sub.1-c-d-3e Tb.sub.c Ce.sub.d A.sub.3e).sub.2 O.sub.3.qP.sub.2 O.sub.5.rSiO.sub.2 wherein Re is at least one of yttrium (Y), lanthanum (La) and gadolinium (Gd); A is at least one of lithium (Li), sodium (Na), potassium (K), rubidium (Rb), and cesium (Cs); and 0<c, O<d, 5×10 -2 ≧e≧1×10 -5 , 0<c+d+3e<1, 0<q, and 0<r; and a red-emitting phosphor consisting essentially of a trivalent europium activated yttrium oxide phosphor having a general formula (Y, Eu) 2 O 3 , wherein the phosphor film comprises 1 to 38% by weight of the blue-emitting phosphor, 13 to 73% by weight of the green-emitting phosphor and 15 to 65% by weight of the red-emitting phosphor based on 100% by weight of a total weight of the phosphors, and wherein said lamp exhibits a starting voltage at 21° C. of 88 V or less.