Developing powder
Assignee: Canon Inc
•
Filing: 1984-07-20
•
Granted: 1986-01-21
•
Expires: 2004-07-20
Abstract
Abstract A developing powder comprises a binder containing 50% by weight or more of a polymer having a gel content of 10% or less and prepared from a vinyl type monomer and a crosslinking agent monomer contained in an amount of 0.01-10% by weight based on the total weight of the monomers, and 0.1-5% by weight of an olefin homopolymer or copolymer having a melt viscosity at 140° C. of 10-10 6 cps.
Inventors
- 👤 Yasuo Mitsuhashi
- 👤 Masaki Uchiyama
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-24 03:10
CPC Classifications
G; G03; G03G; G03G9/00; G03G9/08; G03G9/087; G03G9/08784; G03G9/08793
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
120 words
An electrophotographic process comprising developing a latent image on a latent image supporting member with a toner, transferring the toner image developed, and removing the toner remaining on said image supporting member, characterized in that said toner is a developing powder which comprises a binder containing 0.1-5% by weight of an olefin homopolymer or copolymer having a melt viscosity at 140° C. of 10-10 6 cps. and containing 50% by weight or more of a crosslinked polymer, said crosslinked polymer in its entirety having a gel content of 10% or less and being prepared from a vinyl type monomer and a crosslinking agent monomer contained in an amount of 0.01-10% by weight based on the total weight of the monomers.
Claim 2
Dependent Claim
120 words
An electrophotographic process comprising developing a latent image on a latent image supporting member with a toner, transferring the toner image developed, and removing the toner remaining on said image supporting member, characterized in that said toner is a developing powder which comprises a binder containing 0.1-5% by weight of an olefin homopolymer or copolymer having a melt viscosity at 140° C. of 10-10 6 cps. and containing 50% by weight or more of a crosslinked polymer, said crosslinked polymer in its entirety having a gel content of 10% or less and being prepared from a vinyl type monomer and a crosslinking agent monomer contained in an amount of 0.01-10% by weight based on the total weight of the monomers.
References Cited (Backward Citations)
US2221776A
Cited
US2297691A
Cited
US2874063A
Cited
US4071361A
Cited
US3666363A
Cited
US3839029A
Cited
US3909258A
Cited
US3941898A
Cited
US4374191A
Cited
US4265992A
Cited
US4340660A
Cited
US4350440A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1989-01-20 | 1989-07-22 | 1990-01-21 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1993-01-20 | 1993-07-22 | 1994-01-21 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1997-01-20 | 1997-07-22 | 1998-01-21 | $7700.00 | Window Closed / Lapsed |