Composite plastic track and method of making
Assignee: Mead Corp
•
Filing: 1984-03-02
•
Granted: 1986-01-21
•
Expires: 2004-03-02
Abstract
Abstract A plastic track of composite construction is for use as an integral part of display stands of the gravity feed type which are commonly used in retail outlets and is formed by a coextrusion method wherein a quantity of high impact polystryene is heated to an extrudable temperature while a mixture of high impact polystryene and organopolysiloxane is similarly heated and extruded and the two molten melts are joined homogeneously under temperature and pressure within the die head to form a mechanically strong strack having a low friction sliding surface.
Inventors
- 👤 William S. Spamer
- 👤 Alan D. Preis
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-03 11:29
CPC Classifications
B; B29; B29C; B29C48/00; B29C48/03; B29C48/07; A; A47; A47F; A47F1/00; A47F1/04; A47F1/12; B29C48/12; B29C48/16; B29C48/18; B29C48/21; B29C48/25; B29C48/30; B29C48/305; B29C48/307; B32; B32B; B32B27/00; B32B27/06; B32B27/08; B32B27/30; B32B27/302; B32B3/00; B32B3/02; B32B3/04; B32B37/00; B32B37/14; B32B37/15; B32B37/153; B29K; B29K2025/00; B29K2083/00; B32B2307/00; B32B2307/50; B32B2307/558; B32B2307/70; B32B2307/746; Y; Y10; Y10T; Y10T428/00; Y10T428/24; Y10T428/24479; Y10T428/2457; Y10T428/31504; Y10T428/31652; Y10T428/31663; Y10T428/31667
Claims Analysis
Total Claims: 9
Claim 1
Independent Claim
43 words
A plastic track comprising an elongated base plate formed of high impact polystyrene and a low friction slide plate bonded to the upper surface of said base plate and formed of high impact polystyrene impregnated with 2% to 10% by weight of organopolysiloxane.
Claim 2
Dependent Claim
43 words
A plastic track comprising an elongated base plate formed of high impact polystyrene and a low friction slide plate bonded to the upper surface of said base plate and formed of high impact polystyrene impregnated with 2% to 10% by weight of organopolysiloxane.
Claim 3
Dependent Claim
31 words
A plastic track according to claim 1 wherein said base plate includes a pair of flange panels of high impact polystyrene integrally formed along the side edges of said base plate.
Claim 4
Independent Claim
152 words
A method of making a composite plastic track having a base plate to which a slide track is secured in flat face contacting relation, the method comprising the steps of heating a quantity of high impact polystyrene to a temperature at which said high impact polystyrene may be extruded, heating a mixture of high impact polystyrene and organopolysiloxane comprising 2% to 10% by weight of said mixture to a temperature at which said mixture may be extruded, pumping these extruded melts of high impact polystyrene and said mixture through a common co-extrusion die which utilizes separate melt channels until such time as the two materials are disposed in contacting relationship while in a hot fluid state so as to form a bond therebetween, the temperature to which the high impact polystyrene is heated is approximately 385 degrees F. and the temperature to which said mixture is heated is approximately 360 degrees F.
Claim 5
Independent Claim
152 words
A method of making a composite plastic track having a base plate to which a slide track is secured in flat face contacting relation, the method comprising the steps of heating a quantity of high impact polystyrene to a temperature at which said high impact polystyrene may be extruded, heating a mixture of high impact polystyrene and organopolysiloxane comprising 2% to 10% by weight of said mixture to a temperature at which said mixture may be extruded, pumping these extruded melts of high impact polystyrene and said mixture through a common co-extrusion die which utilizes separate melt channels until such time as the two materials are disposed in contacting relationship while in a hot fluid state so as to form a bond therebetween, the temperature to which the high impact polystyrene is heated is approximately 385 degrees F. and the temperature to which said mixture is heated is approximately 360 degrees F.
Claim 6
Dependent Claim
24 words
A method according to claim 3 wherein the die through which said high impact polystyrene is extruded is generally rectangular in cross sectional configuration.
Claim 7
Dependent Claim
35 words
A method according to claim 4 wherein the die through which said high impact polystyrene is extruded includes parts communicating with opposite ends of the rectangularly shaped part thereof and in substantially normal relation thereto.
Claim 8
Dependent Claim
67 words
A method according to claim 3 wherein the die through which said mixture is extruded in configured to form a slide plate having one surface which is flat and an opposite surface having a plurality of spaced parallel ribs of generally triangular cross section and wherein the flat surface of said slide plate is secured in flat face contacting relation with a surface of said base plate.
Claim 9
Dependent Claim
38 words
A method according to claim 3 wherein the pressure of said high impact polystyrene after heating is approximately 1070 pounds per square inch and the pressure of said mixture after heating is approximately 950 pounds per square inch.
References Cited (Backward Citations)
US2218444A
Cited
US4470943A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1989-01-20 | 1989-07-22 | 1990-01-21 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1993-01-20 | 1993-07-22 | 1994-01-21 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1997-01-20 | 1997-07-22 | 1998-01-21 | $7700.00 | Window Closed / Lapsed |