Claims Analysis
Total Claims: 13
Claim 1
Independent Claim
94 words
A capacitance humidity sensing element comprising: a non-conducting substrate; at least two separate thin metal film electrodes deposited on said substrate; a first thin dielectric film of a water absorbing material covering said electrodes and the supporting substrate, said material being such that its dielectric constant varies with the amount of water absorbed; an electrically conductive water permeable mesh covering said first dielectric film, said mesh having openings which are substantially evenly distributed over its surface to provide its water permeable characteristic; and a second thin film of water absorbing material covering said mesh.
Claim 2
Dependent Claim
94 words
A capacitance humidity sensing element comprising: a non-conducting substrate; at least two separate thin metal film electrodes deposited on said substrate; a first thin dielectric film of a water absorbing material covering said electrodes and the supporting substrate, said material being such that its dielectric constant varies with the amount of water absorbed; an electrically conductive water permeable mesh covering said first dielectric film, said mesh having openings which are substantially evenly distributed over its surface to provide its water permeable characteristic; and a second thin film of water absorbing material covering said mesh.
Claim 3
Dependent Claim
32 words
An element as set forth in claim 1 in which said electrodes have interdigitated fingers; and the period of the spacing of said fingers is less than the thickness of the substrate.
Claim 4
Dependent Claim
47 words
An element as set forth in claim 1 in which the openings in the mesh have an average diameter which is less than the thickness of said second dielectric film; and the average spacing of said openings is less than the thickness of said first dielectric film.
Claim 5
Dependent Claim
95 words
An element as set forth in claim 3 in which the average diameter of the openings in said mesh, the average spacing of said openings, and the sheet resistance of the mesh material are such that the resistance of the conductive path carrying the current between adjacent electrodes is small with respect to the capacitive reactance in that path due to said first dielectric film so that changes in capacitive reactance due to changes in the humidity being measured are large with respect to any changes in the resistance of the path which may occur.
Claim 6
Dependent Claim
51 words
An element as set forth in claims 3 or 4 in which the square of the sum of the thicknesses of said first and second dielectric film is minimized while maintaining the average spacing of the openings, the average diameter of the openings and the path resistance within the desired limits.
Claim 7
Dependent Claim
25 words
An element as set forth in claims 1, 2, or 3 in which the material of the first and second dielectric film is a polymer.
Claim 8
Dependent Claim
21 words
An element as set forth in claim 1 in which the thickness of the mesh is between 50 and 100 angstroms.
Claim 9
Independent Claim
120 words
A method for producing a humidity measuring element, comprising the steps of: providing a non-conductive substrate; depositing on said substrate two separate closely spaced interdigitated thin metal film electrodes with fingers having a period less than the thickness of said substrate; overlaying said substrate and said electrodes with a first thin dielectric film of a water absorbing material whose dielectric constant varies with the amount of water absorbed; depositing over said first dielectric film an electrically conductive water permeable mesh, said mesh being deposited to a thickness such that it has openings which are substantially evenly distributed over its surface to provide its water permeable characteristic; and overlaying said mesh with a second thin dielectric film of water absorbing material.
Claim 10
Independent Claim
120 words
A method for producing a humidity measuring element, comprising the steps of: providing a non-conductive substrate; depositing on said substrate two separate closely spaced interdigitated thin metal film electrodes with fingers having a period less than the thickness of said substrate; overlaying said substrate and said electrodes with a first thin dielectric film of a water absorbing material whose dielectric constant varies with the amount of water absorbed; depositing over said first dielectric film an electrically conductive water permeable mesh, said mesh being deposited to a thickness such that it has openings which are substantially evenly distributed over its surface to provide its water permeable characteristic; and overlaying said mesh with a second thin dielectric film of water absorbing material.
Claim 11
Independent Claim
180 words
A method for producing a fast responding humidity sensing element which will not be subject to influence from surface contamination, comprising the steps of: providing a non-conductive planar substrate of a certain thickness; depositing on said substrate two thin film interdigitated electrodes whose fingers are spaced apart by a distance such that the period of said fingers is less than the thickness of said substrate; depositing over said interdigitated fingers a first water absorbing polymer film whose dielectric constant varies with the amount of water absorbed, said film having the thickness necessary to obtain the response time desired for the element; depositing over said first polymer film a thin conductive mesh whose thickness is such that there are produced holes in said mesh which have an average spacing less than the thickness of said first polymer film; and depositing over said mesh a second water absorbing polymer film whose thickness is greater than the average diameter of the holes in said mesh but is still within the thickness range required to keep the elements response time within the required range.
Claim 12
Independent Claim
180 words
A method for producing a fast responding humidity sensing element which will not be subject to influence from surface contamination, comprising the steps of: providing a non-conductive planar substrate of a certain thickness; depositing on said substrate two thin film interdigitated electrodes whose fingers are spaced apart by a distance such that the period of said fingers is less than the thickness of said substrate; depositing over said interdigitated fingers a first water absorbing polymer film whose dielectric constant varies with the amount of water absorbed, said film having the thickness necessary to obtain the response time desired for the element; depositing over said first polymer film a thin conductive mesh whose thickness is such that there are produced holes in said mesh which have an average spacing less than the thickness of said first polymer film; and depositing over said mesh a second water absorbing polymer film whose thickness is greater than the average diameter of the holes in said mesh but is still within the thickness range required to keep the elements response time within the required range.
Claim 13
Dependent Claim
48 words
A method for producing a humidity sensing element as set forth in claim 9 in which; the water absorbing polymer of the first and second films is a polyimide; and the mesh is of a metal and has a thickness in the range of 50 to 100 angstroms.