← Back to Patent Explorer
US4550050A Expired / Lapsed US ⏱️ 0.0 years remaining

Fiberous batt

Assignee: Fiberlok Inc
•
Filing: 1984-03-21
•
Granted: 1985-10-29
•
Expires: 2004-03-21
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for producing a fiberous batt by contacting fibers with particles of a copolymer of vinyl chloride and a diester of a vinyl unsaturated dicarboxylic acid.

Inventors

  • 👤 George S. Buck, Jr.

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 21:10
CPC Classifications
D; D04; D04H; D04H1/00; D04H1/40; D04H1/58; D04H1/60; Y; Y10; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31855; Y10T428/3188; Y10T428/31884; Y10T428/31891; Y10T428/31895; Y10T428/31906; Y10T428/31935; Y10T442/00; Y10T442/20; Y10T442/2926; Y10T442/2934; Y10T442/60; Y10T442/699

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 40 words
A fibrous batt, the individual fibers of which are bonded at their intersection by melted and refrozen particles of a copolymer of vinyl chloride and a diester of vinyl unsaturated dicarboxylic acid wherein the diester is maleic acid dibutyl ester.
Claim 2
Dependent Claim 40 words
A fibrous batt, the individual fibers of which are bonded at their intersection by melted and refrozen particles of a copolymer of vinyl chloride and a diester of vinyl unsaturated dicarboxylic acid wherein the diester is maleic acid dibutyl ester.
Claim 3
Dependent Claim 113 words
A fiberous batt of high compressive strength, the individual fibers of which are bonded at their intersection by melted and refrozen particles of a copolymer of vinyl chloride and a diester of vinyl unsaturated dicarboxylic acid; wherein the fibers have a fiber denier from 1 to 22; and wherein the weight ratio of vinyl unsaturated dicarboxylic acid to vinyl chloride is 3:97 to 20:80; and wherein the weight ratio of the copolymer to the fibers is 3:97 to 35:65; and wherein the copolymer particles have a size range of 6 to 25 microns; and wherein the copolymer has a melting point of 135° to 190° C.; and wherein the diester is dibutyl maleate.
Claim 4
Dependent Claim 113 words
A fiberous batt of high compressive strength, the individual fibers of which are bonded at their intersection by melted and refrozen particles of a copolymer of vinyl chloride and a diester of vinyl unsaturated dicarboxylic acid; wherein the fibers have a fiber denier from 1 to 22; and wherein the weight ratio of vinyl unsaturated dicarboxylic acid to vinyl chloride is 3:97 to 20:80; and wherein the weight ratio of the copolymer to the fibers is 3:97 to 35:65; and wherein the copolymer particles have a size range of 6 to 25 microns; and wherein the copolymer has a melting point of 135° to 190° C.; and wherein the diester is dibutyl maleate.

References Cited (Backward Citations)

US3325344A Cited
US3862287A Cited
US3993518A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-10-28 1989-04-29 1989-10-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-10-28 1993-04-29 1993-10-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-10-28 1997-04-29 1997-10-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag