Claims Analysis
Total Claims: 9
Claim 1
Independent Claim
359 words
A substituted pyrrole polymer linked through N-adjacent carbon atoms of the pyrrole nucleus, said polymer being represented by the structure: ##STR16## wherein, n is an integer in the range from about 2 to about 100; R 1 is selected from the group consisting of hydrogen, alkyl having from 1 to about 6 carbon atoms, cycloalkyl having from 3 to about 7 ring carbon atoms one or more of which may be substituted, alkoxyalkyl having from 3 to about 24 carbon atoms, and benzyl which may optionally be ring-substituted with halogen or lower alkyl having from 1 to about 6 carbon atoms; R 2 is selected from the group consisting of hydroxyphenyl which may be ring-substituted, and an acyclic ether selected from the group consisting of (i) alkoxy represented by --OR 3 , wherein R 3 represents alkyl having from 1 to about 12 carbon atoms, alkoxyalkyl having from 2 to about 24 carbon atoms, phenyl which may be substituted, benzyl or substituted benzyl, heteroaryl or substituted heteroaryl; (ii) polyalkoxy represented by the structure CH 3 --OCH 2 CH 2 -- n' wherein n' is an integer in the range from 1 to about 20; and (iii) R 4 --O--R 5 wherein either R 4 or R 5 is a linking group selected from the group consisting of phenyl and benzyl, each of which may be substituted, alkyl having from 1 to about 25 carbon atoms, and cycloalkyl having from 3 to about 7 ring carbon atoms one or more of which may be substituted; and, R 1 may be substituted with R 2 , and if so substituted, each R 2 substituent may be the same or different; said polymer being formed by a process comprising, (a) forming a solution of said monomer and an electrolyte which generates an acid ion in a mutual solvent, said monomer having the structure ##STR17## wherein R 1 and R 2 have the same connotation as that given hereinabove; (b) passing electrical current between electrodes placed in said solution at an applied voltage and intensity sufficient to deposit a polymer on the anode; and, (c) recovering a compactable powdery deposit of said polymer.
Claim 2
Dependent Claim
359 words
A substituted pyrrole polymer linked through N-adjacent carbon atoms of the pyrrole nucleus, said polymer being represented by the structure: ##STR16## wherein, n is an integer in the range from about 2 to about 100; R 1 is selected from the group consisting of hydrogen, alkyl having from 1 to about 6 carbon atoms, cycloalkyl having from 3 to about 7 ring carbon atoms one or more of which may be substituted, alkoxyalkyl having from 3 to about 24 carbon atoms, and benzyl which may optionally be ring-substituted with halogen or lower alkyl having from 1 to about 6 carbon atoms; R 2 is selected from the group consisting of hydroxyphenyl which may be ring-substituted, and an acyclic ether selected from the group consisting of (i) alkoxy represented by --OR 3 , wherein R 3 represents alkyl having from 1 to about 12 carbon atoms, alkoxyalkyl having from 2 to about 24 carbon atoms, phenyl which may be substituted, benzyl or substituted benzyl, heteroaryl or substituted heteroaryl; (ii) polyalkoxy represented by the structure CH 3 --OCH 2 CH 2 -- n' wherein n' is an integer in the range from 1 to about 20; and (iii) R 4 --O--R 5 wherein either R 4 or R 5 is a linking group selected from the group consisting of phenyl and benzyl, each of which may be substituted, alkyl having from 1 to about 25 carbon atoms, and cycloalkyl having from 3 to about 7 ring carbon atoms one or more of which may be substituted; and, R 1 may be substituted with R 2 , and if so substituted, each R 2 substituent may be the same or different; said polymer being formed by a process comprising, (a) forming a solution of said monomer and an electrolyte which generates an acid ion in a mutual solvent, said monomer having the structure ##STR17## wherein R 1 and R 2 have the same connotation as that given hereinabove; (b) passing electrical current between electrodes placed in said solution at an applied voltage and intensity sufficient to deposit a polymer on the anode; and, (c) recovering a compactable powdery deposit of said polymer.
Claim 3
Dependent Claim
48 words
The polymer of claim 1 obtained by the electrodeposition of a monomer from a solvent for it, in the presence of an electrolyte which generates an acid ion, said monomer having the structure: ##STR18## wherein, R 1 and R 2 have the same connotation as in claim 1.
Claim 4
Dependent Claim
17 words
The polymer of claim 2 obtained as a powdery deposit which is compactable into a shaped article.
Claim 5
Dependent Claim
41 words
The polymer of claim 3 wherein said electrolyte is an alkylammonium salt, and said polymer is soluble in aprotic aromatic and heteroaromatic solvents selected from the group consisting of toluene, xylene, chlorinated and fluorinated hydrocarbons, lower alkyl esters, dimethylsulfoxide, and tetrahydrofuran.
Claim 6
Dependent Claim
340 words
A process for polymerizing a substituted pyrrole monomer, comprising, (a) forming a solution of said monomer and an electrolyte which generates an acid ion in a mutual solvent, said monomer having the structure ##STR19## wherein, R 1 is selected from the group consisting of hydrogen, alkyl having from 1 to about 6 carbon atoms, cycloalkyl having from 3 to about 7 ring carbon atoms one or more of which may be substituted, alkoxyalkyl having from 3 to about 24 carbon atoms, and benzyl which may optionally be ring-substituted with halogen or lower alkyl having from 1 to about 6 carbon atoms; R 2 is selected from the group consisting of hydroxyphenyl which may be ring-substituted, and an acyclic ether selected from the group consisting of (i) alkoxy represented by -OR 3 , wherein R 3 represents alkyl having from 1 to about 12 carbon atoms, alkoxyalkyl having from 2 to about 24 carbon atoms, phenyl which may be substituted, benzyl or substituted benzyl, heteroaryl or substituted heteroaryl; (ii) polyalkoxy represented by the structure CH 3 --OCH 2 CH 2 -- n' wherein n' is an integer in the range from 1 to about 20; and (iii) R 4 -O-R 5 wherein either R 4 or R 5 is a linking group selected from phenyl and benzyl, each of which may be substituted, alkyl having from 1 to about 24 carbon atoms, and cycloalkyl having from 3 to about 7 ring carbon atoms one or more of which may be substituted; and, R 1 may be substituted with R 2 , and if so substituted, each R 2 substituent may be the same or different; (b) passing electrical current between electrodes placed in said solution at an applied voltage and intensity sufficient to deposit a polymer on the anode; and, (c) recovering a compactable powdery deposit of said polymer which is linked through N-adjacent carbon atoms of the pyrrole nucleus and represented by the structure: ##STR20## wherein R 1 and R 2 have the same connotation as that set forth hereinabove.
Claim 7
Dependent Claim
340 words
A process for polymerizing a substituted pyrrole monomer, comprising, (a) forming a solution of said monomer and an electrolyte which generates an acid ion in a mutual solvent, said monomer having the structure ##STR19## wherein, R 1 is selected from the group consisting of hydrogen, alkyl having from 1 to about 6 carbon atoms, cycloalkyl having from 3 to about 7 ring carbon atoms one or more of which may be substituted, alkoxyalkyl having from 3 to about 24 carbon atoms, and benzyl which may optionally be ring-substituted with halogen or lower alkyl having from 1 to about 6 carbon atoms; R 2 is selected from the group consisting of hydroxyphenyl which may be ring-substituted, and an acyclic ether selected from the group consisting of (i) alkoxy represented by -OR 3 , wherein R 3 represents alkyl having from 1 to about 12 carbon atoms, alkoxyalkyl having from 2 to about 24 carbon atoms, phenyl which may be substituted, benzyl or substituted benzyl, heteroaryl or substituted heteroaryl; (ii) polyalkoxy represented by the structure CH 3 --OCH 2 CH 2 -- n' wherein n' is an integer in the range from 1 to about 20; and (iii) R 4 -O-R 5 wherein either R 4 or R 5 is a linking group selected from phenyl and benzyl, each of which may be substituted, alkyl having from 1 to about 24 carbon atoms, and cycloalkyl having from 3 to about 7 ring carbon atoms one or more of which may be substituted; and, R 1 may be substituted with R 2 , and if so substituted, each R 2 substituent may be the same or different; (b) passing electrical current between electrodes placed in said solution at an applied voltage and intensity sufficient to deposit a polymer on the anode; and, (c) recovering a compactable powdery deposit of said polymer which is linked through N-adjacent carbon atoms of the pyrrole nucleus and represented by the structure: ##STR20## wherein R 1 and R 2 have the same connotation as that set forth hereinabove.
Claim 8
Dependent Claim
10 words
The process of claim 5 wherein said polymer is compactable.
Claim 9
Dependent Claim
16 words
The process of claim 6 wherein said polymer is soluble in aprotic aromatic and heteroaromatic solvents.