Abstract

Abstract Sintered aluminum nitride having a high thermal conductivity, which comprises at least 65% by weight of aluminum nitride, and at least one of beryllium, a beryllium compound, lithium and a lithium compound, and a semi-conductor device using the same.

Inventors

  • 👤 Yukio Takeda
  • 👤 Satoru Ogihara
  • 👤 Mitsuru Ura
  • 👤 Kousuke Nakamura
  • 👤 Tadamichi Asai
  • 👤 Tokio Ohkoshi
  • 👤 Yasuo Matsushita
  • 👤 Kunihiro Maeda

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 14:44
CPC Classifications
H; H10; H10W; H10W70/00; H10W70/60; H10W70/67; H10W70/69; H10W70/692; C; C04; C04B; C04B35/00; C04B35/515; C04B35/58; C04B35/581; H10P; H10P14/00; H10P14/60; H10P14/69; H10P14/694; H10P14/6943; H10P14/69433; H10W72/00; H10W72/50; H10W72/531; H10W72/5363; H10W72/551; H10W72/552; H10W72/5524; H10W74/00; Y; Y10; Y10T; Y10T428/00; Y10T428/12; Y10T428/12493; Y10T428/12528; Y10T428/12535; Y10T428/12576; Y10T428/12583; Y10T428/12674

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 39 words
Sintered aluminum nitride having a thermal conductivity at room temperature of 0.2 cal/cm.sec.°C. or higher, which consists essentially of at least 65% by weight of aluminum nitride and at least one of beryllium, beryllium compound, lithium and lithium compound.
Claim 2
Dependent Claim 39 words
Sintered aluminum nitride having a thermal conductivity at room temperature of 0.2 cal/cm.sec.°C. or higher, which consists essentially of at least 65% by weight of aluminum nitride and at least one of beryllium, beryllium compound, lithium and lithium compound.
Claim 3
Dependent Claim 42 words
The sintered aluminum nitride according to claim 1, wherein 0.05 to 10% by weight of at least one of the beryllium and the beryllium compound in terms of beryllium atom is contained in the aluminum nitride on the basis of aluminum nitride.
Claim 4
Dependent Claim 66 words
Sintered aluminum nitride having a thermal conductivity at room temperature of 0.2 cal/cm.sec.°C. or higher, which comprises at least 65% by weight of aluminum nitride and at least one of lithium and lithium compound, with 0.05-5% by weight of at least one of the lithium and the lithium compound in terms of lithium atom being contained in the aluminum nitride on the basis of aluminum nitride.
Claim 5
Dependent Claim 66 words
Sintered aluminum nitride having a thermal conductivity at room temperature of 0.2 cal/cm.sec.°C. or higher, which comprises at least 65% by weight of aluminum nitride and at least one of lithium and lithium compound, with 0.05-5% by weight of at least one of the lithium and the lithium compound in terms of lithium atom being contained in the aluminum nitride on the basis of aluminum nitride.
Claim 6
Dependent Claim 181 words
The sintered aluminum nitride according to claim 1, wherein 0.05 to 10% by weight of at least one of the beryllium and the beryllium compound in terms of beryllium atom and 0.05 to 5% by weight of at least one of the lithium and the lithium compound in terms of lithium atom are contained in the aluminum nitride on the basis of aluminum nitride, and when at least one of the lithium and the lithium compound takes the major proportion, the sum total of at least one of the beryllium and the beryllium compound and at least one of the lithium and the lithium compound is not more than 5% by weight in terms of beryllium and lithium atoms, and when at least one of the beryllium and the beryllium compound takes the major portion, the sum total of at least one of the beryllium and the beryllium compound and at least one of the lithium and the lithium compound is not more than 10% by weight in the term of beryllium and lithium atoms on the basis of aluminum nitride.
Claim 7
Dependent Claim 73 words
Sintered aluminum nitride having a thermal conductivity at room temperature of 0.2 cal/cm.sec.°C. or higher, which consists essentially of at least 65% by weight of aluminum nitride, not more than 5% by weight of at least one of Y 2 O 3 , MgO, Al 2 O 3 and SiO 2 in terms of atoms on the basis of aluminum nitride and at least one of beryllium, beryllium compound, lithium and lithium compound.
Claim 8
Dependent Claim 73 words
Sintered aluminum nitride having a thermal conductivity at room temperature of 0.2 cal/cm.sec.°C. or higher, which consists essentially of at least 65% by weight of aluminum nitride, not more than 5% by weight of at least one of Y 2 O 3 , MgO, Al 2 O 3 and SiO 2 in terms of atoms on the basis of aluminum nitride and at least one of beryllium, beryllium compound, lithium and lithium compound.
Claim 9
Dependent Claim 20 words
The sintered aluminum nitride according to claim 1, which has a density of 90% or more of its theoretical density.
Claim 10
Dependent Claim 22 words
The sintered aluminum nitride according to claim 6, which has an electrical resistivity of 10 12 Ω.cm or higher at room temperature.
Claim 11
Dependent Claim 28 words
The sintered aluminum nitride according to claim 1, which has an average coefficient of thermal expansion of 5×10 -6 /°C. or less between room temperature and 300° C.
Claim 12
Dependent Claim 48 words
The sintered aluminum nitride according to claim 1, wherein said beryllium compound is selected from the group consisting of beryllium nitrate, beryllium sulfate, beryllium carbonate, beryllium phosphate, beryllium hydroxide, beryllium chloride, beryllium fluoride, beryllium acetylacetonate, beryllium oxalate, beryllium carbide, beryllium boride, beryllium silicide, beryllium nitride and beryllium oxide.
Claim 13
Dependent Claim 35 words
The sintered aluminum nitride according to claim 9, wherein the lithium compound is selected from the group consisting of lithium oxide, lithium chloride, lithium fluoride, lithium nitrate, lithium carbonate, lithium sulfate and a mixture thereof.
Claim 14
Dependent Claim 56 words
Sintered aluminum nitride having a thermal conductivity at room temperature of 0.2 cal/cm.sec.°C. or higher, which comprises at least 65% by weight of aluminum nitride and at least one of lithium and lithium compound selected from the group consisting of lithium oxide, lithium chloride, lithium fluoride, lithium nitrate, lithium carbonate, lithium sulfate and a mixture thereof.
Claim 15
Dependent Claim 56 words
Sintered aluminum nitride having a thermal conductivity at room temperature of 0.2 cal/cm.sec.°C. or higher, which comprises at least 65% by weight of aluminum nitride and at least one of lithium and lithium compound selected from the group consisting of lithium oxide, lithium chloride, lithium fluoride, lithium nitrate, lithium carbonate, lithium sulfate and a mixture thereof.

References Cited (Backward Citations)

US3930875A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-09-09 1989-03-11 1989-09-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-09-09 1993-03-11 1993-09-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-09-09 1997-03-11 1997-09-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag