Abstract

Abstract A silver halide light-sensitive material is disclosed. The material is comprised of a support comprising thereon at least two emulsion layers having the same color sensitivity and being different light-sensitivities, with a layer containing comparatively light-insensitive silver halide grains of 0.05 to 0.6 μm in average grain size being positioned in at least one of interspaces defined by every two adjacent members of said at least two emulsion layers. The resulting material has both raised sensitivity and improved graininess.

Inventors

  • 👤 Tsutomu Saito
  • 👤 Keiji Mihayashi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 19:48
CPC Classifications
G; G03; G03C; G03C1/00; G03C1/005; G03C1/46; G03C7/00; G03C7/30; G03C7/3029; G03C2007/3034

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 95 words
A silver halide light-sensitive material comprising a support comprising thereon (1) at least two emulsion layers having the same color sensitivity and being different in sensitivity, and (2) an intermediate layer sandwiched between said at least two emulsion layers, said intermediate layer containing comparatively light-insensitive silver halide grains of 0.05 to 0.6 μm in average grain size and wherein said intermediate layer does not contain couplers and has a sensitivity lower than the least sensitive layer of the two light-sensitive silver halide emulsion layers of the same color sensitivity by 0.5 or more log units.
Claim 2
Dependent Claim 95 words
A silver halide light-sensitive material comprising a support comprising thereon (1) at least two emulsion layers having the same color sensitivity and being different in sensitivity, and (2) an intermediate layer sandwiched between said at least two emulsion layers, said intermediate layer containing comparatively light-insensitive silver halide grains of 0.05 to 0.6 μm in average grain size and wherein said intermediate layer does not contain couplers and has a sensitivity lower than the least sensitive layer of the two light-sensitive silver halide emulsion layers of the same color sensitivity by 0.5 or more log units.
Claim 3
Dependent Claim 50 words
A silver halide light-sensitive material as claimed in claim 1, wherein the layer containing comparatively light-insensitive silver halide grains has a sensitivity lower than the least sensitive layer of at least two light sensitive silver halide emulsion layers of the same color sensitivity by 1.0 or more in log units.
Claim 4
Dependent Claim 41 words
A silver halide light-sensitive material as claimed in claim 1, wherein the layer containing comparatively light-insensitive silver halide grains is comprised of an emulsion containing 60% or more silver bromide, 30% or less silver chloride, and 40% or less silver iodide.
Claim 5
Dependent Claim 27 words
A silver halide light-sensitive material as claimed in claim 1, wherein the light-insensitive silver halide grains have a size in the range of 0.08 to 0.4 μm.
Claim 6
Dependent Claim 40 words
A silver halide light-sensitive material as claimed in claim 1, wherein said at least two emulsion layers are blue-sensitive emulsion layers and the light-insensitive layer includes silver halide grains having a size in the range of 0.08 to 0.25 μm.
Claim 7
Dependent Claim 40 words
A silver halide light-sensitive material as claimed in claim 1, wherein said at least two emulsion layers are green-sensitive silver halide emulsion layers and the light-insensitive silver halide grains have a size in the range of 0.1 to 0.3 μm.
Claim 8
Dependent Claim 40 words
A silver halide light-sensitive material as claimed in claim 1, wherein said at least two emulsion layers are red-sensitive silver halide emulsion layers and the light-insensitive silver halide grains have a size in the range of 0.1 to 0.4 μm.
Claim 9
Dependent Claim 39 words
A silver halide light-sensitive material as claimed in claim 1, wherein the layer containing comparatively light-insensitive silver halide grains is present in an amount in the range of 0.03 to 5 g/m 2 based on the amount of silver.
Claim 10
Dependent Claim 39 words
A silver halide light-sensitive material as claimed in claim 8, wherein the layer containing comparatively light-insensitive silver halide grains is present in an amount in the range of 0.05 to 1 g/m 2 based on the amount of silver.

References Cited (Backward Citations)

US3728121A Cited
US3737317A Cited
US4129446A Cited
US4438194A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-09-02 1989-03-04 1989-09-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-09-02 1993-03-04 1993-09-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-09-02 1997-03-04 1997-09-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag