Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
135 words
A method for delignifying or bleaching cellulose pulp which comprises in at least one stage adding a liquid containing chlorine dioxide to the cellulose pulp; reacting the cellulose pulp with the chlorine dioxide over a selected period of time; and then decreasing the amount of active chlorine available to the pulp by removing at least a substantial amount of the chlorine by removing a portion of the liquid accompanying the pulp; replenishing active chlorine as chlorine dioxide in the liquid removed from the pulp by regenerating chlorine dioxide in situ by adding chlorine as chlorine only in an amount from 10 to 35% of the amount of active chlorine already present in the liquid; and then recyling the replenished liquid as chlorine dioxide liquor to newly supplied cellulose pulp for delignifying or bleaching the pulp.
Claim 2
Independent Claim
135 words
A method for delignifying or bleaching cellulose pulp which comprises in at least one stage adding a liquid containing chlorine dioxide to the cellulose pulp; reacting the cellulose pulp with the chlorine dioxide over a selected period of time; and then decreasing the amount of active chlorine available to the pulp by removing at least a substantial amount of the chlorine by removing a portion of the liquid accompanying the pulp; replenishing active chlorine as chlorine dioxide in the liquid removed from the pulp by regenerating chlorine dioxide in situ by adding chlorine as chlorine only in an amount from 10 to 35% of the amount of active chlorine already present in the liquid; and then recyling the replenished liquid as chlorine dioxide liquor to newly supplied cellulose pulp for delignifying or bleaching the pulp.
Claim 3
Dependent Claim
23 words
A method according to claim 1 in which the liquid is removed by displacing the liquid with liquid containing substantially no active chlorine.
Claim 4
Dependent Claim
25 words
A method according to claim 2 in which in addition to regenerating chlorine dioxide in situ the fresh liquid is also replenished with chlorine dioxide.
Claim 5
Dependent Claim
53 words
A method according to claim 1 in which the cellulose pulp prior to the commencement of the delignification or bleaching is at a pulp concentration within the range from 2 to 40%, and the pulp concentration is lowered to within the range from 5 to 30%, by supplying the liquid containing chlorine dioxide.
Claim 6
Dependent Claim
33 words
A method according to claim 1 in which the selected time period before decreasing the amount of active chlorine available to the cellulose pulp is within the range from 0.1 to 30 minutes.
Claim 7
Dependent Claim
25 words
A method according to claim 1 in which the liquid replenished with chlorine is recycled to newly supplied cellulose pulp in the same bleaching stage.
Claim 8
Dependent Claim
25 words
A method according to claim 1 in which the pH of the liquid throughout the process is maintained within the range from 4 to 6.
Claim 9
Dependent Claim
48 words
A method according to claim 1 in which after the liquid accompanying the pulp is removed and the amount of active chlorine available to the cellulose pulp is reduced, the cellulose pulp is caused to continue to react with the residual active chlorine-containing liquid in a second stage.
Claim 10
Dependent Claim
30 words
A method according to claim 8, in which the cellulose pulp is caused to react with the residual active chlorine-containing liquid over a period of from 0.1 to 60 minutes.