Abstract
Abstract A homogeneous boron containing alloy is disclosed with a composition which can be essentially represented by the formula of: MiTjBk where M is a metal from the group of nickel, iron, cobalt or a mixture thereof; T is a refractory metal from the group of molybdenum, tungsten, or a mixture thereof; and B is the element boron. The subscripts i, j, k are the respective atomic percent of each of the constituents and vary respectively between about 25 and 98, between about 1 and 40, and between 1 and 35 with the proviso that j>k, and i+j+k=100. By further limitation of the chemistry, it is possible to assure the alloy will age harden.
Inventors
- 👤 Deepak Kapoor
- 👤 Chung-Chu Wan
- 👤 Rong Y. Wang
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-24 00:57
CPC Classifications
C; C22; C22C; C22C45/00; C22C45/008; Y; Y10; Y10T; Y10T428/00; Y10T428/12; Y10T428/12431
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
89 words
A single-phase, boride-free, homogeneous microcrystalline boron-containing alloy consisting of the formula: M i T j B k where M is a metal selected from the group Ni, Fe, Co or a mixture thereof; T is a refractory metal selected from the group Mo, W, or a mixture thereof; B is the element boron; and i, j and k are the atomic percent of M, T and B and are between 45 and 82, 12 and 35, and 1 and 20 respectively with the proviso that i+j+k=100% and that j>k.
Claim 2
Dependent Claim
89 words
A single-phase, boride-free, homogeneous microcrystalline boron-containing alloy consisting of the formula: M i T j B k where M is a metal selected from the group Ni, Fe, Co or a mixture thereof; T is a refractory metal selected from the group Mo, W, or a mixture thereof; B is the element boron; and i, j and k are the atomic percent of M, T and B and are between 45 and 82, 12 and 35, and 1 and 20 respectively with the proviso that i+j+k=100% and that j>k.
Claim 3
Dependent Claim
12 words
The alloy of claim 1 wherein said alloy is in powder form.
Claim 4
Dependent Claim
16 words
The powder of claim 2 wherein the mesh size range is between about -35 and +325.
Claim 5
Dependent Claim
12 words
The alloy of claim 1 wherein said alloy is in ribbon form.
Claim 6
Dependent Claim
10 words
The alloys of claim 1, 2, or 4 wherein j-k<2.
References Cited (Backward Citations)
US3856513A
Cited
US4116682A
Cited
US4133681A
Cited
US4133679A
Cited
US4133682A
Cited
US4365994A
Cited
US4297135A
Cited
US4318733A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1988-08-05 | 1989-02-04 | 1989-08-06 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1992-08-05 | 1993-02-04 | 1993-08-06 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1996-08-05 | 1997-02-04 | 1997-08-06 | $7700.00 | Window Closed / Lapsed |