← Back to Patent Explorer
US4529835A Expired / Lapsed US ⏱️ 0.0 years remaining

Ceramic thick film circuit substrate

Assignee: NGK Insulators Ltd
•
Filing: 1983-10-21
•
Granted: 1985-07-16
•
Expires: 2003-10-21
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Disclosed herein is a ceramic thick film circuit substrate for use in an electronic circuit part, characterized in that a conductive layer at a place where it is to be connected with a thick film circuit is composed of a mixture of tungsten and at least one of platinum and palladium. Based on 100 parts by weight of tungsten, platinum is 0.1-100 parts by weight in the case of platinum alone, palladium is 0.1-20 parts by weight in the case of palladium alone; and a total amount of platinum and palladium is 0.1-76 parts by weight in the case of combination of platinum and palladium. Thereby, the ceramic thick film circuit substrate has an excellent oxidation resistance, and low contact resistance to the thick film circuit.

Inventors

  • 👤 Fukuzo Mizuno

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 17:41
CPC Classifications
H; H05; H05K; H05K1/00; H05K1/02; H05K1/09; H05K1/092

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 137 words
In a ceramic thick film circuit substrate in which a thick film conductor which is to be fired in an oxidizing atmosphere, is provided on a ceramic multilayer substrate, the improvement comprises that a conductive layer of the ceramic thick film circuit substrate to which the thick film conductor is connected, is composed of tungsten, and at least one of platinum and palladium, and that platinum is 0.1-100 parts by weight in the case of platinum alone, palladium is 0.1-20 parts by weight in the case of palladium alone, and a total amount of platinum and palladium is 0.1-76 parts by weight in the case of combination of these elements provided that palladium is 20 parts by weight or less, the part by weight of platinum and palladium being based on 100 parts by weight of tungsten.
Claim 2
Dependent Claim 137 words
In a ceramic thick film circuit substrate in which a thick film conductor which is to be fired in an oxidizing atmosphere, is provided on a ceramic multilayer substrate, the improvement comprises that a conductive layer of the ceramic thick film circuit substrate to which the thick film conductor is connected, is composed of tungsten, and at least one of platinum and palladium, and that platinum is 0.1-100 parts by weight in the case of platinum alone, palladium is 0.1-20 parts by weight in the case of palladium alone, and a total amount of platinum and palladium is 0.1-76 parts by weight in the case of combination of these elements provided that palladium is 20 parts by weight or less, the part by weight of platinum and palladium being based on 100 parts by weight of tungsten.

References Cited (Backward Citations)

US1096655A Cited
GB157988A Cited
US1779603A Cited
US2094570A Cited
US3838204A Cited
US3511640A Cited
US3872360A Cited
US3912611A Cited
US4155660A Cited
US4434544A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-07-15 1989-01-14 1989-07-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-07-15 1993-01-14 1993-07-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-07-15 1997-01-14 1997-07-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag