US4529672A Expired / Lapsed US ⏱️ 0.0 years remaining

Process of making electrochemical electrodes and electrodes made thereby

Assignee: Graftech Technology LLC
•
Filing: 1983-03-29
•
Granted: 1985-07-16
•
Expires: 2003-03-29
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for making an improved electrode by providing on a conductive current distributor layers of active and hydrophobic materials, uniting these materials together with sufficient force to lock them together and subsequently roll-bonding the resulting preformed assembly to form the finished electrode.

Inventors

  • 👤 Ronald A. Howard
  • 👤 Paul S. Sirocky

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 19:36
CPC Classifications
H; H01; H01M; H01M4/00; H01M4/86; H01M4/88; H01M4/8878; H01M4/8896; H01M4/8663; H01M4/8668; H01M4/8673; H01M4/96; Y; Y02; Y02E; Y02E60/00; Y02E60/30; Y02E60/50

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 134 words
A process for making an electrode comprising the steps: (a) providing an electrochemically active material; (b) providing a hydrophobic material; (c) placing on a conductive current distributor a first layer of said electrochemically active material and a second layer of said hydrophobic material over said first layer to produce an unbonded electrode; (d) applying a pressure of 0.1 to 5 tons per square inch on the face area of the unbonded electrode in step (c) so as to only lock said first layer, said second layer and said conductive current distributor together to produce an electrode assembly; and (e) roll-bonding said assembly of step (d) between counter-rotating rollers so as to exert a linear force pressure of from 0.1 to 10 tons per linear inch on said electrode assembly to produce a bonded electrode.
Claim 2
Dependent Claim 134 words
A process for making an electrode comprising the steps: (a) providing an electrochemically active material; (b) providing a hydrophobic material; (c) placing on a conductive current distributor a first layer of said electrochemically active material and a second layer of said hydrophobic material over said first layer to produce an unbonded electrode; (d) applying a pressure of 0.1 to 5 tons per square inch on the face area of the unbonded electrode in step (c) so as to only lock said first layer, said second layer and said conductive current distributor together to produce an electrode assembly; and (e) roll-bonding said assembly of step (d) between counter-rotating rollers so as to exert a linear force pressure of from 0.1 to 10 tons per linear inch on said electrode assembly to produce a bonded electrode.
Claim 3
Dependent Claim 48 words
The process of claim 1 wherein a pore-former is included in at least one of the layers selected from the group consisting of said first layer and said second layer and wherein after step (e) the following step is added: (f) removing said pore-former from the bonded electrode.
Claim 4
Dependent Claim 13 words
The process of claim 1 wherein step (e) is repeated at least once.
Claim 5
Dependent Claim 13 words
The process of claim 2 wherein step (e) is repeated at least once.
Claim 6
Dependent Claim 21 words
The process of claims 1, 2, 3 or 4 wherein in step (a) said first layer comprises activated carbon and polytetrafluoroethylene.
Claim 7
Dependent Claim 18 words
The process of claims 1, 2, 3 or 4 wherein in step (b) said second layer comprises polytetrafluoroethylene.
Claim 8
Dependent Claim 40 words
The process of claims 1, 2, 3 or 4 wherein said conductive current distributor in step (c) is a material selected from the group consisting of metals, metal alloys, metals plated with noble metals, and alloys plated with noble metals.
Claim 9
Dependent Claim 32 words
An electrode made by the process of claims 1, 2, 3 or 4 and characterized by said bonded electrode having a disbond strength of about 5 to 30 pounds per square inch.

References Cited (Backward Citations)

US3158510A Cited
US3594236A Cited
US3647617A Cited
US4152489A Cited
US4370284A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-07-15 1989-01-14 1989-07-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-07-15 1993-01-14 1993-07-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-07-15 1997-01-14 1997-07-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag