In a method of purifying uraniferous aqueous solutions containing impurities comprising at least one of the elements zirconium and/or hafnium, and also containing at least one of the anions SO 4 = , NO 3 - , Cl - or F - , said anions acting as complexing agents for the uranium and impurities, said impurities being precipitated by means of an alkaline agent, said method comprising the following steps carried out for the purpose of selectively and quantitatively separating the impurities from the uranium: (a) bringing said uraniferous solution to a temperature of at least 40° C.; (b) adjusting the content of complexing agent to bring the molar ratio: [complexing agent]/[soluble U+Zr and/or Hf] to at least 3; (c) introducing an alkaline agent to adjust the pH of said solution to between 2.2 and 4.3; and (d) separating the alkaline-treated solution into a solid phase and a liquid phase, said liquid phase comprising a purified uraniferous solution, and said solid phase comprising a zirconium and/or hafnium precipitate.
Claim 2
Dependent Claim
168 words
In a method of purifying uraniferous aqueous solutions containing impurities comprising at least one of the elements zirconium and/or hafnium, and also containing at least one of the anions SO 4 = , NO 3 - , Cl - or F - , said anions acting as complexing agents for the uranium and impurities, said impurities being precipitated by means of an alkaline agent, said method comprising the following steps carried out for the purpose of selectively and quantitatively separating the impurities from the uranium: (a) bringing said uraniferous solution to a temperature of at least 40° C.; (b) adjusting the content of complexing agent to bring the molar ratio: [complexing agent]/[soluble U+Zr and/or Hf] to at least 3; (c) introducing an alkaline agent to adjust the pH of said solution to between 2.2 and 4.3; and (d) separating the alkaline-treated solution into a solid phase and a liquid phase, said liquid phase comprising a purified uraniferous solution, and said solid phase comprising a zirconium and/or hafnium precipitate.
Claim 3
Dependent Claim
24 words
The method of claim 1, wherein said uraniferous solution is brought to a temperature between 80° C. and the boiling point of the solution.
Claim 4
Independent Claim
25 words
The method of any of claims 1 or 2, wherein the content of complexing agent is adjusted to a molar ratio of at least 5.
Claim 5
Dependent Claim
22 words
The method of claim 3, wherein the alkaline agent is selected from the group comprising alkaline and ammonium hydroxides, carbonates and bicarbonates.
Claim 6
Dependent Claim
19 words
The method of claim 3, wherein the alkaline agent is introduced over a period of at least 10 minutes.
Claim 7
Dependent Claim
26 words
The method of claim 3, wherein the alkaline agent is introduced in the form of an aqueous solution with a molar concentration no greater than four.
Claim 8
Dependent Claim
23 words
The method of claim 3, wherein a fraction of the zirconium and/or hafnium precipitate obtained in step (d) is recycled to step (a).