← Back to Patent Explorer
US4521459A Expired / Lapsed US ⏱️ 0.0 years remaining

Coating method and apparatus

Assignee: Fujifilm Holdings Corp
•
Filing: 1983-05-19
•
Granted: 1985-06-04
•
Expires: 2003-05-19
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In a coating method, a coating section is arranged immediately before a coil bar while a smoother is disposed immediately after the coil bar, immediately after a coating solution is applied to a web which is run continuously a surplus of coating solution is scraped off and the web is subjected to smoothing by the smoother directly without undergoing a gaseous phase.

Inventors

  • 👤 Hideo Takeda

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 11:30
CPC Classifications
B; B05; B05D; B05D1/00; B05D1/26; B05C; B05C11/00; B05C11/02; B05C11/023; B05C11/025; B05D1/40; B05C3/00; B05C3/18

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 94 words
In a coating method which comprises applying a coating solution to a continuously running web, the improvement comprising the steps of; applying a coating solution to said running web from a coating section arranged immediately upstream of a coil bar with a smoother disposed immediately downstream of a coil bar, immediately after the coating solution is applied to the web scraping off surplus coating solution from the web by contact of said coating solution and said coil bar and, immediately smoothing by said smoother directly without having said coating solution undergoing a gaseous phase.
Claim 2
Dependent Claim 94 words
In a coating method which comprises applying a coating solution to a continuously running web, the improvement comprising the steps of; applying a coating solution to said running web from a coating section arranged immediately upstream of a coil bar with a smoother disposed immediately downstream of a coil bar, immediately after the coating solution is applied to the web scraping off surplus coating solution from the web by contact of said coating solution and said coil bar and, immediately smoothing by said smoother directly without having said coating solution undergoing a gaseous phase.
Claim 3
Dependent Claim 19 words
The method of claim 1 wherein said coil bar rotates in the same direction as movement of said web.
Claim 4
Dependent Claim 33 words
The method of claim 1 further comprising the steps of disposing guide rollers upstream and downstream of said coating section, said guide rolls rotating in the same direction as movement of said web.
Claim 5
Dependent Claim 96 words
Apparatus of the extruder type for coating a web with a coating solution comprising: a coating solution supplying extruder outlet at the upper portion of a supply slot, a coil bar disposed at the rear of and adjacent to the supply slot and a smoother arranged at the rear of the coil bar and adjacent to the coil bar, wherein immediately after a coating solution is applied to a web which is continuously run surplus coating solution is scraped off and the web is subjected to smoothing by the smoother directly without undergoing a gaseous phase.
Claim 6
Dependent Claim 96 words
Apparatus of the extruder type for coating a web with a coating solution comprising: a coating solution supplying extruder outlet at the upper portion of a supply slot, a coil bar disposed at the rear of and adjacent to the supply slot and a smoother arranged at the rear of the coil bar and adjacent to the coil bar, wherein immediately after a coating solution is applied to a web which is continuously run surplus coating solution is scraped off and the web is subjected to smoothing by the smoother directly without undergoing a gaseous phase.
Claim 7
Dependent Claim 25 words
The apparatus of claim 4 further comprising a holder for said coil bar, one wall of said holder forming a wall of said supply slot.
Claim 8
Dependent Claim 20 words
The apparatus of claim 4 further comprising said extruder outlet facing in the downstream direction and confronting said coil bar.
Claim 9
Dependent Claim 24 words
The apparatus of claim 4 comprising a slide surface inclined downward and positioned upstream relative to said extruder outlet to remove excess coating solution.
Claim 10
Dependent Claim 28 words
A coating apparatus as claimed in claim 4, wherein the top surface of the coil bar and the top surface of the smoother are substantially equal in level.
Claim 11
Dependent Claim 24 words
The apparatus of claim 4 further comprising guide rolls positioned upstream of said extruder outlet and downstream of said smoother to guide said web.
Claim 12
Dependent Claim 122 words
In a coating method which comprises applying a coating solution to a continuously running web, the improvement comprising the steps of delivering a coating solution from a coating section having a source and arranged immediately upstream of a coil bar with a smoother disposed immediately downstream of a coil bar, applying said coating solution to said running web through an extension slot, immediately after the coating solution is applied to the web scraping off surplus coating solution from the web by contact of said coating solution and said coil bar, removing said surplus coating solution by transfer to a slide surface upstream of said extrusion slot and, immediately smoothing by said smoother directly without having said coating solution undergoing a gaseous phase.
Claim 13
Dependent Claim 122 words
In a coating method which comprises applying a coating solution to a continuously running web, the improvement comprising the steps of delivering a coating solution from a coating section having a source and arranged immediately upstream of a coil bar with a smoother disposed immediately downstream of a coil bar, applying said coating solution to said running web through an extension slot, immediately after the coating solution is applied to the web scraping off surplus coating solution from the web by contact of said coating solution and said coil bar, removing said surplus coating solution by transfer to a slide surface upstream of said extrusion slot and, immediately smoothing by said smoother directly without having said coating solution undergoing a gaseous phase.

References Cited (Backward Citations)

US2285041A Cited
DE1964908A1 Cited
GB2046138A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-06-03 1988-12-03 1989-06-04 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-06-03 1992-12-03 1993-06-04 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-06-03 1996-12-03 1997-06-04 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag