Claims Analysis
Total Claims: 16
Claim 1
Independent Claim
149 words
An assembly for machining patterns comprising: (a) a fastening plate which is shaped for mounting in a machine tool; (b) a block of machinable wax, the wax block comprising a mixture of: 5 to 15 percent by volume paraffin wax having a melting point of substantially 150° F. to 152° F., 5 to 15 percent by volume microcrystalline wax, 5 to 10 percent by volume ethylene/vinyl acetate copolymer, 40 to 50 percent by volume nonemulsifiable polyethylene wax having a melting point of substantially 220° F., a hardness of generally 4 dmm., and a Brookfield viscosity at 302° F. of about 9400 cps, 25 to 35 percent by volume nonemulsifiable polyethylene wax having a melting point of substantially 240° F., a hardness of generally 1 dmm., and a viscosity at 284° F. of about 350 cps; and, (c) anchoring means for anchoring the machinable wax block to the fastening plate.
Claim 2
Dependent Claim
149 words
An assembly for machining patterns comprising: (a) a fastening plate which is shaped for mounting in a machine tool; (b) a block of machinable wax, the wax block comprising a mixture of: 5 to 15 percent by volume paraffin wax having a melting point of substantially 150° F. to 152° F., 5 to 15 percent by volume microcrystalline wax, 5 to 10 percent by volume ethylene/vinyl acetate copolymer, 40 to 50 percent by volume nonemulsifiable polyethylene wax having a melting point of substantially 220° F., a hardness of generally 4 dmm., and a Brookfield viscosity at 302° F. of about 9400 cps, 25 to 35 percent by volume nonemulsifiable polyethylene wax having a melting point of substantially 240° F., a hardness of generally 1 dmm., and a viscosity at 284° F. of about 350 cps; and, (c) anchoring means for anchoring the machinable wax block to the fastening plate.
Claim 3
Dependent Claim
19 words
The assembly as set forth in claim 1 wherein the ethylene/vinyl acetate copolymer is substantially 18 percent vinyl acetate.
Claim 4
Dependent Claim
50 words
The assembly as set forth in claim 1 wherein the paraffin wax is substantially 10 percent by volume of the wax block, the microcrystalline wax is substantially 10 percent by volume of the wax block, and the ethylene/vinyl acetate copolymer is substantially 5 percent by volume of the wax block.
Claim 5
Dependent Claim
50 words
The assembly as set forth in claim 3 wherein the nonemulsifiable polyethylene wax having the 240° F. melting point is substantially 30 percent by volume of the wax block and the nonemulsifiable polyethylene wax having the 220° F. melting point is substantially 45 percent by volume of the wax block.
Claim 6
Dependent Claim
20 words
The assembly as set forth in claim 4 wherein the wax block further includes a dark colored oil base dye.
Claim 7
Dependent Claim
13 words
The assembly as set forth in claim 5 wherein the dye is blue.
Claim 8
Dependent Claim
27 words
The assembly as set forth in claim 1 further including a layer of adhesive disposed between the wax block and the fastening plate to anchor them together.
Claim 9
Dependent Claim
110 words
An assembly for machining prototype patterns with tolerances in the range of 0.001 inches or better, the assembly comprising: (a) holding means for stably holding a wax block during a machining operation; (b) anchoring means for anchoring the wax block to the holding means; and, (c) the wax block comprising a mixture of: (i) 40-50 percent nonemulsifiable polyethylene wax having a melting point of about 220° F.; (ii) 24-35 percent nonemulsifiable polyethylene wax having a melting point of at least 230° F.; (iii) 10-30 percent hydrocarbon wax including paraffin, microcrystalline wax, and mixtures thereof; and, (iv) 5-10 percent resin which improves compatibility between the hydrocarbon wax and the polyethylene waxes.
Claim 10
Dependent Claim
110 words
An assembly for machining prototype patterns with tolerances in the range of 0.001 inches or better, the assembly comprising: (a) holding means for stably holding a wax block during a machining operation; (b) anchoring means for anchoring the wax block to the holding means; and, (c) the wax block comprising a mixture of: (i) 40-50 percent nonemulsifiable polyethylene wax having a melting point of about 220° F.; (ii) 24-35 percent nonemulsifiable polyethylene wax having a melting point of at least 230° F.; (iii) 10-30 percent hydrocarbon wax including paraffin, microcrystalline wax, and mixtures thereof; and, (iv) 5-10 percent resin which improves compatibility between the hydrocarbon wax and the polyethylene waxes.
Claim 11
Dependent Claim
111 words
An assembly for machinin prototype patterns with tolerances in the range of 0.001 inches or better, the assembly comprising: (a) holding means for stably holding a wax block during a machining operation; (b) anchoring means for anchoring the wax block to the holding means; and, (c) the wax block comprising a mixture of: (i) 50-85 percent nonemulsifiable polyethylene wax having a density of 0.90-0.94 grams per cubic centimeter at 77° F.; (ii) at least 5 percent hydrocarbon wax which lowers the melting point of the mixture and acts as a lubricant; and, (iii) at least 5 percent synthetic resin which includes a vinyl acetate polymeric component to improve hydrocarbon wax compatibility.
Claim 12
Dependent Claim
111 words
An assembly for machinin prototype patterns with tolerances in the range of 0.001 inches or better, the assembly comprising: (a) holding means for stably holding a wax block during a machining operation; (b) anchoring means for anchoring the wax block to the holding means; and, (c) the wax block comprising a mixture of: (i) 50-85 percent nonemulsifiable polyethylene wax having a density of 0.90-0.94 grams per cubic centimeter at 77° F.; (ii) at least 5 percent hydrocarbon wax which lowers the melting point of the mixture and acts as a lubricant; and, (iii) at least 5 percent synthetic resin which includes a vinyl acetate polymeric component to improve hydrocarbon wax compatibility.
Claim 13
Dependent Claim
20 words
The assembly as set forth in claim 9 wherein the hydrocarbon wax is a mixture of paraffin and microcrystaline wax.
Claim 14
Dependent Claim
18 words
The assembly as set forth in claim 9 wherein the synthetic resin is about 18 percent vinyl acetate.
Claim 15
Dependent Claim
24 words
The assembly as set forth in claim 9 wherein the wax block has a dark blue pigmentation to facilitate visual examination of machined surfaces.
Claim 16
Dependent Claim
47 words
The assembly as set forth in claim 9 wherein the nonemulsifiable polyethylene wax comprises 25 to 35 percent by volume nonemulsifiable polyethylene wax with a hardness of substantially 1 dmm. and 40 to 50 percent by volume nonemulsifiable polyethylene wax having a hardness of generally 4 dmm.