Abstract

Abstract Method for making a window weather stripping having a rough surface including extruding a rubber weather strip material, curing and coating the vulcanized strip with a nylon-based adhesive containing nylon particles.

Inventors

  • 👤 Toshiaki Yamaguchi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 19:19
CPC Classifications
B; B60; B60J; B60J10/00; B60J10/15; B60J10/17; Y; Y10; Y10T; Y10T428/00; Y10T428/24; Y10T428/2419; Y10T428/24198

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 102 words
A method of manufacturing window weather stripping having a rough surface for sealing a gap between a movable glass and a window frame, which comprises the following steps of: (1) extrusion-molding a rubber material into the shape of window weather stripping; (2) vulcanizing the extrusion-molded rubber material to form a vulcanized rubber material; (3) applying a paint consisting essentially of nylon particles contained in a nylon-based bonding agent onto at least one sliding surface of the vulcanized rubber material so that the nylon particles form at least one rough surface; (4) drying the paint-containing nylon particles; and (5) baking the dried paint.
Claim 2
Independent Claim 102 words
A method of manufacturing window weather stripping having a rough surface for sealing a gap between a movable glass and a window frame, which comprises the following steps of: (1) extrusion-molding a rubber material into the shape of window weather stripping; (2) vulcanizing the extrusion-molded rubber material to form a vulcanized rubber material; (3) applying a paint consisting essentially of nylon particles contained in a nylon-based bonding agent onto at least one sliding surface of the vulcanized rubber material so that the nylon particles form at least one rough surface; (4) drying the paint-containing nylon particles; and (5) baking the dried paint.
Claim 3
Dependent Claim 42 words
A method of manufacturing window weather stripping for sealing a gap between a movable glass and a window frame, as set forth in claim 1, wherein the step of painting the paint with nylon particles is performed by a roller painting machine.
Claim 4
Dependent Claim 88 words
A method of manufacturing window weather stripping for sealing a gap between a movable glass and a window frame, as set forth in claim 1, which further comprises the step of painting a thermoplastic synthetic resin film onto the rough surface of the paint with nylon particles to such an extent that the thickness of the resin film is less than the diameter of the nylon particles, said step of forming a thermoplastic synthetic resin film being performed after the step of drying the paint with nylon particles.
Claim 5
Dependent Claim 42 words
A method of manufacturing window weather stripping for sealing a gap between a movable glass and a window frame, as set forth in claim 3, wherein the step of painting the thermoplastic synthetic resin film is performed by a roller painting machine.
Claim 6
Independent Claim 109 words
A method of manufacturing window weather stripping having a rough surface for sealing a gap between a movable glass and a window frame, which comprises the following steps of: (1) extrusion-molding a rubber material into the shape of window weather stripping; (2) applying a paint consisting essentially of nylon particles contained in a nylon-based bonding agent onto at least one sliding surface of the extrusion-molded rubber material so that the nylon particles form at least one rough surface; (3) drying the paint-containing nylon particles by application of heat generated in the extrusion-molding step; and (4) vulcanizing the extrusion-molded rubber material and baking the dried paint at the same time.
Claim 7
Independent Claim 109 words
A method of manufacturing window weather stripping having a rough surface for sealing a gap between a movable glass and a window frame, which comprises the following steps of: (1) extrusion-molding a rubber material into the shape of window weather stripping; (2) applying a paint consisting essentially of nylon particles contained in a nylon-based bonding agent onto at least one sliding surface of the extrusion-molded rubber material so that the nylon particles form at least one rough surface; (3) drying the paint-containing nylon particles by application of heat generated in the extrusion-molding step; and (4) vulcanizing the extrusion-molded rubber material and baking the dried paint at the same time.
Claim 8
Dependent Claim 42 words
A method of manufacturing window weather stripping for sealing a gap between a movable glass and a window frame, as set forth in claim 5, wherein the step of painting the paint with nylon particles is performed by a roller painting machine.
Claim 9
Dependent Claim 88 words
A method of manufacturing window weather stripping for sealing a gap between a movable glass and a window frame, as set forth in claim 5, which further comprises the step of painting a thermoplastic synthetic resin film onto the rough surface of the paint with nylon particles to such an extent that the thickness of the resin film is less than the diameter of the nylon particles, said step of forming a thermoplastic synthetic resin film being performed after the step of drying the paint with nylon particles.
Claim 10
Dependent Claim 42 words
A method of manufacturing window weather stripping for sealing a gap between a movable glass and a window frame, as set forth in claim 7, wherein the step of painting the thermoplastic synthetic resin film is performed by a roller painting machine.

References Cited (Backward Citations)

US1251182A Cited
US2175099A Cited
US2289777A Cited
US3969232A Cited
US4035436A Cited
US4103385A Cited
US4226823A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-04-15 1988-10-15 1989-04-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-04-15 1992-10-15 1993-04-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-04-15 1996-10-15 1997-04-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag