← Back to Patent Explorer
US4508673A Expired / Lapsed US ⏱️ 0.0 years remaining

Molding of glass wool with wrinkle-free surface

Assignee: Owens Corning Fiberglas Technology Inc
•
Filing: 1984-05-04
•
Granted: 1985-04-02
•
Expires: 2004-05-04
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The process includes a first molding step with an upper surface of the glass wool pelt having been sprayed with water and with a lower surface of the glass wool pelt insulated from the lower mold portion by a previously molded glass wool insulating sheet, and a second molding step with the insulating sheet removed.

Inventors

  • 👤 Steven B. Stahl
  • 👤 Shiv K. Bakhshi
  • 👤 George M. Naul

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 14:04
CPC Classifications
B; B29; B29C; B29C70/00; B29C70/04; B29C70/28; B29C70/40; B29C70/42; B29C70/46; D; D04; D04H; D04H1/00; D04H1/40; D04H1/42; D04H1/4209; D04H1/4218; D04H1/58; B29C2791/00; B29C2791/001; B29K; B29K2105/00; B29K2105/06; B29K2105/08; B29K2105/0854; B29K2503/00; B29K2503/04; B29L; B29L2031/00; B29L2031/30; B29L2031/3005

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 114 words
A process of molding a wool batt comprising mineral or glass wool with uncured thermosettable binder to produce a molded mineral or glass wool part with a wrinkle-free surface, said process comprising subjecting the wool batt to an initial molding step between heated molds after moistening the surface which is to be wrinkle-free, said initial molding step being carried out with an insulating sheet on the side of the wool batt opposite the moistened surface and resulting in a partially cured wrinkle-free skin at the surface which was moistened, and subjecting the wool batt to a second molding step between heated molds without the insulating sheet to cure the wool batt throughout its thickness.
Claim 2
Dependent Claim 114 words
A process of molding a wool batt comprising mineral or glass wool with uncured thermosettable binder to produce a molded mineral or glass wool part with a wrinkle-free surface, said process comprising subjecting the wool batt to an initial molding step between heated molds after moistening the surface which is to be wrinkle-free, said initial molding step being carried out with an insulating sheet on the side of the wool batt opposite the moistened surface and resulting in a partially cured wrinkle-free skin at the surface which was moistened, and subjecting the wool batt to a second molding step between heated molds without the insulating sheet to cure the wool batt throughout its thickness.
Claim 3
Dependent Claim 143 words
A process of molding a wool batt comprising mineral or glass wool with uncured thermosettable binder in a molding press to produce a molded mineral or glass wool part with a wrinkle-free surface, said process comprising placing a molded mineral or glass wool insulating sheet previously molded in the same or a similar molding press on a heated lower mold portion of the press, moistening a surface of the wool batt and placing the wool batt over the molded insulating sheet with the moistened surface facing a heated upper mold portion of the press, closing the press long enough to produce a wrinkle-free skin at the moistened surface, opening the press and removing the molded insulating sheet, closing the press long enough to cure the wool batt throughout its thickness, and opening the press and removing the molded mineral or glass wool part.
Claim 4
Dependent Claim 143 words
A process of molding a wool batt comprising mineral or glass wool with uncured thermosettable binder in a molding press to produce a molded mineral or glass wool part with a wrinkle-free surface, said process comprising placing a molded mineral or glass wool insulating sheet previously molded in the same or a similar molding press on a heated lower mold portion of the press, moistening a surface of the wool batt and placing the wool batt over the molded insulating sheet with the moistened surface facing a heated upper mold portion of the press, closing the press long enough to produce a wrinkle-free skin at the moistened surface, opening the press and removing the molded insulating sheet, closing the press long enough to cure the wool batt throughout its thickness, and opening the press and removing the molded mineral or glass wool part.
Claim 5
Dependent Claim 31 words
A molding process as claimed in claim 2 wherein the upper and lower mold portions of the press are heated to a temperature of from 205 degrees to 260 degrees C.
Claim 6
Dependent Claim 32 words
A molding process as claimed in claim 3 wherein the press is closed for from 20 to 40 seconds the first time and for from 30 to 60 seconds the second time.
Claim 7
Dependent Claim 111 words
A process of molding a wool batt comprising mineral or glass wool with uncured thermosettable binder to produce a molded mineral or glass wool part with a wrinkle-free surface, said process comprising subjecting the wool batt to an initial molding step between heated molds, said initial molding step being carried out with an insulating sheet on the side of the wool batt opposite the surface which is to be wrinkle-free and resulting in a partially cured wrinkle-free skin at the surface which is to be wrinkle-free, and subjecting the wool batt to a second molding step between heated molds without the insulating sheet to cure the wool batt throughout its thickness.
Claim 8
Dependent Claim 111 words
A process of molding a wool batt comprising mineral or glass wool with uncured thermosettable binder to produce a molded mineral or glass wool part with a wrinkle-free surface, said process comprising subjecting the wool batt to an initial molding step between heated molds, said initial molding step being carried out with an insulating sheet on the side of the wool batt opposite the surface which is to be wrinkle-free and resulting in a partially cured wrinkle-free skin at the surface which is to be wrinkle-free, and subjecting the wool batt to a second molding step between heated molds without the insulating sheet to cure the wool batt throughout its thickness.
Claim 9
Dependent Claim 151 words
A process of molding a wool batt comprising mineral or glass wool with uncured thermosettable binder in a molding press to produce a molded mineral or glass wool part with a wrinkle-free surface, said process comprising placing a molded mineral or glass wool insulating sheet previously molded in the same or a similar molding press on a heated lower mold portion of the press, placing the wool batt over the molded insulating sheet with the surface which is to be wrinkle-free facing a heated upper mold portion of the press, closing the press long enough to produce a wrinkle-free skin on the side of the wool batt facing the heated upper mold portion of the press, opening the press and removing the molded insulating sheet, closing the press long enough to cure the wool batt throughout its thickness, and opening the press and removing the molded mineral or glass wool part.
Claim 10
Dependent Claim 151 words
A process of molding a wool batt comprising mineral or glass wool with uncured thermosettable binder in a molding press to produce a molded mineral or glass wool part with a wrinkle-free surface, said process comprising placing a molded mineral or glass wool insulating sheet previously molded in the same or a similar molding press on a heated lower mold portion of the press, placing the wool batt over the molded insulating sheet with the surface which is to be wrinkle-free facing a heated upper mold portion of the press, closing the press long enough to produce a wrinkle-free skin on the side of the wool batt facing the heated upper mold portion of the press, opening the press and removing the molded insulating sheet, closing the press long enough to cure the wool batt throughout its thickness, and opening the press and removing the molded mineral or glass wool part.
Claim 11
Dependent Claim 31 words
A molding process as claimed in claim 6 wherein the upper and lower mold portions of the press are heated to a temperature of from 205 degrees to 260 degrees C.
Claim 12
Dependent Claim 32 words
A molding process as claimed in claim 7 wherein the press is closed for from 20 to 40 seconds the first time and for from 30 to 60 seconds the second time.

References Cited (Backward Citations)

CA754055A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-04-01 1988-10-01 1989-04-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-04-01 1992-10-01 1993-04-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-04-01 1996-10-01 1997-04-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag