Abstract

Abstract A method of ameliorating high-temperature slagging conditions which result from impaction on the boiler interior surfaces of molten or semi-molten ash particles in flue gas resulting from the combustion of fuel. The method comprises adding a conditioner to the flue gas at or upstream of the high temperature region in the boiler system where slagging tends to occur, and thereafter causing the mixed flue gas and conditioner to flow through the region. Suitable conditioners include strontium carbonate, a mixture of zircon with copper oxychloride and a mixture of alumina with aluminum fluoride, zircon, or zirconyl chloride.

Inventors

  • 👤 Alfred E. Kober
  • 👤 Christopher J. Macey

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 19:18
CPC Classifications
C; C10; C10L; C10L10/00; C10L10/04; C10L10/06

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 122 words
A method of ameliorating high-temperature slagging conditions which result from impaction on the boiler interior surfaces of molten or semi-molten ash particles in flue gas resulting from the combustion of coal, which method comprises (a) at or upstream of the high-temperature region in said boiler system where slagging tends to occur, adding to said flue gas a conditioner selected from the group consisting of strontium carbonate, a mixture of zircon with copper oxychloride, a mixture of alumina with aluminum fluoride, zircon or zirconyl chloride, and a mixture of hydrated aluminum silicate, unexpanded perlite ore, unexpanded vermiculite ore or strontium carbonate with copper oxychloride, zircon, or zirconyl chloride; and (b) thereafter causing said mixed flue gas and conditioner to flow through said region.
Claim 2
Independent Claim 122 words
A method of ameliorating high-temperature slagging conditions which result from impaction on the boiler interior surfaces of molten or semi-molten ash particles in flue gas resulting from the combustion of coal, which method comprises (a) at or upstream of the high-temperature region in said boiler system where slagging tends to occur, adding to said flue gas a conditioner selected from the group consisting of strontium carbonate, a mixture of zircon with copper oxychloride, a mixture of alumina with aluminum fluoride, zircon or zirconyl chloride, and a mixture of hydrated aluminum silicate, unexpanded perlite ore, unexpanded vermiculite ore or strontium carbonate with copper oxychloride, zircon, or zirconyl chloride; and (b) thereafter causing said mixed flue gas and conditioner to flow through said region.
Claim 3
Dependent Claim 11 words
The method of claim 1 wherein said conditioner is strontium carbonate.
Claim 4
Dependent Claim 37 words
The method of claim 1 wherein said conditioner is a synergistic mixture selected from the group consisting of a mixture of zircon with copper oxychloride and a mixture of alumina with aluminum fluoride, zircon, or zirconyl chloride.
Claim 5
Dependent Claim 31 words
The method of claim 3 wherein said conditioner mixtures comprise from 50 to 98% by weight of the first ingredient and from 50 to 2% by weight of the second ingredient.
Claim 6
Dependent Claim 11 words
The method of claim 3 wherein said alumina is hydrated alumina.
Claim 7
Dependent Claim 32 words
The method of claim 1, in which said conditioner is initially added to said flue gas in the form of particles of said conditioner of or precursors thereof under flue gas conditions.
Claim 8
Dependent Claim 27 words
The method of claim 1 in which said conditioner is added to said flue gas by being introduced into the combustion region when said coal is burned.
Claim 9
Dependent Claim 20 words
The method of claim 1, in which said conditioner is injected into said flue gas downstream of the combustion region.
Claim 10
Dependent Claim 26 words
The method of claim 1, in which said conditioner is provided at a rate of about 0.1-10.0% by weight of the ash content of said coal.
Claim 11
Dependent Claim 26 words
The method of claim 9, in which said conditioner is provided at a rate of about 0.2-5.0% by weight of the ash content of said coal.
Claim 12
Dependent Claim 26 words
The method of claim 10, in which said conditioner is provided at a rate of about 0.2-2.0% by weight of the ash content of said coal.
Claim 13
Dependent Claim 131 words
A fly ash conditioner for use in a method of ameliorating high-temperature slagging conditions which result from impaction on the boiler interior surfaces of molten or semi-molten ash particles in flue gas resulting from the combustion of coal, which method comprises, at or upstream of the high-temperature region in the boiler system where slagging tends to occur, adding to the flue gas a conditioner and thereafter causing the mixed flue gas and conditioner to flow through the said region, said conditioner being selected from the group consisting of strontium carbonate, a mixture of zircon with copper oxychloride, a mixture of alumina with aluminum fluoride, zircon or zirconyl chloride, and a mixture of hydrated aluminum silicate, unexpanded perlite ore, unexpanded vermiculite ore or strontium carbonate with copper oxychloride, zircon, or zirconyl chloride.
Claim 14
Dependent Claim 131 words
A fly ash conditioner for use in a method of ameliorating high-temperature slagging conditions which result from impaction on the boiler interior surfaces of molten or semi-molten ash particles in flue gas resulting from the combustion of coal, which method comprises, at or upstream of the high-temperature region in the boiler system where slagging tends to occur, adding to the flue gas a conditioner and thereafter causing the mixed flue gas and conditioner to flow through the said region, said conditioner being selected from the group consisting of strontium carbonate, a mixture of zircon with copper oxychloride, a mixture of alumina with aluminum fluoride, zircon or zirconyl chloride, and a mixture of hydrated aluminum silicate, unexpanded perlite ore, unexpanded vermiculite ore or strontium carbonate with copper oxychloride, zircon, or zirconyl chloride.
Claim 15
Dependent Claim 11 words
The conditioner of claim 12 wherein said conditioner is strontium carbonate.
Claim 16
Dependent Claim 37 words
The conditioner of claim 1 wherein said conditioner is a synergistic mixture selected from the group consisting of a mixture of zircon with copper oxychloride and a mixture of alumina with aluminum fluoride, zircon, or zirconyl chloride.
Claim 17
Dependent Claim 11 words
The method of claim 12 wherein said alumina is hydrated alumina.

References Cited (Backward Citations)

US4245573A Cited
US4369719A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-02-12 1988-08-13 1989-02-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-02-12 1992-08-13 1993-02-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-02-12 1996-08-13 1997-02-12 $7700.00 Window Closed / Lapsed