Nondestructive testing of stress in a ferromagnetic structural material utilizing magnetically induced velocity change measurements

Assignee: Southwest Research Institute
•
Filing: 1983-07-12
•
Granted: 1985-02-05
•
Expires: 2003-07-12
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract This disclosure relates to a nondestructive method of measuring stress in a ferromagnetic structural material. One method involves the measurement of the change in ultrasonic velocity induced by an externally applied magnetic field; the method enables nondestructively determining the magnitude, the direction, and the sign (i.e., tensile or compressive) of a stress in a ferromagnetic material. The magnetically induced velocity change of an ultrasonic wave is caused by the magnetoelastic coupling in the ferromagnetic material. This magnetically induced velocity change is characteristically dependent on the magnitude and the sign of the stress and also on the relative orientation of the stress, the magnetic field, and the polarization and propagation direction of the ultrasonic wave. The dependence of magnetically induced velocity changes can be utilized for nondestructive stress measurements. In one version, for measuring bulk stresses, either a longitudinal ultrasonic wave or a shear ultrasonic wave is used. In another version, for measuring surface stresses, a surface ultrasonic wave is preferably used. By using surface waves at several different frequencies, a stress gradient can also be determined.

Inventors

  • 👤 Hegeon Kwun
  • 👤 II Cecil M. Teller

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 00:59
CPC Classifications
G; G01; G01N; G01N27/00; G01N27/72; G01N27/725; G01N29/00; G01N29/04; G01N29/07; G01N2291/00; G01N2291/02; G01N2291/028; G01N2291/02863

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 79 words
A method of determining the stress in a ferromagnetic material specimen comprising the steps of: (a) propagating an ultrasonic wave of suitable frequency and mode in a given direction through the specimen and detecting such a propagated wave; (b) applying a magnetic field to the specimen of a specified strength; and (c) measuring the change in velocity of the propagated ultrasonic wave in the specimen having the applied magnetic field to obtain an indication of stress in the specimen.
Claim 2
Independent Claim 79 words
A method of determining the stress in a ferromagnetic material specimen comprising the steps of: (a) propagating an ultrasonic wave of suitable frequency and mode in a given direction through the specimen and detecting such a propagated wave; (b) applying a magnetic field to the specimen of a specified strength; and (c) measuring the change in velocity of the propagated ultrasonic wave in the specimen having the applied magnetic field to obtain an indication of stress in the specimen.
Claim 3
Dependent Claim 32 words
The method of claim 1 including the step of positioning a magnet having spaced pole faces against the specimen, and further forming a fixed field in the specimen between the pole faces.
Claim 4
Dependent Claim 48 words
The method of claim 1 including the step of forming the magnetic field in the specimen by flowing the DC current through a coil to form a magnetic field in a C-shaped magnet having a pair of spaced pole faces adapted to be facially contacted against the specimen.
Claim 5
Dependent Claim 21 words
The method of claim 3 including the step of measuring the magnetic field strength in the specimen between the pole faces.
Claim 6
Dependent Claim 35 words
The method of claim 4 including the step of measuring the magnetic field strength in the specimen by positioning a magnetic field strength measuring means against a surface of the specimen between the pole faces.
Claim 7
Dependent Claim 21 words
The method of claim 4 including the step of setting the magnetic field strength in the specimen to a specified level.
Claim 8
Dependent Claim 44 words
The method of claim 1 including the step of propagating an ultrasonic, longitudinal or shear wave in the specimen propagating from one surface of the specimen toward an opposing surface of the specimen for reflection thereby back toward the origin of the acoustic wavefront.
Claim 9
Dependent Claim 20 words
The method of claim 7 including the step of propagating an ultrasonic surface wave along the surface of the specimen.
Claim 10
Dependent Claim 46 words
The method of claim 7 including the step of propagating the ultrasonic wave at a location between a pair of magnetic pole faces on a C-shaped magnet positioned against the specimen so that the ultrasonic wave passes through a portion of the specimen exposed magnetic flux.
Claim 11
Dependent Claim 65 words
The method of claim 1 in repetitively testing a set of similar specimens including the step of releasably positioning a magnet to a specimen, the magnet having a pair of spaced pole faces to create a magnetic field in the specimen, and also attaching an ultrasonic transducer means to a surface of the specimen between the pole faces to obtain measurements of acoustic velocity change.
Claim 12
Dependent Claim 30 words
The method of claim 10 further including the step of positioning a magnetic field strength measuring means adjacent to the specimen to measure the magnetic field strength in the specimen.
Claim 13
Dependent Claim 16 words
The method of claim 11 wherein the magnetic field strength is measured between the pole faces.
Claim 14
Dependent Claim 30 words
The method of claim 1 including the step of propagating the ultrasonic wave repetitively at different frequencies, and measuring the change in velocity as a function of magnetic field strength.
Claim 15
Dependent Claim 19 words
The method of claim 13 including the step of transmitting the ultrasonic wave along the surface of the specimen.
Claim 16
Dependent Claim 29 words
The method of claim 1 including the step of comparing the measured MIVC to a set of calibration curves to determine the magnitude and the sign of the stress.
Claim 17
Dependent Claim 37 words
The method of claim 1 including the step of determining the direction of stress utilizing the characteristic dependence of MIVC on the relative orientation of stress, magnetic field, and propagation and/or polarization direction of the ultrasonic wave.

References Cited (Backward Citations)

US2998536A Cited
US3577774A Cited
FR2053185A1 Cited
US3872378A Cited
US4167878A Cited
US4080836A Cited
US4314202A Cited
US4309905A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-02-05 1988-08-06 1989-02-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-02-05 1992-08-06 1993-02-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-02-05 1996-08-06 1997-02-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag