Aerosol gel

Assignee: BASF Corp
•
Filing: 1983-08-22
•
Granted: 1985-01-22
•
Expires: 2003-08-22
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A pressurized composition in an aerosol container and adapted to form a spray upon release of pressure therefrom which composition is a liquid inside the container and forms a gel on contact with living tissue comprising water, propellant and a polyoxyethylene-polyoxybutylene copolymer. The preferred composition also includes a volatile solvent and may advantageously include a skin treating agent, and conventional adjuvants.

Inventors

  • 👤 Irving R. Schmolka

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 18:42
CPC Classifications
A; A61; A61K; A61K8/00; A61K8/02; A61K8/04; A61K8/042; A61K47/00; A61K47/06; A61K47/08; A61K47/10; A61K8/046; A61K8/18; A61K8/72; A61K8/90; A61K9/00; A61K9/0012; A61K9/0014; A61K9/10; A61K9/12; A61L; A61L26/00; A61L26/0009; A61L26/0019; A61L26/0061; A61L26/0076; A61Q; A61Q19/00; A61Q9/00; A61Q9/02; Y; Y10; Y10S; Y10S424/00; Y10S424/13

Claims Analysis

Total Claims: 20
Claim 1
Independent Claim 171 words
A pressurized composition in an aerosol container and adapted to form a spray upon release of pressure therefrom which composition is a liquid inside the container and forms a gel on contact with living tissue comprising by weight about 35 to 80 percent water, 10 to 25 percent polyoxyethylene-polyoxybutylene copolymer of the formula: Y[(C.sub.4 H.sub.8 O).sub.n (C.sub.2 H.sub.4 O).sub.m H].sub.x wherein Y is the residue of a water-soluble organic compound containing therein x active hydrogen atoms; n is an integer; x is an integer greater than 1; the value of n and x are such that the molecular weight of the oxybutylene groups is from about 1000 to 20,000; and the value of m is such that the oxyethylene groups constitute about 60 to 90 percent of the total weight of the compound, and about 3 to 50 percent propellant which is a solvent for the composition in said container or propellant which is not a solvent for said composition plus about 1 to 10 percent of a non-propellant volatile solvent.
Claim 2
Dependent Claim 171 words
A pressurized composition in an aerosol container and adapted to form a spray upon release of pressure therefrom which composition is a liquid inside the container and forms a gel on contact with living tissue comprising by weight about 35 to 80 percent water, 10 to 25 percent polyoxyethylene-polyoxybutylene copolymer of the formula: Y[(C.sub.4 H.sub.8 O).sub.n (C.sub.2 H.sub.4 O).sub.m H].sub.x wherein Y is the residue of a water-soluble organic compound containing therein x active hydrogen atoms; n is an integer; x is an integer greater than 1; the value of n and x are such that the molecular weight of the oxybutylene groups is from about 1000 to 20,000; and the value of m is such that the oxyethylene groups constitute about 60 to 90 percent of the total weight of the compound, and about 3 to 50 percent propellant which is a solvent for the composition in said container or propellant which is not a solvent for said composition plus about 1 to 10 percent of a non-propellant volatile solvent.
Claim 3
Dependent Claim 118 words
A composition of matter comprising by weight about 35 to 80 percent water, about 3 to 50 percent propellant, about 1 to 10 percent non-propellant volatile solvent and about 10 to 25 percent polyoxyethylene-polyoxybutylene copolymer of the formula: Y[(C.sub.4 H.sub.8 O).sub.n (C.sub.2 H.sub.4 O).sub.m H].sub.x wherein Y is the residue of a water-soluble organic compound containing therein x active hydrogen atoms; n is an integer; x is an integer greater than 1; the value of n and x are such that the molecular weight of the oxybutylene groups is from about 1000 to 20,000; and the value of m is such that the oxyethylene groups constitute about 60 to 90 percent of the total weight of the compound.
Claim 4
Dependent Claim 118 words
A composition of matter comprising by weight about 35 to 80 percent water, about 3 to 50 percent propellant, about 1 to 10 percent non-propellant volatile solvent and about 10 to 25 percent polyoxyethylene-polyoxybutylene copolymer of the formula: Y[(C.sub.4 H.sub.8 O).sub.n (C.sub.2 H.sub.4 O).sub.m H].sub.x wherein Y is the residue of a water-soluble organic compound containing therein x active hydrogen atoms; n is an integer; x is an integer greater than 1; the value of n and x are such that the molecular weight of the oxybutylene groups is from about 1000 to 20,000; and the value of m is such that the oxyethylene groups constitute about 60 to 90 percent of the total weight of the compound.
Claim 5
Dependent Claim 79 words
The composition of claim 2 wherein Y is a butylene glycol whereby the resulting compounds have the structure HO(C 2 H 4 O) m (C 4 H 8 O) n (C 2 H 4 O) m H wherein n has a value such that the oxybutylene groups have a molecular weight of about 2000 to 10,000 and m has a value such that the oxyethylene groups constitute about 60 to 90 percent of the total weight of the compound.
Claim 6
Dependent Claim 18 words
The composition of claim 3 including about 0.05 to 20 percent of at least one skin treatment agent.
Claim 7
Dependent Claim 16 words
The composition of claim 4 including about 1.0 to 20 percent of at least one adjuvant.
Claim 8
Dependent Claim 13 words
The composition of claim 5 wherein said composition is a burn treatment composition.
Claim 9
Dependent Claim 12 words
The composition of claim 5 wherein said composition is a shaving cream.
Claim 10
Dependent Claim 123 words
The composition of matter comprising by weight about 35 to 80 percent water, about 3 to 50 percent propellant which is a solvent, 0 to about 10 percent of a non-propellant volatile solvent and 10 to 25 percent polyoxyethylene-polyoxybutylene copolymer of the formula: Y[(C.sub.4 H.sub.8 O).sub.n (C.sub.2 H.sub.4 O).sub.m H].sub.x wherein Y is the residue of a water-soluble organic compound containing therein x active hydrogen atoms; n is an integer; x is an integer greater than 1; the value of n and x are such that the molecular weight of the oxybutylene groups is from about 1000 to 20,000; and the value of m is such that the oxyethylene groups constitute about 60 to 90 percent of the total weight of the compound.
Claim 11
Dependent Claim 123 words
The composition of matter comprising by weight about 35 to 80 percent water, about 3 to 50 percent propellant which is a solvent, 0 to about 10 percent of a non-propellant volatile solvent and 10 to 25 percent polyoxyethylene-polyoxybutylene copolymer of the formula: Y[(C.sub.4 H.sub.8 O).sub.n (C.sub.2 H.sub.4 O).sub.m H].sub.x wherein Y is the residue of a water-soluble organic compound containing therein x active hydrogen atoms; n is an integer; x is an integer greater than 1; the value of n and x are such that the molecular weight of the oxybutylene groups is from about 1000 to 20,000; and the value of m is such that the oxyethylene groups constitute about 60 to 90 percent of the total weight of the compound.
Claim 12
Dependent Claim 79 words
The composition of claim 8 wherein Y is a butylene glycol whereby the resulting compounds have the structure HO(C 2 H 4 O) m (C 4 H 8 O) n (C 2 H 4 O) m H wherein n has a value such that the oxybutylene groups have a molecular weight of about 2000 to 10,000 and m has a value such that the oxyethylene groups constitute about 60 to 90 percent of the total weight of the compound.
Claim 13
Dependent Claim 18 words
The composition of claim 9 including about 0.05 to 10 percent of at least one skin treatment agent.
Claim 14
Dependent Claim 16 words
The composition of claim 10 including about 1.0 to 20 percent of at least one adjuvant.
Claim 15
Dependent Claim 13 words
The composition of claim 11 wherein said composition is a burn treatment composition.
Claim 16
Dependent Claim 12 words
The composition of claim 11 wherein said composition is a shaving cream.
Claim 17
Dependent Claim 181 words
A process for treating living skin comprising subjecting a gel composition to an elevated pressure in an aerosol container whereby said gel composition is a liquid, spraying said composition onto living skin, whereby a gel is formed on contact therewith, said composition comprising by weight about 35 to 80 percent water, about 10 to 25 percent of a polyoxyethylene-polyoxybutylene copolymer of the formula Y[(C.sub.4 H.sub.8 O).sub.n (C.sub.2 H.sub.4 O).sub.m H].sub.x wherein Y is the residue of a water-soluble organic compound containing therein x active hydrogen atoms; n is an integer; x is an integer greater than 1; the value of n and x are such that the molecular weight of the oxybutylene groups is from about 1000 to 20,000; and the value of m is such that the oxyethylene groups constitute about 60 to 90 percent of the total weight of the compound, and about 3 to 50 percent propellant which is a solvent for the composition in said container or propellant which is not a solvent for said composition plus about 1 to 10 percent of a non-propellant volatile solvent.
Claim 18
Dependent Claim 181 words
A process for treating living skin comprising subjecting a gel composition to an elevated pressure in an aerosol container whereby said gel composition is a liquid, spraying said composition onto living skin, whereby a gel is formed on contact therewith, said composition comprising by weight about 35 to 80 percent water, about 10 to 25 percent of a polyoxyethylene-polyoxybutylene copolymer of the formula Y[(C.sub.4 H.sub.8 O).sub.n (C.sub.2 H.sub.4 O).sub.m H].sub.x wherein Y is the residue of a water-soluble organic compound containing therein x active hydrogen atoms; n is an integer; x is an integer greater than 1; the value of n and x are such that the molecular weight of the oxybutylene groups is from about 1000 to 20,000; and the value of m is such that the oxyethylene groups constitute about 60 to 90 percent of the total weight of the compound, and about 3 to 50 percent propellant which is a solvent for the composition in said container or propellant which is not a solvent for said composition plus about 1 to 10 percent of a non-propellant volatile solvent.
Claim 19
Independent Claim 205 words
An apparatus for treating skin comprising an aerosol container adapted to hold a material under pressure, a gel composition provided inside said container which is liquid when under the pressure normally found inside an aerosol container and which gels on contact with living skin at atmospheric pressure, a valve adapted to close off or release the liquid under pressure in the form of a spray, said gel composition comprising by weight abut 35 to 80 percent water, and 10 to 25 percent polyoxethylene-polyoxybutylene copolymer of the formula: Y[(C.sub.4 H.sub.8 O).sub.n (C.sub.2 H.sub.4 O).sub.m H].sub.x wherein Y is the residue of a water-soluble organic compound containing therein x active hydrogen atoms; n is an integer; x is an integer greater than 1; the value of n and x are such that the molecular weight of the oxybutylene groups is from about 1000 to 20,000; and the value of m is such that the oxyethylene groups constitute about 60 to 90 percent of the total weight of the compound, and about 3 to 50 percent propellant which is a solvent for the composition in said container or propellant which is not a solvent for said composition plus about 1 to 10 percent of a non-propellant volatile solvent.
Claim 20
Independent Claim 205 words
An apparatus for treating skin comprising an aerosol container adapted to hold a material under pressure, a gel composition provided inside said container which is liquid when under the pressure normally found inside an aerosol container and which gels on contact with living skin at atmospheric pressure, a valve adapted to close off or release the liquid under pressure in the form of a spray, said gel composition comprising by weight abut 35 to 80 percent water, and 10 to 25 percent polyoxethylene-polyoxybutylene copolymer of the formula: Y[(C.sub.4 H.sub.8 O).sub.n (C.sub.2 H.sub.4 O).sub.m H].sub.x wherein Y is the residue of a water-soluble organic compound containing therein x active hydrogen atoms; n is an integer; x is an integer greater than 1; the value of n and x are such that the molecular weight of the oxybutylene groups is from about 1000 to 20,000; and the value of m is such that the oxyethylene groups constitute about 60 to 90 percent of the total weight of the compound, and about 3 to 50 percent propellant which is a solvent for the composition in said container or propellant which is not a solvent for said composition plus about 1 to 10 percent of a non-propellant volatile solvent.

References Cited (Backward Citations)

US3476853A Cited
US3740421A Cited
US3639575A Cited
US4001391A Cited
US3751562A Cited
GB1444334A Cited
US4293542A Cited
US4360451A Cited
US4376764A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-01-22 1988-07-23 1989-01-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-01-22 1992-07-23 1993-01-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-01-22 1996-07-23 1997-01-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag