Abstract
Abstract A metallization system for high temperature use comprises a layer strongly bonded to the surface of a semiconductor substrate in the form of an alloy of a metal in the amorphous state in which the metal is a transition metal, transition metal/normal metal alloy or transition metal/metalloid alloy having a crystallization temperature from the amorphous state in excess of 200 DEG C. The as-deposited amorphous films exhibit good adhesion and show at least an order of magnitude improvement in corrosion protection compared to polycrystalline coatings. Annealing treatments below the glass transition temperature have been found to further enhance this protective behavior of the amorphous films.
Inventors
- 👤 John H. Perepezko
- 👤 John D. Wiley
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-31 05:55
CPC Classifications
H; H10; H10W; H10W99/00; H10D; H10D64/00; H10D64/01; H10D64/011; H10D64/0111; H10D64/0116
Claims Analysis
Total Claims: 17
Claim 1
Independent Claim
81 words
A metallization device characterized by resistance to corrosion and suitably for high temperature applicantions which comprises a base selected from the group consisting of semiconductor devices, insulators, ohmic contacts, Schottky barrier contacts, rectifying contacts, metal interconnects, bonded lead wires and gate metallizations and, bonded to the surface of said base, a layer of a metal elected from the group consisting of a transition metal, a transition metal/normal metal alloy and a transition metal/metalloid alloy, said layer being in an amorphous state.
Claim 2
Dependent Claim
81 words
A metallization device characterized by resistance to corrosion and suitably for high temperature applicantions which comprises a base selected from the group consisting of semiconductor devices, insulators, ohmic contacts, Schottky barrier contacts, rectifying contacts, metal interconnects, bonded lead wires and gate metallizations and, bonded to the surface of said base, a layer of a metal elected from the group consisting of a transition metal, a transition metal/normal metal alloy and a transition metal/metalloid alloy, said layer being in an amorphous state.
Claim 3
Dependent Claim
39 words
A metallization device as claimed in claim 1 in which the amorphous metal layer is characterized by improved resistance to corrosion after being annealed to the base at a temperature below the crystallization temperature of the amorphous metal layer.
Claim 4
Dependent Claim
14 words
A device as claimed in claim 1 in which the base is a semiconductor.
Claim 5
Dependent Claim
14 words
A device as claimed in claim 1 in which the base is an insulator.
Claim 6
Dependent Claim
26 words
A device as claimed in claim 1 in which the base is selected from the group consisting of Si, GaAs, GaP, glass and SiO 2 .
Claim 7
Dependent Claim
31 words
A device as claimed in claim 1 in which the amorphous metal layer has a crystallization temperature in the range from above 200° C. to the melting point of the alloy.
Claim 8
Dependent Claim
20 words
A device as claimed in claim 1 in which the amorphous metal layer has a crystallization temperature above 500° C.
Claim 9
Dependent Claim
15 words
A device as claimed in claim 1 in which the alloy is a multicomponent alloy.
Claim 10
Dependent Claim
17 words
A device as claimed in claim 8 in which the alloy is a binary or ternary alloy.
Claim 11
Dependent Claim
24 words
A device as claimed in claim 1 in which the alloy is selected from the group consisting of Ni-Mo, Ni-Nb, Mo-Si, W-Si and Ni-Ta.
Claim 12
Dependent Claim
17 words
A device as claimed in claim 1 in which hafnium is included in the amorphous metal layer.
Claim 13
Dependent Claim
25 words
A device as claimed in claim 1 in which the amorphous metal layer is of a thickness within the range of 0.01 to 50 microns.
Claim 14
Dependent Claim
21 words
A device as claimed in claim 1 in which the amorphous metal layer is deposited by atomic deposition onto the base.
Claim 15
Dependent Claim
21 words
A device as claimed in claim 1 in which the amorphous metal layer is deposited onto the base by RF sputtering.
Claim 16
Dependent Claim
21 words
A device as claimed in claim 1 in which the amorphous metal functions as a barrier to interdiffusion between adjacent layers.
Claim 17
Dependent Claim
38 words
A device as claimed in claim 2 in which the amorphous metal layer is resistant to corrosion in the presence of a reagent selected from the group consisting of hydrochloric acid, nitric acid, ferric chloride and sodium chloride.
References Cited (Backward Citations)
US3582324A
Cited
US3607240A
Cited
US3675090A
Cited
US3664874A
Cited
US3746944A
Cited
US3886577A
Cited
US4181913A
Cited
US4177475A
Cited
US4350994A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1988-01-15 | 1988-07-16 | 1989-01-15 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1992-01-15 | 1992-07-16 | 1993-01-15 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1996-01-15 | 1996-07-16 | 1997-01-15 | $7700.00 | Window Closed / Lapsed |