Abstract
Abstract A method is provided for the production of ultrahigh molecular weight drag reducing substances and the like comprising: (a) preparing under an inert atmosphere a catalyst comprising: (1) titanium halide of the general formula TiX m wherein m=2.5 to 4.0; (2) a co-catalyst such as an organo-aluminum halide of the formula AlR n X 3-n where r is a hydrocarbon radical, X is a halogen and n is 2 or 3; (3) a phosphorous compound of the formula PR 1 R 2 R 3 or P(OR 1 )(OR 2 )(OR 3 ) where R 1 , R 2 , and R 3 are, independently, aryl, alkyl, aralkyl, or alkaryl, containing from 1 to 12 carbon atoms and placing the catalyst in contact with; (b) alpha-monoolefinic hydrocarbons from C 2 -C 30 under suitable temperature conditions to provide a hydrocarbon soluble ultrahigh molecular weight polymer, then ceasing polymerization at a polymer content level of 20% by weight or less, based on the total reaction mixture.
Inventors
- 👤 Mark P. Mack
Bibliographic Details
Claims Analysis
Total Claims: 4References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1988-01-15 | 1988-07-16 | 1989-01-15 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1992-01-15 | 1992-07-16 | 1993-01-15 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1996-01-15 | 1996-07-16 | 1997-01-15 | $7700.00 | Window Closed / Lapsed |