Abstract

Abstract A method for forming a multilayered electroluminescent device having dielectric layers sandwiched between two electrodes. One dielectric layer includes phosphor particles dispersed throughout. Each dielectric layer is subjected to three distinct heat levels: a preheat temperature level; a fusing temperature heat level; and a cooling/heat temperature level which enables the contiguous layers to gradually cool into fusion. One electrode may be a solid substrate which is fused to a contiguous dielectric layer and the other electrode substance may be sprayed in a liquid state onto the surface of the phosphor-dielectric layer when it is also in a liquified state after being cooled to the cooling/heat level prior to solidifying. The illuminating phosphors are mixed in the liquified dielectric material just prior to forming the phosphor-dielectric layer and applying the three heat levels thereto.

Inventors

  • 👤 Manley D. Emmett
  • 👤 Robert L. McNellis

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 12:25
CPC Classifications
H; H05; H05B; H05B33/00; H05B33/10

Claims Analysis

Total Claims: 34
Claim 1
Independent Claim 139 words
A process for forming an electroluminescent device including the steps of: forming an electrical conductive means to provide an electrode for applying electrical voltage; disposing a layer of dielectric material over said electrode; inserting the electrode and said dielectric layer into a first furnace having a first heating temperature level; removing said electrode and dielectric layer after a first predetermined time period; inserting the electrode and dielectric layer into a second furnace having a second heating temperature level greater than the first temperature level; removing the electrode and dielectric layer from the second furnace after a second predetermined time period; inserting the electrode and dielectric layer into a third furnace having a temperature level less than the second temperature level in said second furnace; and cooling the electrode and dielectric layer for fusing the electrode and dielectric layer together.
Claim 2
Dependent Claim 139 words
A process for forming an electroluminescent device including the steps of: forming an electrical conductive means to provide an electrode for applying electrical voltage; disposing a layer of dielectric material over said electrode; inserting the electrode and said dielectric layer into a first furnace having a first heating temperature level; removing said electrode and dielectric layer after a first predetermined time period; inserting the electrode and dielectric layer into a second furnace having a second heating temperature level greater than the first temperature level; removing the electrode and dielectric layer from the second furnace after a second predetermined time period; inserting the electrode and dielectric layer into a third furnace having a temperature level less than the second temperature level in said second furnace; and cooling the electrode and dielectric layer for fusing the electrode and dielectric layer together.
Claim 3
Dependent Claim 23 words
The process of claim 1 wherein the temperature level of said third furnace is greater than the temperature level in said first furnace.
Claim 4
Dependent Claim 178 words
The process of claim 1 includes: disposing a second layer of dielectric material over said first-mentioned layer; inserting said electrode and said first and second layers into said first furnace having a fourth heating temperature level; removing said electrode and said first and second layers from said first furnace after a fourth predetermined time period; inserting said electrode and first and second layers into said second furnace having a fifth temperature level; removing said electrode and first and second layers from said second furnace after a fifth predetermined time period; inserting said electrode and said first and second layers into said third furnace having a sixth temperature level; removing said electrode and said first and second layers from said third furnace after a sixth predetermined time period, said fifth temperature level being greater than said fourth temperature level and said sixth temperature level being less than the fifth temperature level for commencing the cooling of the device; and cooling the electrode and said first and second layers to room temperature for fusing the first and second layers together.
Claim 5
Dependent Claim 137 words
The process of claim 3 includes: disposing a third layer of dielectric material over said second layer; inserting said device including said three layers of dielectric material and said electrode into said first furnace having a seventh temperature level; removing said device from said first furnace after a seventh predetermined time period; inserting said device into said second furnace having an eighth temperature level; removing said device from said second furnace after an eighth predetermined time period; inserting said device into said third furnace having a ninth temperature level; removing said device from said third furnace after a ninth predetermined time period, said eighth temperature level being greater than said seventh temperature level and said ninth temperature level being less than the eighth temperature level; and cooling said device for fusing the second and third layers together.
Claim 6
Dependent Claim 46 words
The process of claim 4, wherein said third layer is formed by: preparing a mixture of frit material combined with an alcohol carrier for liquifying the mixture; and adding electric field responsive phosphors just prior to disposing said third dielectric layer over said second dielectric layer.
Claim 7
Dependent Claim 38 words
The process of claim 4 includes: applying an electrically conductive material on said third dielectric material to provide a second electrode when said third dielectric material is melted and prior to solidifying and fusing with the second layer.
Claim 8
Dependent Claim 22 words
The process of claim 6 wherein said conductive material is applied to said third dielectric layer after said ninth predetermined time period.
Claim 9
Dependent Claim 85 words
The process of claim 7, wherein said outer furnace has an exit opening leading to the outside; steam is ejected adjacent said exit on the outside of the furnace prior to applying said second electrode on said thrid dielectric layer, to provide a steam vapor over said third dielectric layer; and cooling said layered device after the second electrode has been applied over said third dielectric, to enable said third dielectric layer to be fused with said second dielectric layer and with said second electrode.
Claim 10
Dependent Claim 18 words
The process of claim 6, wherein said electrically conductive material is a mist of tin oxide forming material.
Claim 11
Dependent Claim 17 words
The process of claim 6, wherein said electrically conductive material has a resistance less than 8,000 ohms.
Claim 12
Dependent Claim 68 words
In a process for forming an electroluminescent device having a pair of electrodes and a plurality of layers of dielectric material between said electrodes, including the steps of: preparing a mixture of frit material combined with an alcohol carrier for liquifying the mixture; and adding electric field responsive phosphor particles just prior to forming one of said layers of dielectric material having said mixture and the phosphor particles.
Claim 13
Dependent Claim 68 words
In a process for forming an electroluminescent device having a pair of electrodes and a plurality of layers of dielectric material between said electrodes, including the steps of: preparing a mixture of frit material combined with an alcohol carrier for liquifying the mixture; and adding electric field responsive phosphor particles just prior to forming one of said layers of dielectric material having said mixture and the phosphor particles.
Claim 14
Dependent Claim 29 words
The process of claim 11 includes: applying said one layer of dielectric material over another of said dielectric layers; and heating said layers for fusing said dielectric layers together.
Claim 15
Dependent Claim 38 words
The process of claim 12, includes: cooling said heated layers; and applying a second electrode material in a liquified state on said one layer having the phosphor particles when said one layer is cooling but prior to solidifying.
Claim 16
Dependent Claim 14 words
The process of claim 13, wherein said second electrode material is a tin oxide.
Claim 17
Dependent Claim 115 words
In a process for forming an electroluminescent device having at least a single layer of dielectric material between layers of electrically conductive material including the steps of: preparing a mixture of dielectric frit material with a liquid carrier and dispersing electrical field sensitive phosphors throughout; applying said liquified mixture over one of said layers to provide a phosphor-dielectric layer; heating said liquified mixture for fusing with said one layer of the device when solidifying, said heating evaporating said carrier; cooling said layers; and applying a liquified electrically conductive material on said phosphor-dielectric prior to said solidifying to provide one of said electrodes, said layers and said electrode being solidified in said device upon said cooling.
Claim 18
Dependent Claim 115 words
In a process for forming an electroluminescent device having at least a single layer of dielectric material between layers of electrically conductive material including the steps of: preparing a mixture of dielectric frit material with a liquid carrier and dispersing electrical field sensitive phosphors throughout; applying said liquified mixture over one of said layers to provide a phosphor-dielectric layer; heating said liquified mixture for fusing with said one layer of the device when solidifying, said heating evaporating said carrier; cooling said layers; and applying a liquified electrically conductive material on said phosphor-dielectric prior to said solidifying to provide one of said electrodes, said layers and said electrode being solidified in said device upon said cooling.
Claim 19
Dependent Claim 34 words
The process of claim 15, includes: applying a vapor of steam to said device after said phosphor dielectric layer has been heated but prior to solidifying, said electrode material being applied through said vapor.
Claim 20
Dependent Claim 13 words
The process of claim 15, wherein: said one layer is another dielectric layer.
Claim 21
Dependent Claim 21 words
The process of claim 17, wherein said one layer includes titanium oxide to enhance the brightness of said phosphors when illuminating.
Claim 22
Dependent Claim 14 words
The process of claim 15, wherein said electrically conductive material is a tin oxide.
Claim 23
Dependent Claim 47 words
The process of claim 15, wherein: said heating includes heating said layers at a first temperature for a predetermined time and heating said layers at a second temperature for a second predetermined time after said first predetermined time, said second temperature being greater than said first temperature.
Claim 24
Dependent Claim 31 words
The process of claim 20, wherein said cooling includes heating said layers at a third temperature less than said second temperature for a third predetermined time after said second predetermined time.
Claim 25
Dependent Claim 15 words
The process of claim 21, wherein said third temperature is greater than said first temperature.
Claim 26
Dependent Claim 34 words
The process of claim 21, wherein said electrode and layers solidify after said third predetermined time and said one electrode is applied after said third predetermined time and prior to said phosphor-dielectric layer solidifying.
Claim 27
Dependent Claim 105 words
A process for forming an electroluminescent device having a pair of electrodes with at least one layer of dielectric material therebetween, including the steps of: dispersing phosphor particles in a dielectric material, said phosphor particles illuminating in response to a voltage being applied across said electrodes; applying a layer of said phosphor-dielectric mixture on said device; heating said phospher-dielectric layer for fusing such layer to said device; cooling said phosphor-dielectric layer for fusing such layer upon solidifying; and applying a layer of electrically conductive material on said phosphor-dielectric layer to form one of said electrodes, when said phosphor-dielectric layer is cooling but prior to solidifying.
Claim 28
Dependent Claim 105 words
A process for forming an electroluminescent device having a pair of electrodes with at least one layer of dielectric material therebetween, including the steps of: dispersing phosphor particles in a dielectric material, said phosphor particles illuminating in response to a voltage being applied across said electrodes; applying a layer of said phosphor-dielectric mixture on said device; heating said phospher-dielectric layer for fusing such layer to said device; cooling said phosphor-dielectric layer for fusing such layer upon solidifying; and applying a layer of electrically conductive material on said phosphor-dielectric layer to form one of said electrodes, when said phosphor-dielectric layer is cooling but prior to solidifying.
Claim 29
Dependent Claim 21 words
The process of claim 24, wherein said electrically conductive material applied to said phosphor-dielectric layer is a mist of tin oxide.
Claim 30
Dependent Claim 21 words
The process of claim 24, includes: circulating steam vapor around said device when said electrically conductive material is being applied thereto.
Claim 31
Dependent Claim 63 words
A process for forming an electrical device having a pair of electrodes with a layer of dielectric material having electrical field sensitive particles dispersed throughout and disposed between said electrodes including the steps of: circulating a vapor of steam around said device; and applying a mist of electrically conductive material through said steam and on said device for forming one of said electrodes.
Claim 32
Dependent Claim 63 words
A process for forming an electrical device having a pair of electrodes with a layer of dielectric material having electrical field sensitive particles dispersed throughout and disposed between said electrodes including the steps of: circulating a vapor of steam around said device; and applying a mist of electrically conductive material through said steam and on said device for forming one of said electrodes.
Claim 33
Dependent Claim 22 words
The process of claim 27, includes: heating said device prior to applying said mist for fusing said one electrode to the device.
Claim 34
Dependent Claim 12 words
The process of claim 28, wherein said mist is a in oxide.

References Cited (Backward Citations)

US3160541A Cited
US4242370A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-11-13 1988-05-14 1988-11-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-11-13 1992-05-14 1992-11-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-11-13 1996-05-14 1996-11-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag