Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
280 words
A paper web product comprising a web of kraft fibers bonded together solely by natural hydrogen bonding between the fibers and with debonding agent mixed therein, and having a basis weight of at least 13.77 pounds per 3,000 square feet, a machine direction tensile strength of at least 34 grams per centimeter, a cross direction tensile strength of at least 12 grams per centimeter, a caliper for 8 plys as measured under 26.6 grams per square centimeter pressure of at least 1.15 millimeters, an oil holding capacity of at least 5.9 milliliters per gram, the web made by the process of: (a) mixing a predetermined amount of chemical debonding agent which inhibits the formation of interfiber bonds into a pulp furnish; (b) forming the pulp furnish and debonding agent mix into a web; (c) pressing the web between a conventional wet press felt and a heated, moving creping surface to reduce the moisture content thereof and transfer the web to the creping surface; (d) drying the web on the creping surface; (e) simultaneously uniformly applying a predetermined amount of creping adhesive to the creping surface ahead of the position at which the web is applied to the moving creping surface; (f) the amount of debonding agent mixed into the pulp furnish and the amount of creping adhesive applied to the creping surface selected such that substantial splitting apart of the web would occur if the web were pulled from the creping surface; and (g) creping the dried web by removing the web from the creping surface with a creping blade having a cutting angle of about 72° or less such that crepes are formed on both sides of the web.
Claim 2
Dependent Claim
280 words
A paper web product comprising a web of kraft fibers bonded together solely by natural hydrogen bonding between the fibers and with debonding agent mixed therein, and having a basis weight of at least 13.77 pounds per 3,000 square feet, a machine direction tensile strength of at least 34 grams per centimeter, a cross direction tensile strength of at least 12 grams per centimeter, a caliper for 8 plys as measured under 26.6 grams per square centimeter pressure of at least 1.15 millimeters, an oil holding capacity of at least 5.9 milliliters per gram, the web made by the process of: (a) mixing a predetermined amount of chemical debonding agent which inhibits the formation of interfiber bonds into a pulp furnish; (b) forming the pulp furnish and debonding agent mix into a web; (c) pressing the web between a conventional wet press felt and a heated, moving creping surface to reduce the moisture content thereof and transfer the web to the creping surface; (d) drying the web on the creping surface; (e) simultaneously uniformly applying a predetermined amount of creping adhesive to the creping surface ahead of the position at which the web is applied to the moving creping surface; (f) the amount of debonding agent mixed into the pulp furnish and the amount of creping adhesive applied to the creping surface selected such that substantial splitting apart of the web would occur if the web were pulled from the creping surface; and (g) creping the dried web by removing the web from the creping surface with a creping blade having a cutting angle of about 72° or less such that crepes are formed on both sides of the web.
Claim 3
Dependent Claim
287 words
A paper web product comprising a web of kraft fibers bonded together solely by natural hydrogen bonding between the fibers and with debonding agent mixed therein, and having a basis weight between 13.77 and 16.10 pounds per 3,000 square feet, a machine direction tensile strength of between 34 grams per centimeter and 78 grams per centimeter, a cross direction tensile strength of between 12 grams per centimeter and 27 grams per centimeter, a caliper for 8 plys as measured under 26.6 grams per square centimeter pressure of between 1.15 millimeters and 1.37 millimeters, an oil holding capacity of at least 8 milliliters per gram, the web formed by (a) mixing a predetermined amount of chemical debonding agent which inhibits the formation of interfiber bonds into a pulp furnish; (b) forming the pulp furnish and debonding agent mix into a web; (c) pressing the web between a conventional wet press felt and a heated, moving creping surface to reduce the moisture content thereof and transfer the web to the creping surface; (d) drying the web on the creping surface; (e) simultaneously uniformly applying a predetermined amount of creping adhesive to the creping surface ahead of the position at which the web is applied to the moving creping surface; (f) the amount of debonding agent mixed into the pulp furnish and the amount of creping adhesive applied to the creping surface selected such that substantial splitting apart of the web would occur if the web were pulled from the creping surface; and (g) creping the dried web by removing the web from the creping surface with a creping blade having a cutting angle of about 72° or less such that crepes are formed on both sides of the web.
Claim 4
Dependent Claim
287 words
A paper web product comprising a web of kraft fibers bonded together solely by natural hydrogen bonding between the fibers and with debonding agent mixed therein, and having a basis weight between 13.77 and 16.10 pounds per 3,000 square feet, a machine direction tensile strength of between 34 grams per centimeter and 78 grams per centimeter, a cross direction tensile strength of between 12 grams per centimeter and 27 grams per centimeter, a caliper for 8 plys as measured under 26.6 grams per square centimeter pressure of between 1.15 millimeters and 1.37 millimeters, an oil holding capacity of at least 8 milliliters per gram, the web formed by (a) mixing a predetermined amount of chemical debonding agent which inhibits the formation of interfiber bonds into a pulp furnish; (b) forming the pulp furnish and debonding agent mix into a web; (c) pressing the web between a conventional wet press felt and a heated, moving creping surface to reduce the moisture content thereof and transfer the web to the creping surface; (d) drying the web on the creping surface; (e) simultaneously uniformly applying a predetermined amount of creping adhesive to the creping surface ahead of the position at which the web is applied to the moving creping surface; (f) the amount of debonding agent mixed into the pulp furnish and the amount of creping adhesive applied to the creping surface selected such that substantial splitting apart of the web would occur if the web were pulled from the creping surface; and (g) creping the dried web by removing the web from the creping surface with a creping blade having a cutting angle of about 72° or less such that crepes are formed on both sides of the web.
Claim 5
Dependent Claim
287 words
A paper web product comprising a web of kraft fibers bonded together solely by natural hydrogen bonding between the fibers and with debonding agent mixed therein, and having a basis weight between 29.89 and 31.18 pounds per 3,000 square feet, a machine direction tensile strength of between 66 grams per centimeter and 134 grams per centimeter, a cross direction tensile strength of between 27 grams per centimeter and 46 grams per centimeter, a caliper for 8 plys as measured under 26.6 grams per square centimeter pressure of between 2.01 millimeters and 2.38 millimeters, an oil holding capacity of at least 5.9 milliliters per gram, the web formed by (a) mixing a predetermined amount of chemical debonding agent which inhibits the formation of interfiber bonds into a pulp furnish; (b) forming the pulp furnish and debonding agent mix into a web; (c) pressing the web between a conventional wet press felt and a heated, moving creping surface to reduce the moisture content thereof and transfer the web to the creping surface; (d) drying the web on the creping surface; (e) simultaneously uniformly applying a predetermined amount of creping adhesive to the creping surface ahead of the position at which the web is applied to the moving creping surface; (f) the amount of debonding agent mixed into the pulp furnish and the amount of creping adhesive applied to the creping surface selected such that substantial splitting apart of the web would occur if the web were pulled from the creping surface; and (g) creping the dried web by removing the web from the creping surface with a creping blade having a cutting angle of about 72° or less such that crepes are formed on both sides of the web.
Claim 6
Dependent Claim
287 words
A paper web product comprising a web of kraft fibers bonded together solely by natural hydrogen bonding between the fibers and with debonding agent mixed therein, and having a basis weight between 29.89 and 31.18 pounds per 3,000 square feet, a machine direction tensile strength of between 66 grams per centimeter and 134 grams per centimeter, a cross direction tensile strength of between 27 grams per centimeter and 46 grams per centimeter, a caliper for 8 plys as measured under 26.6 grams per square centimeter pressure of between 2.01 millimeters and 2.38 millimeters, an oil holding capacity of at least 5.9 milliliters per gram, the web formed by (a) mixing a predetermined amount of chemical debonding agent which inhibits the formation of interfiber bonds into a pulp furnish; (b) forming the pulp furnish and debonding agent mix into a web; (c) pressing the web between a conventional wet press felt and a heated, moving creping surface to reduce the moisture content thereof and transfer the web to the creping surface; (d) drying the web on the creping surface; (e) simultaneously uniformly applying a predetermined amount of creping adhesive to the creping surface ahead of the position at which the web is applied to the moving creping surface; (f) the amount of debonding agent mixed into the pulp furnish and the amount of creping adhesive applied to the creping surface selected such that substantial splitting apart of the web would occur if the web were pulled from the creping surface; and (g) creping the dried web by removing the web from the creping surface with a creping blade having a cutting angle of about 72° or less such that crepes are formed on both sides of the web.