Method for decontaminating metals contaminated with radioactive substances
Assignee: Hitachi Ltd
•
Filing: 1984-02-22
•
Granted: 1984-11-06
•
Expires: 2004-02-22
Abstract
Abstract The present invention provides a method for decontaminating metal components which have been contaminated on their surfaces with radioactive substances, characterized in that radioactivated oxide films on the metal surfaces are electrolytically removed by an alternating electrolysis method in a neutral salt solution. According to the invention, oxides and hydroxides for metals removed by the electrolytic treatment are separated from the electrolyte and solidified. The method of this invention makes it possible to positively remove the radioactivated oxide films from a base metal.
Inventors
- 👤 Tatsuo Izumida
- 👤 Koji Kato
- 👤 Fumio Kawamura
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-08 11:47
CPC Classifications
G; G21; G21F; G21F9/00; G21F9/28; G21F9/30; C; C25; C25F; C25F3/00; C25F3/02; C25F1/00; G21F9/001
Claims Analysis
Total Claims: 15
Claim 1
Independent Claim
93 words
A method for electrolytically decontaminating metals which have been contaminated on their surfaces with radioactive substances, which comprises subjecting a metal to be decontaminated to an alternating electrolysis treatment consisting of alternately repeated cathode electrolysis in a unit period of 30 to 180 seconds and anode electrolysis in a unit period of 15 to 60 seconds with a ratio of the cathode electrolysis time to the anode electrolysis time of 1 to 4 by using an aqueous solution of a neutral salt as electrolyte, thereby removing the radioactivated oxide films and metal surfaces.
Claim 2
Independent Claim
93 words
A method for electrolytically decontaminating metals which have been contaminated on their surfaces with radioactive substances, which comprises subjecting a metal to be decontaminated to an alternating electrolysis treatment consisting of alternately repeated cathode electrolysis in a unit period of 30 to 180 seconds and anode electrolysis in a unit period of 15 to 60 seconds with a ratio of the cathode electrolysis time to the anode electrolysis time of 1 to 4 by using an aqueous solution of a neutral salt as electrolyte, thereby removing the radioactivated oxide films and metal surfaces.
Claim 3
Dependent Claim
42 words
A method according to claim 1, wherein the cathode electrolysis in a unit period is 60 to 90 seconds, the anode electrolysis in a unit period is 30 seconds and the ratio of the former to the latter is 2 to 3.
Claim 4
Dependent Claim
19 words
A method according to claim 1, wherein the total time of alternating electrolysis treatment is 10 to 20 minutes.
Claim 5
Dependent Claim
26 words
A method according to claim 1, wherein the neutral salt is at least one salt selected from the group consisting of hydrochlorides, sulfates, nitrates and phosphates.
Claim 6
Dependent Claim
17 words
A method according to claim 4, wherein the neutral salt is Na 2 SO 4 or NaCl.
Claim 7
Independent Claim
114 words
A method for electrolytically decontaminating metals which have been contaminated on their surfaces with radioactive substances, which comprises subjecting a metal to be decontaminated to an alternating electrolysis treatment consisting of alternately repeated cathode electrolysis in a unit period of 30 to 180 seconds and anode electrolysis in a unit period of 15 to 60 seconds with a ratio of the cathode electrolysis time to the anode electrolysis time of 1 to 4 by using an aqueous solution of a neutral salt to thereby remove the radioactivated oxide films and metal surfaces, separating a decontamination residue contained in the electrolyte from the electrolyte, and solidifying the separated residue by adding a solidifying agent thereto.
Claim 8
Independent Claim
114 words
A method for electrolytically decontaminating metals which have been contaminated on their surfaces with radioactive substances, which comprises subjecting a metal to be decontaminated to an alternating electrolysis treatment consisting of alternately repeated cathode electrolysis in a unit period of 30 to 180 seconds and anode electrolysis in a unit period of 15 to 60 seconds with a ratio of the cathode electrolysis time to the anode electrolysis time of 1 to 4 by using an aqueous solution of a neutral salt to thereby remove the radioactivated oxide films and metal surfaces, separating a decontamination residue contained in the electrolyte from the electrolyte, and solidifying the separated residue by adding a solidifying agent thereto.
Claim 9
Dependent Claim
42 words
A method according to claim 6, wherein the cathode electrolysis in a unit period is 60 to 90 seconds, the anode electrolysis in a unit period is 30 seconds and the ratio of the former to the latter is 2 to 3.
Claim 10
Dependent Claim
19 words
A method according to claim 6, wherein the total time of alternating electrolysis treatment is 10 to 20 minutes.
Claim 11
Dependent Claim
26 words
A method according to claim 6, wherein the neutral salt is at least one salt selected from the group consisting of hydrochlorides, sulfates, nitrates and phosphates.
Claim 12
Dependent Claim
17 words
A method according to claim 9, wherein the neutral salt is Na 2 SO 4 or NaCl.
Claim 13
Dependent Claim
32 words
A method according to claim 6, wherein in the steps of separating and solidifying the decontamination residue, said residue is first concentrated by dewatering and then mixed with water glass for solidification.
Claim 14
Dependent Claim
22 words
A method according to claim 11, wherein the concentration by dewatering of said decontamination residue is conducted by a centrifugal separation method.
Claim 15
Dependent Claim
18 words
A method according to claim 11, wherein the mixing ratio of decontamination residue to water glass is 1:2-1:3.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-11-06 | 1988-05-07 | 1988-11-06 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-11-06 | 1992-05-07 | 1992-11-06 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-11-06 | 1996-05-07 | 1996-11-06 | $7700.00 | Window Closed / Lapsed |