Magnetic storage medium

Assignee: Agfa Gevaert AG
•
Filing: 1982-07-08
•
Granted: 1984-10-16
•
Expires: 2002-07-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The present invention relates to a magnetic storage medium consisting of a non-magnetic layer support and, applied thereto, a binder-containing magnetic layer, the binder consisting of from 25 to 100% of a thermoplastic polyurethane substantially free from reactive terminal groups obtained by reacting a linear polyester of at least one dicarboxylic acid containing from 2 to 8 carbon atoms and/or hydroxy carboxylic acid containing from 4 to 6 carbon atoms and at least one glycol containing from 2 to 6 carbon atoms, the polyester having a molecular weight of from 1200 to 6000, at least one diisocyanate and a mixture of at least two glycols containing from 2 to 20 carbon atoms, the molar fraction of the individual components not exceeding 0.8. The polyurethane has a hardness of from 80 to 100 Shore A, a tensile strength of from 30 to 75 MPa and a breaking elongation of from 320 to 520%.

Inventors

  • 👤 Robert Kohler
  • 👤 Burkhard Nippe
  • 👤 Heinrich Kober
  • 👤 Karlchristian Schilffarth
  • 👤 Walter Meckel
  • 👤 Bernd Quiring

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 09:57
CPC Classifications
G; G11; G11B; G11B5/00; G11B5/62; G11B5/68; G11B5/70; G11B5/702; G11B5/7021; Y; Y10; Y10S; Y10S428/00; Y10S428/90; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31551; Y10T428/31609; Y10T428/31855; Y10T428/31935; Y10T428/31942

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 170 words
A magnetic storage medium consisting of a non-magnetic layer support and, applied thereto, at least one magnetisable layer containing finely particulate magnetic pigments and polyurethanes as binder, characterised in that the binder consists of from 25 to 100% of a thermoplastic polyurethane having a hardness of from 80 to 100 Shore A, a tensile strength of from 30 to 75 MPa and a breaking elongation of from 320 to 520% and substantially free from reactive terminal groups; obtained by reacting: (a) a linear polyester of at least one dicarboxylic acid containing from 2 to 8 carbon atoms and/or hydroxy carboxylic acid containing from 4 to 6 carbon atoms and at least one glycol containing from 2 to 12 carbon atoms, the molecular weight of the polyester being from 1200 to 6000, with (b) at least one diisocyanate, and (c) a mixture consisting of at least two straight-chain diols containing from 2 to 20 carbon atoms, and free of branchedchain diols, the molar fraction of the individual components not exceeding 0.8.
Claim 2
Dependent Claim 170 words
A magnetic storage medium consisting of a non-magnetic layer support and, applied thereto, at least one magnetisable layer containing finely particulate magnetic pigments and polyurethanes as binder, characterised in that the binder consists of from 25 to 100% of a thermoplastic polyurethane having a hardness of from 80 to 100 Shore A, a tensile strength of from 30 to 75 MPa and a breaking elongation of from 320 to 520% and substantially free from reactive terminal groups; obtained by reacting: (a) a linear polyester of at least one dicarboxylic acid containing from 2 to 8 carbon atoms and/or hydroxy carboxylic acid containing from 4 to 6 carbon atoms and at least one glycol containing from 2 to 12 carbon atoms, the molecular weight of the polyester being from 1200 to 6000, with (b) at least one diisocyanate, and (c) a mixture consisting of at least two straight-chain diols containing from 2 to 20 carbon atoms, and free of branchedchain diols, the molar fraction of the individual components not exceeding 0.8.
Claim 3
Dependent Claim 55 words
A magnetic storage medium as claimed in claim 1, characterised in that the polyurethane is obtained by reacting a copolyester of ethylene glycol/butane diol and adipic acid having a molecular weight of 2000, 4,4'-diphenyl methane diisocyanate and a mixture consisting of 1,4-butane diol and 1,6-hexane diol in a molar ratio of from 3:2 to 2:3.
Claim 4
Dependent Claim 54 words
A magnetic storage medium as claimed in claim 1, characterised in that the polyurethane is obtained by reacting a copolyester of ethylene glycol/butane diol and adipic acid having a molecular weight of 2000, 4,4'-diphenyl methane diisocyanate and a mixture of ethylene glycol and 1,4-butane diol in a molar ratio of from 3:2 to 2:3.
Claim 5
Dependent Claim 50 words
A magnetic storage medium as claimed in claim 1, characterised in that the polyurethane is obtained by reacting a polyester of 1,4-butane diol and adipic acid having a molecular weight of 2000, 4,4'-diphenyl methane diisocyanate and a mixture of 1,4-butane diol and 1,6-hexane diol in a molar ratio of 70:30.
Claim 6
Dependent Claim 20 words
A magnetic storage medium as claimed in claim 4, characterised in that a polyvinyl acetal is used as additional binder.
Claim 7
Dependent Claim 20 words
A magnetic storage medium as claimed in claim 4, characterised in that a polyvinyl formal is used as additional binder.
Claim 8
Dependent Claim 20 words
A magnetic storage medium as claimed in claim 4 characterised in that a polyvinyl butyral is used as additional binder.
Claim 9
Dependent Claim 26 words
A magnetic storage medium as claimed in claim 4, characterised in that a hydroxyl-containing copolymer of vinyl acetate and vinyl chloride is used as additional binder.
Claim 10
Dependent Claim 28 words
A magnetic storage medium as claimed in claim 4, characterised in that a copolymer of vinyl chloride and hydroxy propyl acrylate or methacrylate is used as additional binder.

References Cited (Backward Citations)

US3149995A Cited
US3650828A Cited
US3922439A Cited
US3929659A Cited
US4018967A Cited
US4058646A Cited
US4320171A Cited
US4328282A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-10-16 1988-04-16 1988-10-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-10-16 1992-04-16 1992-10-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-10-16 1996-04-16 1996-10-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag