Patent US5799067A successfully refreshed from Google Patents.
US4477485A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Process for forming an electrode of an organic cell
Assignee: Denso Corp
•
Filing: 1983-06-30
•
Granted: 1984-10-16
•
Expires: 2003-06-30
Abstract
Abstract An electrode for use in an organic cell is provided by forming a thin film of a metal such as aluminum on the sheet of an organic electroconductive material such as polyacetylene by, for example, a vacuum evaporation method, and then forming an atom-interdiffused layer at the interface between the sheet and the thin film by a recoil ion implantation method, thereby enhancing the current collecting efficiency of the electrode.
Inventors
- 👤 Hiromochi Muramatsu
- 👤 Atsushi Watanabe
- 👤 Kunihiko Hara
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-04 14:53
CPC Classifications
C; C23; C23C; C23C14/00; C23C14/58; C23C14/5826; C23C14/5833; C23C14/06; C23C14/14; C23C14/20; C23C14/5893; H; H01; H01M; H01M10/00; H01M10/05; H01M4/00; H01M4/02; H01M4/13; H01M4/137; H01M4/139; H01M4/1399; H01M4/64; H01M4/66; H01M50/00; H01M50/50; H01M50/531; H01M50/534; H01M50/536; Y; Y02; Y02E; Y02E60/00; Y02E60/10
Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
85 words
A process for forming an electrode of an organic electroconductive material for use in an organic cell, in which a thin film of a metal is formed on the surface of at least a part of at least one side of the organic electroconductive material in a sheet form at such a temperature that no thermal deterioration occurs in said organic material, and then an atom-interdiffused layer is formed at the interface between said thin film and said electrode by a recoil ion implantation method.
Claim 2
Dependent Claim
85 words
A process for forming an electrode of an organic electroconductive material for use in an organic cell, in which a thin film of a metal is formed on the surface of at least a part of at least one side of the organic electroconductive material in a sheet form at such a temperature that no thermal deterioration occurs in said organic material, and then an atom-interdiffused layer is formed at the interface between said thin film and said electrode by a recoil ion implantation method.
Claim 3
Dependent Claim
16 words
The process according to claim 1, wherein the organic electroconductive material is polyacetylene, polyparaphenylene or polypyrrole.
Claim 4
Dependent Claim
18 words
The process according to claim 1, wherein the metal forming the thin film is aluminum, nickel or tin.
Claim 5
Dependent Claim
26 words
The process according to claim 1, wherein the thin film is so configured that it will not cover the whole surface of said organic material electrode.
Claim 6
Dependent Claim
28 words
The process according to claim 4, wherein the thin metal film has a shape like a comb, meshes, dots or a reticulate pattern with dots connected by lines.
Claim 7
Dependent Claim
20 words
The process according to claim 1, wherein the thin metal film is formed by a vacuum evaporation or printing method.
Claim 8
Dependent Claim
19 words
The process according to claim 1, wherein the thin metal film is formed at a temperature below 200° C.
Claim 9
Dependent Claim
32 words
The process according to claim 1, wherein the thin metal film is formed on a polyacetylene sheet by an electron beam method under a vacuum of 5×10 -5 Torr at room temperature.
Claim 10
Dependent Claim
45 words
The process according to claim 1, wherein the recoil ion implantation is carried out by using Xe+ ions under the following conditions: vacuum of not more than 1×10 -6 Torr, acceleration voltage of 1.5 MeV, implantation density of 1×10 16 cm -2 and room temperature.
References Cited (Backward Citations)
No citation records indexed.
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-10-16 | 1988-04-16 | 1988-10-16 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-10-16 | 1992-04-16 | 1992-10-16 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-10-16 | 1996-04-16 | 1996-10-16 | $7700.00 | Window Closed / Lapsed |