← Back to Patent Explorer
US4476201A Expired / Lapsed US ⏱️ 0.0 years remaining

Electrochemical storage cell

Assignee: BBC Brown Boveri AG Germany
•
Filing: 1983-07-08
•
Granted: 1984-10-09
•
Expires: 2003-07-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Electrochemical storage cell of the alkali metal and sulfur type with an anode space and a cathode space which are separated from each other by an alkali ion-conducting solid electrolyte and are bounded at least in some regions by a metallic housing. A safety insert is provided for receiving the alkali metal. The alkali metal can emerge via at least one discharge opening into a safety gap. A fusible part is arranged for closing the discharge opening within the safety insert. The part is made of an alloy which contains at least two metals of the groups IB, IIA and/or IIIA of the periodic system. A material for increasing the melting point of the alloy is arranged in the discharge opening.

Inventors

  • 👤 Detlev Repenning
  • 👤 Bernd Lindner

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 14:26
CPC Classifications
H; H01; H01M; H01M10/00; H01M10/42; H01M10/36; H01M10/39; H01M10/3909; Y; Y02; Y02E; Y02E60/00; Y02E60/10

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 172 words
An electrochemical storage cell based on alkali metal and chalcogen with an anode space and a cathode space which are separated from each other by an alkali ion-conducting solid electrolyte and are bounded at least in some regions by a metallic housing, a safety insert in the anode space into which safety insert the alkali metal is received, a safety gap between the surface of the safety insert and the surface of the electrolyte, a discharge opening in the safety insert for the discharge of alkali metal from the safety insert into the safety gap, the combination therewith of closing the discharge opening at a predetermined cell temperature comprising a fusible alloy part melting at said predetermined cell temperature and containing at least two metals selected from the group consisting of metals in Groups IB, IIA and IIIA, and a material in the discharge opening which on contact with said alloy in molten condition increases the melting point of the alloy causing the alloy to solidify and close off the discharge opening.
Claim 2
Dependent Claim 172 words
An electrochemical storage cell based on alkali metal and chalcogen with an anode space and a cathode space which are separated from each other by an alkali ion-conducting solid electrolyte and are bounded at least in some regions by a metallic housing, a safety insert in the anode space into which safety insert the alkali metal is received, a safety gap between the surface of the safety insert and the surface of the electrolyte, a discharge opening in the safety insert for the discharge of alkali metal from the safety insert into the safety gap, the combination therewith of closing the discharge opening at a predetermined cell temperature comprising a fusible alloy part melting at said predetermined cell temperature and containing at least two metals selected from the group consisting of metals in Groups IB, IIA and IIIA, and a material in the discharge opening which on contact with said alloy in molten condition increases the melting point of the alloy causing the alloy to solidify and close off the discharge opening.
Claim 3
Dependent Claim 30 words
Storage cell according to claim 1, wherein the fusible alloy part is ring-shaped and arranged within the safety insert without obstructing flow of the alkali metal through the discharge opening.
Claim 4
Dependent Claim 39 words
Electrochemical storage cell according to claim 1, wherein the fusible alloy part is made of an alloy which contains about 65% by weight aluminum and about 35% by weight of magnesium based on the total weight of the alloy.
Claim 5
Dependent Claim 37 words
Storage cell according to claim 1, wherein the fusible alloy part is made of an alloy which contains about 50% by weight aluminum and about 50% by weight magnesium, based on the total weight of the alloy.
Claim 6
Dependent Claim 36 words
Electrochemical storage cell according to claim 1, wherein the fusible alloy part is made of an alloy which contains 30.7% by weight copper and 69.3% by weight magnesium, based on the total weight of the alloy.
Claim 7
Dependent Claim 24 words
Electrochemical storage cell according to claim 1, wherein said material is a wick of aluminum arranged in the discharge opening of the safety insert.
Claim 8
Dependent Claim 24 words
Electrochemical storage cell according to claim 3, wherein said material is a wick of aluminum arranged in the discharge opening of the safety insert.
Claim 9
Dependent Claim 24 words
Electrochemical storage cell according to claim 4, wherein said material is a wick of aluminum arranged in the discharge opening of the safety insert.
Claim 10
Dependent Claim 24 words
Electrochemical storage cell according to claim 5, wherein said material is a wick of aluminum arranged in the discharge opening of the safety insert.
Claim 11
Dependent Claim 31 words
Storage cell according to claim 1, wherein a metal screen of aluminum is arranged in the region of the safety gap which directly adjoins the discharge opening of the safety insert.
Claim 12
Dependent Claim 31 words
Storage cell according to claim 6, wherein a metal screen of aluminum is arranged in the region of the safety gap which directly adjoins the discharge opening of the safety insert.

References Cited (Backward Citations)

US4206272A Cited
US4246325A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-10-09 1988-04-09 1988-10-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-10-09 1992-04-09 1992-10-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-10-09 1996-04-09 1996-10-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag