Abstract
Abstract Sheet type felt material and sheet type roofing material such as shingles and rolls made therefrom. The felt comprises 10-60 wt % glass fibers of varying lengths, 15-80 wt % cellulosic fiber and 5-25% binder. The roofing material is felt of the invention saturated with asphaltic saturant and coated with filled asphaltic coating material and conventional roofing granules.
Inventors
- 👤 Alfredo A. Bondoc
- 👤 Eugene J. Flood
- 👤 Frederick W. Sieling
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-04 10:12
CPC Classifications
C; C09; C09K; C09K21/00; C09K21/06; D; D21; D21H; D21H13/00; D21H13/36; D21H13/38; D21H13/40; E; E04; E04D; E04D5/00; E04D5/02; Y; Y10; Y10T; Y10T428/00; Y10T428/24; Y10T428/24355; Y10T428/31504; Y10T428/31815; Y10T428/31819; Y10T442/00; Y10T442/50
Claims Analysis
Total Claims: 15
Claim 1
Independent Claim
146 words
Sheet type felt comprising on a dry basis: (a) between about 10 and about 60 wt % glass fiber having diameters between about 3 and about 20 microns, said glass fibers comprising between about 50 and about 95% fibers between about 3 and about 7 millimeters in length and between about 5 and about 50% fibers between about 10 and about 15 millimeters in length; (b) between about 15 and about 80 wt % cellulosic fibers, said cellulosic fibers comprising between about 25 and about 75 wt % short fibers between about 0.5 and about 1.5 millimeters and between about 25 and about 75 wt % long fibers between about 1.5 and about 3.5 millimeters in length; and (c) between about 5 and about 25 wt % binder with at least about 0.5 wt % of the binder based on dry felt being hot strength binder.
Claim 2
Dependent Claim
146 words
Sheet type felt comprising on a dry basis: (a) between about 10 and about 60 wt % glass fiber having diameters between about 3 and about 20 microns, said glass fibers comprising between about 50 and about 95% fibers between about 3 and about 7 millimeters in length and between about 5 and about 50% fibers between about 10 and about 15 millimeters in length; (b) between about 15 and about 80 wt % cellulosic fibers, said cellulosic fibers comprising between about 25 and about 75 wt % short fibers between about 0.5 and about 1.5 millimeters and between about 25 and about 75 wt % long fibers between about 1.5 and about 3.5 millimeters in length; and (c) between about 5 and about 25 wt % binder with at least about 0.5 wt % of the binder based on dry felt being hot strength binder.
Claim 3
Dependent Claim
31 words
Felt according to claim 1 comprising on a dry basis between about 15 and about 35 wt % glass fibers and between about 50 and about 60 wt % cellulosic fibers.
Claim 4
Dependent Claim
39 words
Felt according to claim 2 wherein the binder comprises between about 5 and about 15 wt % based on dry felt of styrene-butadiene rubber latex and between about 1 and about 10 wt % starch on the same basis.
Claim 5
Dependent Claim
40 words
Felt according to claim 2 wherein the binder comprises between about 5 and about 15 wt % based on dry felt of styrene-butadiene rubber latex and between about 0.5 and about 5 wt % acrylamide resin on the same basis.
Claim 6
Dependent Claim
43 words
Sheet type roofing material comprising sheet rype felt according to claim 1 said felt being saturated with between about 80 and about 150 wt % based on dry felt of asphaltic saturant having a softening point between about 25° and about 110° C.
Claim 7
Dependent Claim
69 words
Roofing material according to claim 5 comprising between about 15 and about 35 wt % glass fibers based on dry felt and between about 50 and about 60 wt % cellulosic fibers on the same basis and wherein the felt is saturated with between about 100 and about 130 wt % based on dry felt of asphaltic saturant having a softening point between about 70 and about 100° C.
Claim 8
Dependent Claim
67 words
Roofing material according to claim 5 which is top coated with between about 25 and about 45 pounds per hundred square feet and back coated with between about 3 and about 10 pounds per hundred square feet of asphaltic coating material, said coating material having a softening point between about 90 and about 115° C. and containing between about 50 and about 75 wt % mineral stabilizer.
Claim 9
Dependent Claim
98 words
Roofing material according claim 5 wherein the saturated felt is top coated with between about 25 and about 45 pounds per hundred square feet and back coated with between about 3 and about 10 pounds per hundred square feet of asphaltic coating material having a softening point between about 90° and about 110° C. and being filled with between about 50 and about 75 wt % mineral stabilizer and wherein the thus top coated material is further coated on the top coated side with between about 25 and about 80 pounds per hundred square feet of roofing granules.
Claim 10
Dependent Claim
150 words
Roofing material according to claim 8 in which (a) glass fibers are present in the felt in amounts between about 15 and about 35 wt % based on dry felt; (b) cellulosic fibers are present in the felt in amounts between about 50 and about 60 wt % based on dry felt; (c) the felt is saturated with between about 100 and about 130 wt % based on dry felt of asphaltic saturant having a softening point between about 70 and about 100° C.; and (d) the saturated felt is top coated with between about 25 and about 35 pounds per hundred square feet of asphaltic coating filled with between about 60 and about 70 wt % mineral stabilizer and having a softening point between about 90° and about 115° C. and is back coated with between about 3 and about 10 pounds per hundred square foot of such coating.
Claim 11
Dependent Claim
41 words
Roofing material according to claim 7 wherein the binder comprises between about 5 and about 15 wt % based on dry felt of styrene-butadiene rubber latex and between about 1 and about 10 wt % on the same basis of starch.
Claim 12
Dependent Claim
42 words
Roofing material according to claim 7 wherein the binder comprises between about 5 and about 15 wt % based on dry felt of styrene-butadiene rubber latex and between about 0.5 and about 5 wt % on the same basis of acrylamide resin.
Claim 13
Dependent Claim
42 words
Roofing material according to claim 9 wherein the binder comprises between about 5 and about 15 wt % based on dry felt of styrene butadiene rubber latex and between about 1 and about 10 wt % on the same basis of starch.
Claim 14
Dependent Claim
43 words
Roofing material according to claim 9 wherein the binder comprises between about 5 and about 15 wt % based on dry felt of styrene butadiene rubber latex and between about 0.5 and about 5 wt % on the same basis of acrylamide resin.
Claim 15
Dependent Claim
11 words
Roofing material according to claim 9 in the form of shingles.
References Cited (Backward Citations)
US2555401A
Cited
US2772603A
Cited
US2702241A
Cited
US3749638A
Cited
US4035544A
Cited
GB2009277A
Cited
US4225383A
Cited
US4284470A
Cited
US4440816A
Cited
US4373992A
Cited
US4442172A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-09-18 | 1988-03-19 | 1988-09-18 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-09-18 | 1992-03-19 | 1992-09-18 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-09-18 | 1996-03-19 | 1996-09-18 | $7700.00 | Window Closed / Lapsed |