Linear medium- or low-density polyethylene composition
Abstract
Abstract A modified linear medium- or low-density polyethylene composition obtained by uniformly melt kneading a mixture of a linear medium- or low-density polyethylene having a density of not less than 0.90 g/cm 3 but less than 0.94 g/cm 3 and a melt index (MI) 1 of not more than 3 g/10 minutes and a radical initiator in an amount of not less than 0.0005% by weight but less than 0.1% by weight based on the weight of the linear medium- or low-density polyethylene at a temperature of from the melting point of the linear medium- or low-density polyethylene to a temperature of less than the thermal decomposition temperature of the linear medium- or low-density polyethylene to such an extent that the ratio of the melt index of the modified linear medium- or low-density polyethylene composition (MI) 2 to that of the linear medium- or low-density polyethylene (MI) 1 [(MI) 2 /(MI) 1 ] is 0.05 to 0.9.
Inventors
- 👤 Kisoo Moriguchi
- 👤 Isaburo Fukawa
Bibliographic Details
Claims Analysis
Total Claims: 7References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-08-14 | 1988-02-13 | 1988-08-14 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-08-14 | 1992-02-13 | 1992-08-14 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-08-14 | 1996-02-13 | 1996-08-14 | $7700.00 | Window Closed / Lapsed |