Abstract

Abstract A method of increasing the efficiency of a cyclone-fired boiler which uses high sodium lignite as fuel. The fuel produces ash deposits on heat transfer surfaces within the boilers, and in accordance with the method, powdered limestone is periodically injected into the firebox of the boiler in a quantity and for a time period such that the limestone is heated to a temperature in the range of from about 2200° F. to about 2700° F. and reacts with ash deposits in the boiler to form layers thereon. The layers so formed have a higher ash fusion temperature than the unreacted deposits and cause the resulting composite deposit to be more friable whereby the deposit can be removed using conventional soot blower apparatus.

Inventors

  • 👤 Elwyn Shimoda

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 03:34
CPC Classifications
F; F23; F23J; F23J3/00; F23J7/00

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 221 words
A method of increasing the efficiency of a cyclone-fired boiler using high sodium lignite fuel which produces ash deposits on heat transfer surfaces within the boiler comprising: (a) cyclically injecting, separately from the supply of said fuel to said boiler, time-spaced doses of powdered limestone into the firebox of said boiler at a location such that said limestone is heated to a temperature in the range of from about 2200° F. to about 2700° F. and maintained in said temperature range for a time period less than the time at which said limestone becomes unreactive, (b) contacting ash deposits on said heat transfer surfaces, which have formed from operation between said doses, with said limestone which is in said temperature range, whereby said limestone and ash deposits react to form a layer which is more friable than said ash deposits and which has an ash fusion temperature higher than that of said ash deposits; and (c) periodically removing said deposits from said heat transfer surfaces; wherein said doses are injected at a location such that the powdered limestone is maintained in said temperature range for about two seconds prior to contacting ash deposits on said heat transfer surfaces and each dose of powdered limestone is injected for a period of ten seconds, and the time interval between doses is thirty minutes.
Claim 2
Independent Claim 221 words
A method of increasing the efficiency of a cyclone-fired boiler using high sodium lignite fuel which produces ash deposits on heat transfer surfaces within the boiler comprising: (a) cyclically injecting, separately from the supply of said fuel to said boiler, time-spaced doses of powdered limestone into the firebox of said boiler at a location such that said limestone is heated to a temperature in the range of from about 2200° F. to about 2700° F. and maintained in said temperature range for a time period less than the time at which said limestone becomes unreactive, (b) contacting ash deposits on said heat transfer surfaces, which have formed from operation between said doses, with said limestone which is in said temperature range, whereby said limestone and ash deposits react to form a layer which is more friable than said ash deposits and which has an ash fusion temperature higher than that of said ash deposits; and (c) periodically removing said deposits from said heat transfer surfaces; wherein said doses are injected at a location such that the powdered limestone is maintained in said temperature range for about two seconds prior to contacting ash deposits on said heat transfer surfaces and each dose of powdered limestone is injected for a period of ten seconds, and the time interval between doses is thirty minutes.
Claim 3
Independent Claim 249 words
A method of increasing the efficiency of a cyclone-fired boiler using high sodium lignite fuel which produces ash deposits containing sodium sulfate and calcium sulfate on convective heat transfer surfaces within said boiler comprising the steps of: (a) cyclically injecting, separately from the supply of said fuel to said boiler, time-spaced doses of powdered calcium carbonate into the firebox of said boiler above the flames of burning sodium lignite fuel therein in a quantity and at a location such that said calcium carbonate is heated to a temperature in the range of from about 2200° F. to about 2700° F. and maintained in said temperature range for a time period less than the time at which calcium carbonate becomes unreactive; (b) contacting ash deposits on said heat transfer surfaces, which have formed from operation between said doses, with said calcium carbonate which is in said temperature range, whereby said calcium carbonate and ash deposits react to form a layer which is more friable than said ash deposits and which has an ash fusion temperature higher than that of said ash deposits; and (c) periodically removing said deposits from said heat transfer surfaces; wherein said doses are injected at a location such that the powdered calcium carbonate is maintained in said temperature range for about two seconds prior to contacting ash deposits on said heat transfer surfaces and each dose of calcium carbonate is injected for a period of ten seconds, and the time interval between doses is thirty minutes.
Claim 4
Independent Claim 249 words
A method of increasing the efficiency of a cyclone-fired boiler using high sodium lignite fuel which produces ash deposits containing sodium sulfate and calcium sulfate on convective heat transfer surfaces within said boiler comprising the steps of: (a) cyclically injecting, separately from the supply of said fuel to said boiler, time-spaced doses of powdered calcium carbonate into the firebox of said boiler above the flames of burning sodium lignite fuel therein in a quantity and at a location such that said calcium carbonate is heated to a temperature in the range of from about 2200° F. to about 2700° F. and maintained in said temperature range for a time period less than the time at which calcium carbonate becomes unreactive; (b) contacting ash deposits on said heat transfer surfaces, which have formed from operation between said doses, with said calcium carbonate which is in said temperature range, whereby said calcium carbonate and ash deposits react to form a layer which is more friable than said ash deposits and which has an ash fusion temperature higher than that of said ash deposits; and (c) periodically removing said deposits from said heat transfer surfaces; wherein said doses are injected at a location such that the powdered calcium carbonate is maintained in said temperature range for about two seconds prior to contacting ash deposits on said heat transfer surfaces and each dose of calcium carbonate is injected for a period of ten seconds, and the time interval between doses is thirty minutes.
Claim 5
Dependent Claim 11 words
The method of claim 2 wherein said calcium carbonate is limestone.

References Cited (Backward Citations)

US1167472A Cited
US2905116A Cited
US2935956A Cited
US3234580A Cited
US4159683A Cited
US4237103A Cited
US4259911A Cited
US4253408A Cited
US4312280A Cited
US4325327A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-08-14 1988-02-13 1988-08-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-08-14 1992-02-13 1992-08-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-08-14 1996-02-13 1996-08-14 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag